A thermodynamic description of the Al–Cu–Fe–Mn system for an immiscible medium-entropy alloy design AITranslate

Pohang University of Science and Technology (POSTECH); Pohang University of Science and Technology (POSTECH); Pohang University of Science and Technology (POSTECH); Pohang University of Science and Technology (POSTECH)
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A thermodynamic description of the Al–Cu–Fe–Mn quaternary system has been developed for the design of high-strength immiscible dual-phase medium-entropy alloys. A new thermodynamic assessment for the Al–Cu–Mn ternary sub-system is performed, covering the entire composition range. Thermodynamic parameters of B2 and AlCuFe_τ and φ phases in the Al–Cu–Fe ternary sub-system are also revised based on a previous description that used different constituent binary descriptions. The reliability of the developed thermodynamic description for the Al–Cu–Fe–Mn quaternary system is experimentally confirmed by designing, fabricating, and analysing the phase structures of Al–Cu–Fe–Mn medium-entropy alloys.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.calphad.2020.101995

Chinese Library Classification Number:

Citation Information:

A thermodynamic description of the Al–Cu–Fe–Mn quaternary system has been developed for the design of high-strength immiscible dual-phase medium-entropy alloys. A new thermodynamic assessment for the Al–Cu–Mn ternary sub-system is performed, covering the entire composition range. Thermodynamic parameters of B2 and AlCuFe_τ and φ phases in the Al–Cu–Fe ternary sub-system are also revised based on a previous description that used different constituent binary descriptions. The reliability of the developed thermodynamic description for the Al–Cu–Fe–Mn quaternary system is experimentally confirmed by designing, fabricating, and analysing the phase structures of Al–Cu–Fe–Mn medium-entropy alloys.

quote

GB/T 7714-2015 [1] HyeonSeok Do, Jongun Moon, Hyoung Seop Kim, et al. Calphad, 2020(71). DOI:10.1016/j.calphad.2020.101995.
MLA [1] HyeonSeok Do, et al., Calphad, no. 71, 2020, https://doi.org/10.1016/j.calphad.2020.101995.
APA [1] HyeonSeok Do, Jongun Moon, Hyoung Seop Kim, & ByeongJoo Lee. (2020). Calphad(71). https://doi.org/10.1016/j.calphad.2020.101995
IEEE [1] HyeonSeok Do, Jongun Moon, Hyoung Seop Kim, and ByeongJoo Lee, Calphad, no. 71, 2020, doi: 10.1016/j.calphad.2020.101995.