Effect of Morphology of APT on Microstructure and Properties of W,WC Powder and Cemented Carbide AITranslate
Abstract AITranslate
Single crystal APT and polycrystalline APT prepared by different crystallization processes were used as raw materials to produce single crystal tungsten trioxide and polycrystalline tungsten trioxide after high temperature calcination.Then, using single crystal tungsten trioxide and polycrystal tungsten trioxide as raw materials, medium grain tungsten powder, tungsten carbide and WC-6%Co cemented carbide were prepared, and the effect of APT morphology on the microstructure, physical and mechanical properties of powder products and cemented carbide were studied in detail.The results show that the tungsten trioxide prepared by calcining APT with different morphologies still retains the morphology of APT.The tungsten powder prepared by two kinds of tungsten trioxide with different morphologies is quasi-spherical, but the tungsten powder prepared by single crystal tungsten trioxide has good uniformity, less fine powder, no obvious crystallographic plane and high spheroidization degree.However, the tungsten powder prepared by polycrystalline tungsten trioxide has poor uniformity, more fine powder and obvious crystallographic plane.In the carbonization process, the grain size of tungsten powder prepared by single crystal tungsten trioxide increases by 21.5%,which is significantly higher compared with tungsten powder prepared by polycrystalline tungsten trioxide, and the granules with high spheroidization degree are more in the prepared tungsten carbide.Compared with WC-6%Co cemented carbide prepared by polycrystalline APT,WC-6%Co cemented carbide prepared by single crystal APT has higher coercive force, hardness and bending strength, better microstructure uniformity and more excellent overall properties.
KeyWords AITranslate
1朱斌,柏振海,高阳,罗兵辉.WC粒度对WC-15Fe-5Ni硬质合金组织与性能的影响[J].中国有色金属学报,2016,26(5):1065-1074. 被引量:11
2周红翠,于涛,贺鸣.WC原料的多晶结构对合金组织及性能的影响[J].硬质合金,2018,35(4):249-257. 被引量:5
3尹超,张卫兵,谢晨辉,陆必志.原始WC粉末粒度组成对超细硬质合金组织及性能的影响[J].硬质合金,2017,34(1):7-13. 被引量:5
4吴桐,唐建成,叶楠,卓海鸥,薛滢妤,周旭升.碳辅助氢还原制备纳米钨粉的工艺及机理[J].中国有色金属学报,2016,26(5):1027-1033. 被引量:8
5卓海鸥,叶楠,周强,刘文胜,唐建成.碳辅助氢还原与普通氢还原制备W粉的对比研究[J].中国有色金属学报,2018,28(4):742-748. 被引量:1
6雷纯鹏,唐建成,蔡旦瑜,吴爱华.高温中颗粒WC粉及其WC-6Co合金的组织和性能[J].稀有金属,2013,37(3):365-371. 被引量:12
7孙亚丽,刘清才,黄新,张发兴,杨剑,梅华.气流粉碎对超细WC粉体微观应变行为及团粒破碎行为的影响(英文)[J].中国有色金属学报:英文版,2019,29(10):2128-2140. 被引量:7
8叶楠,唐建成,吴爱华,魏晓枭.碳氢协同还原-碳化法制备纳米WC粉的工艺及机理[J].稀有金属材料与工程,2017,46(1):143-149. 被引量:6
9郭圣达,鲍瑞,易健宏,羊建高,刘亮,杨平.SPS制备含钼WC-6Co硬质合金的工艺性能[J].中国有色金属学报,2018,28(3):556-564. 被引量:6
10羊求民,唐彦渊,赖星任,张龙辉,邓登飞,李倩.Mo含量对烧结WC-CoCrCuFeNiMo_x硬质合金性能的影响[J].材料热处理学报,2018,39(11):46-51. 被引量:2
1王晓灵,雍薇,彭晖.研磨体材质对WC-6%Co硬质合金显微组织及性能的影响[J].稀有金属与硬质合金,2022,50(1):89-95.
2余灿生,张龙超,郑之旺,龚慧,张达富.退火温度对钒微合金化780 MPa级冷轧双相钢组织性能的影响[J].钢铁钒钛,2021,42(5):158-163. 被引量:4
3刘东洋,虞秀勇,高文理,陆政,毛郭灵.金属型铸造条件下Sb元素对ZL114A合金共晶Si和拉伸性能的影响[J].金属热处理,2021,46(11):36-41.
4顾金宝,刁椿珉,时凯华,董定乾,曾伟,董凯林,向新.碳含量对非均匀硬质合金组织和性能的影响[J].硬质合金,2021,38(3):193-200. 被引量:1
5赵帆,胡昊,刘雅政,张志豪,谢建新.基于23MnNiMoCr54钢复杂显微组织和表面脱碳演变规律的退火条件控制[J].材料导报,2022,36(1):126-131.
6蒋国璋,邱鹤,林昕,刘江昊.SLM成型件表面球化程度表征方法及等级检测[J].激光与红外,2021,51(12):1576-1585.
7何涛,何立柱,郑云锋,孙书红,刘涛,谭争国.催化裂化装置油浆固体质量浓度升高原因分析及对策[J].石化技术与应用,2022,40(2):126-131.
8宋光杰,何佳乐,闫震.晶体学中的简单立体几何知识[J].中学化学教学参考,2022(2):62-63.
9贾冉冉,刘虎,佘洁,黄小川,李力成.不同形貌固体酸的纤维素乙酰化催化性能研究[J].纤维素科学与技术,2022,30(1):71-80.
10祝文沙,潘明艳.一种近α钛合金管在热轧过程中位向对组织球化的影响[J].钢铁钒钛,2021,42(5):69-73.
Basic Information:
DOI:
Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程]
Citation Information:
Single crystal APT and polycrystalline APT prepared by different crystallization processes were used as raw materials to produce single crystal tungsten trioxide and polycrystalline tungsten trioxide after high temperature calcination.Then, using single crystal tungsten trioxide and polycrystal tungsten trioxide as raw materials, medium grain tungsten powder, tungsten carbide and WC-6%Co cemented carbide were prepared, and the effect of APT morphology on the microstructure, physical and mechanical properties of powder products and cemented carbide were studied in detail.The results show that the tungsten trioxide prepared by calcining APT with different morphologies still retains the morphology of APT.The tungsten powder prepared by two kinds of tungsten trioxide with different morphologies is quasi-spherical, but the tungsten powder prepared by single crystal tungsten trioxide has good uniformity, less fine powder, no obvious crystallographic plane and high spheroidization degree.However, the tungsten powder prepared by polycrystalline tungsten trioxide has poor uniformity, more fine powder and obvious crystallographic plane.In the carbonization process, the grain size of tungsten powder prepared by single crystal tungsten trioxide increases by 21.5%,which is significantly higher compared with tungsten powder prepared by polycrystalline tungsten trioxide, and the granules with high spheroidization degree are more in the prepared tungsten carbide.Compared with WC-6%Co cemented carbide prepared by polycrystalline APT,WC-6%Co cemented carbide prepared by single crystal APT has higher coercive force, hardness and bending strength, better microstructure uniformity and more excellent overall properties.
quote
| GB/T 7714-2015 | [1] ZHANG Long-hui, ZHOU Jun-an, XU Guo-zuan, et al. Effect of Morphology of APT on Microstructure and Properties of W,WC Powder and Cemented Carbide[J]. Rare Metals and Cemented Carbides, 2022(1): 81-88. |
| MLA | [1] ZHANG Long-hui, et al., "Effect of Morphology of APT on Microstructure and Properties of W,WC Powder and Cemented Carbide." Rare Metals and Cemented Carbides, no. 1, 2022, pp. 81-88. |
| APA | [1] ZHANG Long-hui, ZHOU Jun-an, XU Guo-zuan, YANG Cheng-hui, YANG Qiu-min, & LIU Ru-tie. (2022). Effect of Morphology of APT on Microstructure and Properties of W,WC Powder and Cemented Carbide. Rare Metals and Cemented Carbides(1), 81-88. |
| IEEE | [1] ZHANG Long-hui, ZHOU Jun-an, XU Guo-zuan, YANG Cheng-hui, YANG Qiu-min, and LIU Ru-tie, "Effect of Morphology of APT on Microstructure and Properties of W,WC Powder and Cemented Carbide," Rare Metals and Cemented Carbides, no. 1, pp. 81-88, 2022. keywords: {single crystal;polycrystalline;APT;W powder;WO3 powder;cemented carbide;property} |