Comparative Analysis of Sulfation Roasting-Water Leaching Process for Recovery of NdFeB and CeFeB Wastes AITranslate
Abstract AITranslate
A separate CeO2phase appears in the oxidized material of CeFeB waste and changes its valence state during the sulfation roasting process,which differs from NdFeB waste.Therefore,this paper conducted a comparative analysis of the sulfation roasting process of the oxidized materials of these two wastes.The research results show that the highest sulfation rates of the oxidized materials of NdFeB and CeFeB wastes are 91.7%and 96.1%,respectively.The sulfation process of the former mainly occurs in the medium-temperature roasting stage,while that of the latter mainly occurs in the low-temperature infiltration stage with the generation of an intermediate Ce(SO4)2in the medium-temperature roasting stage.The final products of sulfation roasting for both are Fe2O3and RE2(SO4)3.Their high-temperature roasted materials have an loose structure with uneven pore size,and most of the rare earth-rich phases are encapsulated by the non-rare earth phases.Apart from CeO2,the roasting mechanism of the CeFeB waste is consistent with that of the NdFeB waste:rare earth oxides and Fe2O3reacts with sulfuric acid to generate water-soluble rare earth sulfates and Fe2(SO4)3;Fe2SO43is decomposed into Fe2O3and SO3at high temperature,and SO3further reacts with unreacted rare earth oxides to generate rare earth sulfates.CeO2reacts with sulfuric acid to form Ce(SO42at first,which is then decomposed into Ce2(SO4)3.The SO3generated during the decomposition process further reacts with CeO2to generate water-soluble Ce2(SO4)3.
KeyWords AITranslate
1冯兴亮,龙志奇,崔大立,王良士,黄小卫,张国成.焙烧氟碳铈矿硫酸浸出稀土的动力学(英文)[J].中国有色金属学报:英文版,2013,23(3):849-854. 被引量:7
2马莹,赵永志.钕铁硼废料回收方法研究进展[J].稀土信息,2019,0(11):11-15. 被引量:7
3栗健茹,徐存英,卢精灵,王姝羡,付飞娥.从废钕铁硼中湿法回收稀土研究进展[J].湿法冶金,2022,41(2):97-103. 被引量:1
4沈保根.稀土磁性材料[J].科学观察,2017,12(4):27-30. 被引量:6
5严密,金佳莹,马天宇,王新华.新型富La/Ce多主相稀土永磁材料研究[J].金属功能材料,2018,25(1):1-9. 被引量:8
6饶晓雷,钮萼,胡伯平.Ce对烧结钕铁硼磁体永磁性的影响[J].中国材料进展,2017,36(1):63-74. 被引量:5
7李安华,李卫,张月明,冯海波,赵扬,朱明刚.(Ce,RE)-Fe-B永磁材料的研究开发新进展[J].中国稀土学报,2016,34(6):715-725. 被引量:12
8李宇航,邓永春,姜银举,辛文彬,唐家悦,梁雨雨.硫酸化焙烧-选择性分解-水浸法回收铈铁硼废料中稀土[J].稀有金属与硬质合金,2022,50(1):1-5. 被引量:2
9杨瑛,杨汝栋.硫酸铈水合物的热分解行为及动力学研究[J].中国稀土学报,1993,11(4):293-296. 被引量:3
10汪金良,王龙君,刘付朋.基于硫酸减量化从钕铁硼废料中选择性转型分离稀土[J].过程工程学报,2020,20(8):921-928. 被引量:2
1廖伟,陆继长,张迎,刘江平,罗永明,朱文杰.锰氧化物中氧空位的构建及其催化氧化苯系物作用机制研究进展[J].分子催化,2022,36(5):467-479.
2张勇,陈为亮,王凯徽,李钦,何昶浩,廖春发,曾颜亮.铜阳极泥硫酸化焙烧真空蒸硒的研究[J].化学工程,2023,51(8):66-71.
3陈晨,孙志涛,张洪峰.大蒜素通过抑制内质网应激减轻血管性痴呆大鼠海马神经元损伤[J].中南药学,2023,21(7):1827-1832.
4文堪,李耀山,周华荣,刘远,高昭伟,郭辉,刘吉良.中温氯化焙烧—浸出法从废炉砖中提取稀贵金属[J].有色金属工程,2023,13(6):60-65.
5黄泽翎,丁盼,万立会,刘浩,赵雪可,曹鸽,周旭阳,曹玉文.无毛蛋白在乳腺癌变和进展过程中的表达及临床意义[J].安徽医药,2023,27(3):453-457.
6刘春华,门正兴,李艳丽,陈晓辉,张宏.激光选区熔化成形不锈钢板材内部缺陷无损检测可靠性分析[J].锻压技术,2023,48(7):212-221.
7董永贞,陈瑞,吴紫荆,陈翊平,潘晖,刘明军.铂壳金核纳米酶介导的磁弛豫免疫传感器快速检测食源性沙门氏菌[J].食品科学,2023,44(4):337-343. 被引量:1
8李栋,李雅彬,乔晋玺,许志鹏,田庆华,郭学益.从废弃CRT荧光粉中回收稀土的研究[J].中南大学学报:英文版,2023,30(5):1539-1551.
9于剑昆.近年来国内CHPPO工业化技术最新进展(待续)[J].化学推进剂与高分子材料,2023,21(4):17-31.
10杨建东.钕钆变质镁铝基合金的固溶及时效行为[J].西安工程大学学报,2023,37(4):56-63.
Basic Information:
DOI:
Chinese Library Classification Number:TM273[一般工业技术—材料科学与工程]
Citation Information:
A separate CeO2phase appears in the oxidized material of CeFeB waste and changes its valence state during the sulfation roasting process,which differs from NdFeB waste.Therefore,this paper conducted a comparative analysis of the sulfation roasting process of the oxidized materials of these two wastes.The research results show that the highest sulfation rates of the oxidized materials of NdFeB and CeFeB wastes are 91.7%and 96.1%,respectively.The sulfation process of the former mainly occurs in the medium-temperature roasting stage,while that of the latter mainly occurs in the low-temperature infiltration stage with the generation of an intermediate Ce(SO4)2in the medium-temperature roasting stage.The final products of sulfation roasting for both are Fe2O3and RE2(SO4)3.Their high-temperature roasted materials have an loose structure with uneven pore size,and most of the rare earth-rich phases are encapsulated by the non-rare earth phases.Apart from CeO2,the roasting mechanism of the CeFeB waste is consistent with that of the NdFeB waste:rare earth oxides and Fe2O3reacts with sulfuric acid to generate water-soluble rare earth sulfates and Fe2(SO4)3;Fe2SO43is decomposed into Fe2O3and SO3at high temperature,and SO3further reacts with unreacted rare earth oxides to generate rare earth sulfates.CeO2reacts with sulfuric acid to form Ce(SO42at first,which is then decomposed into Ce2(SO4)3.The SO3generated during the decomposition process further reacts with CeO2to generate water-soluble Ce2(SO4)3.
quote
| GB/T 7714-2015 | [1] DENG Yong-chun, YUAN Lu, LI Yu-hang, et al. Comparative Analysis of Sulfation Roasting-Water Leaching Process for Recovery of NdFeB and CeFeB Wastes[J]. Rare Metals and Cemented Carbides, 2023(4): 1-7. |
| MLA | [1] DENG Yong-chun, et al., "Comparative Analysis of Sulfation Roasting-Water Leaching Process for Recovery of NdFeB and CeFeB Wastes." Rare Metals and Cemented Carbides, no. 4, 2023, pp. 1-7. |
| APA | [1] DENG Yong-chun, YUAN Lu, LI Yu-hang, XIN Wen-bin, JIANG Yin-ju, & WANG Liang. (2023). Comparative Analysis of Sulfation Roasting-Water Leaching Process for Recovery of NdFeB and CeFeB Wastes. Rare Metals and Cemented Carbides(4), 1-7. |
| IEEE | [1] DENG Yong-chun, YUAN Lu, LI Yu-hang, XIN Wen-bin, JIANG Yin-ju, and WANG Liang, "Comparative Analysis of Sulfation Roasting-Water Leaching Process for Recovery of NdFeB and CeFeB Wastes," Rare Metals and Cemented Carbides, no. 4, pp. 1-7, 2023. keywords: {NdFeB;CeFeB;waste recovery;sulfation roasting;water leaching;roasting mechanism} |