Different factors’ effect on the SWNT-fluorocarbon resin interaction: A MD simulation study AITranslate

China University of Petroleum; China University of Petroleum; China University of Petroleum; University of Aarhus; University of Aarhus
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Molecular mechanics (MM) and molecular dynamics (MD) simulations are conducted to investigate the influence of four different factors, namely temperature, chirality, radius and surface chemical modification, on the interaction between single-walled carbon nanotubes (SWNTs) and three fluorocarbon resins: PVF, PVDF, and PTFE. The results show that the interactions between the SWNTs and fluorocarbon resins are not influenced by temperature and chirality but strongly depend on the radius of SWNTs with the interactions increasing monotonously with the radius. Also the surface chemical modification on the SWNTs has a great effect on the interaction between the nanotubes and the fluorocarbon resins. Among five kinds of functional groups: methyl, amidogen, hydroxyl, –F and carboxyl, the three fluorocarbon resins can only adhere onto the SWNTs modified by methyl. The interactions between the SWNTs and the fluorocarbon resins are observed to increase with increasing functional group coverage. However, in the case for PTFE, an optimum functional group coverage is found beyond which the interactions decrease again. In addition, the ability of the PTFE to adsorb onto the methylic SWNTs is weaker than that of the other two resins due to its non-adhesive nature.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.commatsci.2010.04.038

Chinese Library Classification Number:

Citation Information:

Molecular mechanics (MM) and molecular dynamics (MD) simulations are conducted to investigate the influence of four different factors, namely temperature, chirality, radius and surface chemical modification, on the interaction between single-walled carbon nanotubes (SWNTs) and three fluorocarbon resins: PVF, PVDF, and PTFE. The results show that the interactions between the SWNTs and fluorocarbon resins are not influenced by temperature and chirality but strongly depend on the radius of SWNTs with the interactions increasing monotonously with the radius. Also the surface chemical modification on the SWNTs has a great effect on the interaction between the nanotubes and the fluorocarbon resins. Among five kinds of functional groups: methyl, amidogen, hydroxyl, –F and carboxyl, the three fluorocarbon resins can only adhere onto the SWNTs modified by methyl. The interactions between the SWNTs and the fluorocarbon resins are observed to increase with increasing functional group coverage. However, in the case for PTFE, an optimum functional group coverage is found beyond which the interactions decrease again. In addition, the ability of the PTFE to adsorb onto the methylic SWNTs is weaker than that of the other two resins due to its non-adhesive nature.

quote

GB/T 7714-2015 [1] Jie Xie, Qingzhong Xue, Huijuan Chen, et al. Computational Materials Science, 2010(49). DOI:10.1016/j.commatsci.2010.04.038.
MLA [1] Jie Xie, et al., Computational Materials Science, no. 49, 2010, https://doi.org/10.1016/j.commatsci.2010.04.038.
APA [1] Jie Xie, Qingzhong Xue, Huijuan Chen, Adrian Keller, & Mingdong Dong. (2010). Computational Materials Science(49). https://doi.org/10.1016/j.commatsci.2010.04.038
IEEE [1] Jie Xie, Qingzhong Xue, Huijuan Chen, Adrian Keller, and Mingdong Dong, Computational Materials Science, no. 49, 2010, doi: 10.1016/j.commatsci.2010.04.038.