Effect of Grinding Body Material on Microstructure and Properties of WC-6%Co Cemented Carbide AITranslate

Chengdu Branch,Zigong Cemented Carbide Co.,Ltd.;Chengdu Branch,Zigong Cemented Carbide Co.,Ltd.;Chengdu Branch,Zigong Cemented Carbide Co.,Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Two kinds of grinding bodies, made with ZLT15 grade alloy(WC-20%TiC-13%Co) and traditional YG6 X grade alloy(WC-6%Co),were respectively used for ball milling of the mixture, and WC-6%Co cemented carbide samples were prepared under the same other process conditions.By testing coercive force, specific saturation magnetization, transverse rupture strength, Vickers hardness and fracture toughness of the alloy samples, analyzing metallographic microstructure and WC grain size distribution, and analyzing composition of the binder phase by SEM-EDS,the influence of grinding body material on microstructure and properties of WC-6%Co cemented carbide was comparatively studied.The results show that compared with the traditional YG6 X grade alloy grinding body, the lightweight ZLT15 grade alloy grinding body has less impact on the powder during ball milling of the mixture and lower grinding strength, which reduces processing distortion, sub-crystalline defect density and chemical activity of the powder, and decreases the driving force of grain growth during sintering.finally, the cemented carbide obtained with ZLT15 grade alloy grinding body has more uniform microstructure and better properties.

KeyWords AITranslate

cemented carbide mixture grinding body material ball milling process microstructure physical and mechanical property

1甘绪发,李海雄,杨文超,夏恩华,张洪刚,姜宁,谭会文.超粗晶粒混合料制备方法研究[J].四川冶金,2015,37(4):18-22. 被引量:1

2雍薇,彭晖,刘益兴,王晓灵.晶粒长大抑制剂对WC-9%Co超细晶硬质合金组织及性能的影响[J].硬质合金,2018,35(5):338-343. 被引量:5

3石丽秋,王晓灵,熊超伟.球磨时间对双晶结构的WC-TiC-Co/Ni硬质合金组织及性能的影响[J].硬质合金,2015,32(3):155-163. 被引量:4

1顾金宝,刁椿珉,时凯华,董定乾,曾伟,董凯林,向新.碳含量对非均匀硬质合金组织和性能的影响[J].硬质合金,2021,38(3):193-200. 被引量:1

2张龙辉,周俊安,徐国钻,杨诚辉,羊求民,刘如铁.APT形貌对W、WC粉及硬质合金组织性能的影响研究[J].稀有金属与硬质合金,2022,50(1):81-88.

3华涛,郭智兴,杨露,荆凯峰,鲜广.粗晶粒硬质合金材料的制备与表征[J].实验室研究与探索,2022,41(1):33-36. 被引量:1

4刘欣.变形对330 MPa级热轧搪瓷钢组织和储氢性能的影响[J].上海金属,2022,44(2):51-55. 被引量:1

5程志瑶,沈显峰,王国伟.退火工艺对选区激光熔化成形AlSi10Mg合金组织和力学性能的影响[J].热加工工艺,2022,51(2):121-125. 被引量:3

6刘娜娜,徐新阳,陈熙,刘源.SCR废催化剂中钒和钨常温常压浸出新工艺[J].东北大学学报:自然科学版,2022,43(3):414-422.

7吴后选,谢梅兰,周小敏,徐旋,鄢鹏.养护温度对C_(3)S-C_(3)A浆体微结构的影响[J].武汉理工大学学报,2021,43(12):18-22. 被引量:1

8张洪,熊计,郭智兴,杨天恩,易建松,杨善东,梁磊.WC粒径对WC-Co硬质合金高温耐磨性的影响[J].热加工工艺,2022,51(2):21-24. 被引量:3

9刘博.稀土Er对Al-Mg合金组织和性能的影响研究[J].功能材料,2022,53(1):1020-1024. 被引量:2

10孙琳,邓运来,池水清.Zn含量对Al-Mg-Si系合金组织与晶间腐蚀性能的影响[J].热加工工艺,2022,51(2):110-113.

Basic Information:

DOI:

Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程]

Citation Information:

Two kinds of grinding bodies, made with ZLT15 grade alloy(WC-20%TiC-13%Co) and traditional YG6 X grade alloy(WC-6%Co),were respectively used for ball milling of the mixture, and WC-6%Co cemented carbide samples were prepared under the same other process conditions.By testing coercive force, specific saturation magnetization, transverse rupture strength, Vickers hardness and fracture toughness of the alloy samples, analyzing metallographic microstructure and WC grain size distribution, and analyzing composition of the binder phase by SEM-EDS,the influence of grinding body material on microstructure and properties of WC-6%Co cemented carbide was comparatively studied.The results show that compared with the traditional YG6 X grade alloy grinding body, the lightweight ZLT15 grade alloy grinding body has less impact on the powder during ball milling of the mixture and lower grinding strength, which reduces processing distortion, sub-crystalline defect density and chemical activity of the powder, and decreases the driving force of grain growth during sintering.finally, the cemented carbide obtained with ZLT15 grade alloy grinding body has more uniform microstructure and better properties.

quote

GB/T 7714-2015 [1] WANG Xiao-ling, YONG Wei, PENG Hui. Effect of Grinding Body Material on Microstructure and Properties of WC-6%Co Cemented Carbide[J]. Rare Metals and Cemented Carbides, 2022(1): 89-95.
MLA [1] WANG Xiao-ling, et al., "Effect of Grinding Body Material on Microstructure and Properties of WC-6%Co Cemented Carbide." Rare Metals and Cemented Carbides, no. 1, 2022, pp. 89-95.
APA [1] WANG Xiao-ling, YONG Wei, & PENG Hui. (2022). Effect of Grinding Body Material on Microstructure and Properties of WC-6%Co Cemented Carbide. Rare Metals and Cemented Carbides(1), 89-95.
IEEE [1] WANG Xiao-ling, YONG Wei, and PENG Hui, "Effect of Grinding Body Material on Microstructure and Properties of WC-6%Co Cemented Carbide," Rare Metals and Cemented Carbides, no. 1, pp. 89-95, 2022. keywords: {cemented carbide;mixture;grinding body;material;ball milling process;microstructure;physical and mechanical property}