Measures for Higher Tungsten Recovery during the Alkaline Decomposition of Tungsten Minerals AITranslate

Chenzhou Diamond Tungsten Products Co., Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The present status of alkali autoclave process of tungsten minerals is described. A deep-processing technology of tungsten minerals for extracting tungsten was developed to optimize the process flowsheet of alkaline decomposition production. Upon taking some corresponding technical measures,the WO3 content in tungsten residue is only 1.0- 1.5%, and the overall recovery of tungsten minerals increases by 1-2 percentage points so that the tungsten resource is effectively utilized.

KeyWords AITranslate

tungsten metallurgy tungsten resource tungsten mineral alkaline decomposition recovery

1孔昭庆.我国钨工业必须加快发展循环经济[J].中国钨业,2005,20(5):1-6. 被引量:10

2李洪桂.浅谈为保证我国钨业可持续发展的某些技术措施[J].中国钨业,2004,19(5):40-43. 被引量:13

3普崇恩.在黑钨矿湿法冶金处理中提高回收率的研究[A].株洲硬质合金厂参加国际科技交流论文集[C].株洲:株洲硬质合金厂,1994.93-98.

4李洪桂 刘茂盛 戴朝嘉 等.白钨矿碱分解过程的热力学.稀有金属与硬质合金,1987,15(1):1-9.

5梁卫东.二次压煮工艺提高钨冶炼金属回收率的应用[J].稀有金属与硬质合金,2006,34(4):45-47. 被引量:6

1艾光华,刘炯天.钨矿选矿药剂和工艺的研究现状及展望[J].矿山机械,2011,39(4):1-7. 被引量:32

2李俊荣,李毅鹏.立式压滤机在钨冶炼碱分解工艺中的应用实践[J].江西化工,2015,31(5):118-120. 被引量:3

1艾光华,李晓波.微细粒黑钨矿选矿研究现状及展望[J].矿山机械,2011,39(10):89-96. 被引量:15

2辛亚淘,邓双丽.低品位白钨矿的浮选实践[J].矿山机械,2012,40(2):88-90. 被引量:6

3李英霞,王国生.广东某白钨矿选矿的试验研究[J].矿产保护与利用,2012,32(2):20-22. 被引量:2

4李英霞,王国生.某白钨矿回收工艺的试验研究[J].中国钨业,2012,27(4):23-25. 被引量:10

5任传成,杨建国.浮选过程精矿品位软测量技术的研究进展[J].矿山机械,2013,41(8):8-12. 被引量:4

6谭鑫,范志鸿,陈定洲,刘龙利.钨矿螯合捕收剂的研究现状及展望[J].现代矿业,2013(9):1-5. 被引量:2

7黄万抚,张小冬.钨矿细泥选矿工艺发展[J].有色金属科学与工程,2013,4(5):54-57. 被引量:4

8齐美超,何桂春,罗仙平,项华妹,蒋巍.钨矿表面特性与可浮性关系研究现状[J].有色金属科学与工程,2014,5(1):73-76. 被引量:3

9毕献武,董少花.我国矿产资源高效清洁利用进展与展望[J].矿物岩石地球化学通报,2014,33(1):14-22. 被引量:25

10王燕,张凌浩.家庭用电监管智能终端系统设计策略研究[J].包装世界,2014(2):90-92.

1张启修,龚柏凡,黄芍英,黄蔚庄,周良益.处理低品位钨物料生产高纯APT的新工艺研究[J].稀有金属与硬质合金,1989(2):2-5. 被引量:1

2于工.日本金属钨产品持续增长[J].中国钨业,1990(7):34-35.

3李洪桂,吕莹,赵中伟.从钨矿物原料制取钨粉的新工艺[J].中国钨业,2007,22(1):30-32. 被引量:1

4柯兆华,张贵清,关文娟,尚广浩.季铵盐从碱性钨酸钠溶液中萃取钨的研究[J].稀有金属与硬质合金,2012,40(6):1-4. 被引量:10

5李裕芳,赖道玉.高碱浸出含高白钨黑钨矿的试验研究[J].中国钨业,1991,0(5):17-19. 被引量:1

6俞集良.钨矿物细菌浸出[J].中国钨业,1990(10):32-33.

7李洪桂,刘茂盛,孙培梅.钨矿物原料碱分解的基础理论研究(摘要)[J].稀有金属与硬质合金,1989(2):6-9. 被引量:2

8廖贡越,严培生,林中梁.热球磨碱分解技术在我厂的应用[J].中国钨业,1992(12):13-17. 被引量:1

9刘茂盛,李洪桂,孙培梅,李运姣,苏鹏抟,赵中伟.机械活化苏打溶液分解白钨中矿试验研究[J].中南矿冶学院学报,1994,25(3):321-325. 被引量:3

10李洪桂.从高钼含量的白钨精矿及复杂钨矿物原料制取高纯APT[J].中国钨业,2003,18(5):36-39. 被引量:4

Basic Information:

DOI:

Chinese Library Classification Number:TF803.22[冶金工程—有色金属冶金]

Citation Information:

The present status of alkali autoclave process of tungsten minerals is described. A deep-processing technology of tungsten minerals for extracting tungsten was developed to optimize the process flowsheet of alkaline decomposition production. Upon taking some corresponding technical measures,the WO3 content in tungsten residue is only 1.0- 1.5%, and the overall recovery of tungsten minerals increases by 1-2 percentage points so that the tungsten resource is effectively utilized.

quote

GB/T 7714-2015 [1] LONG Yang. Measures for Higher Tungsten Recovery during the Alkaline Decomposition of Tungsten Minerals[J]. Rare Metals and Cemented Carbides, 2008(4): 20-23.
MLA [1] LONG Yang. "Measures for Higher Tungsten Recovery during the Alkaline Decomposition of Tungsten Minerals." Rare Metals and Cemented Carbides, no. 4, 2008, pp. 20-23.
APA [1] LONG Yang. (2008). Measures for Higher Tungsten Recovery during the Alkaline Decomposition of Tungsten Minerals. Rare Metals and Cemented Carbides(4), 20-23.
IEEE [1] LONG Yang, "Measures for Higher Tungsten Recovery during the Alkaline Decomposition of Tungsten Minerals," Rare Metals and Cemented Carbides, no. 4, pp. 20-23, 2008. keywords: {tungsten metallurgy;tungsten resource;tungsten mineral;alkaline decomposition;recovery}