The spin dynamic process of the IrMn/CoFe system has been investigated by the time-resolved magneto-optical Kerr effect. It is found that both spin pumping and the interfacial exchange spring effect between IrMn and CoFe layers contribute to the total effective Gilbert damping. With the increase in IrMn layer thickness (tIrMn), the saturated damping factor initially increases and subsequently starts to decline beyond 2.4 nm. The results demonstrate that the damping factor drops due to the exchange spring effect in the IrMn/CoFe system, where the IrMn layer features additionally as a spin source when the antiferromagnetic order of the IrMn layer is built at tIrMn > 2.4 nm. With an inserted Cu layer in between, the damping factor behaves differently by remaining nearly constant in a small range with increasing tIrMn after its initial increase. This results from the exchange-decoupling of IrMn and CoFe layers in the presence of a 3 nm thick Cu interlayer and the disappearance of the exchange spring effect.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.3c00215
Chinese Library Classification Number:
Citation Information:
The spin dynamic process of the IrMn/CoFe system has been investigated by the time-resolved magneto-optical Kerr effect. It is found that both spin pumping and the interfacial exchange spring effect between IrMn and CoFe layers contribute to the total effective Gilbert damping. With the increase in IrMn layer thickness (tIrMn), the saturated damping factor initially increases and subsequently starts to decline beyond 2.4 nm. The results demonstrate that the damping factor drops due to the exchange spring effect in the IrMn/CoFe system, where the IrMn layer features additionally as a spin source when the antiferromagnetic order of the IrMn layer is built at tIrMn > 2.4 nm. With an inserted Cu layer in between, the damping factor behaves differently by remaining nearly constant in a small range with increasing tIrMn after its initial increase. This results from the exchange-decoupling of IrMn and CoFe layers in the presence of a 3 nm thick Cu interlayer and the disappearance of the exchange spring effect.
quote
| GB/T 7714-2015 | [1] Yu Liu, Zhihao Ji, Yu Zhang, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00215. |
| MLA | [1] Yu Liu, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00215. |
| APA | [1] Yu Liu, Zhihao Ji, Yu Zhang, Yuna Song, Guangjie Wu, Shitao Lou, Zongzhi Zhang, & Qingyuan Jin. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00215 |
| IEEE | [1] Yu Liu, Zhihao Ji, Yu Zhang, Yuna Song, Guangjie Wu, Shitao Lou, Zongzhi Zhang, and Qingyuan Jin, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00215. keywords: {antiferromagnet exchange spring effect interface Gilbert damping spin pumping} |