Ultrastretchable, Highly Conductive, Rapid Self-Recovery, and Antiswelling Hydrogels as Multifunctional Wearable Electronic Devices AITranslate

Hunan University of Technology; Hunan University of Technology; Hunan University of Technology; South China University of Technology; Hunan University of Technology; Hunan University of Technology;The Orthopedics Hospital of Traditional Chinese Medicine Zhuzhou City, Zhuzhou 412007; Hunan University of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The development of wearable electronic devices requires stretchable, highly conductive, self-recovery, and ideally environmentally resistant sensors. Hydrogels are ideal candidates for fabricating flexible sensors due to their stretchability and unique ionic conduction pathways. However, the intrinsic incompatibility of the conductive and elastic networks in hydrogels and the high hydrophilicity of the hydrogel network led to difficulties in obtaining hydrogels with strong mechanical properties, high conductivity, rapid self-recovery ability, and antiswelling properties. Based on the single-core multidentate coordination strategy, single-core multidentate coordinated chitosan/poly(acrylic acid)/Al3+ (CPAL) hydrogels were prepared with Al3+ as a metal coordination center and the amino group of chitosan (CS) and the carboxyl group of poly(acrylic acid) (PAA) as coordination atoms. The obtained hydrogels exhibit excellent tensile stress/strain: 1.11 ± 0.04 MPa/2472.79 ± 99.27%, rapid self-recovery capability (mechanical properties were fully recovered in 10 min), antifatigue property, good conductivity (1.09 ± 0.02 S/m), and antiswelling property. Furthermore, flexible sensors based on CPAL hydrogels demonstrated multiplex mode sensing. It was worth noting that the flexible devices based on CPAL hydrogel could not only use Morse code table to realize mechanical-information visualization but also detect the human condition in multiple dimensions, including temperature, electromyographic (EMG), and electrocardiogram (ECG). In this work, we reported a single-core multidentate coordination strategy that provided a pathway for fabricating the ideal hydrogel-based flexible sensors, showing great potential for wearable electronic devices.

KeyWords AITranslate

conductive hydrogels flexible sensor mechanical property coordination antiswelling property
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c00997

Chinese Library Classification Number:

Citation Information:

The development of wearable electronic devices requires stretchable, highly conductive, self-recovery, and ideally environmentally resistant sensors. Hydrogels are ideal candidates for fabricating flexible sensors due to their stretchability and unique ionic conduction pathways. However, the intrinsic incompatibility of the conductive and elastic networks in hydrogels and the high hydrophilicity of the hydrogel network led to difficulties in obtaining hydrogels with strong mechanical properties, high conductivity, rapid self-recovery ability, and antiswelling properties. Based on the single-core multidentate coordination strategy, single-core multidentate coordinated chitosan/poly(acrylic acid)/Al3+ (CPAL) hydrogels were prepared with Al3+ as a metal coordination center and the amino group of chitosan (CS) and the carboxyl group of poly(acrylic acid) (PAA) as coordination atoms. The obtained hydrogels exhibit excellent tensile stress/strain: 1.11 ± 0.04 MPa/2472.79 ± 99.27%, rapid self-recovery capability (mechanical properties were fully recovered in 10 min), antifatigue property, good conductivity (1.09 ± 0.02 S/m), and antiswelling property. Furthermore, flexible sensors based on CPAL hydrogels demonstrated multiplex mode sensing. It was worth noting that the flexible devices based on CPAL hydrogel could not only use Morse code table to realize mechanical-information visualization but also detect the human condition in multiple dimensions, including temperature, electromyographic (EMG), and electrocardiogram (ECG). In this work, we reported a single-core multidentate coordination strategy that provided a pathway for fabricating the ideal hydrogel-based flexible sensors, showing great potential for wearable electronic devices.

quote

GB/T 7714-2015 [1] Li Tang, Youwei Li, Fang Liu, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00997.
MLA [1] Li Tang, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00997.
APA [1] Li Tang, Youwei Li, Fang Liu, Shaoji Wu, Wu Wang, Xiuli Sun, Zehua Chen, & Jianxin Tang. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00997
IEEE [1] Li Tang, Youwei Li, Fang Liu, Shaoji Wu, Wu Wang, Xiuli Sun, Zehua Chen, and Jianxin Tang, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00997. keywords: {conductive hydrogels flexible sensor mechanical property coordination antiswelling property}