Abstract AITranslate
For producing fluorescent-grade low-Cl-Eu2O3, research was made on the ef fects of oxalic acid precipitation conditions (temperature, feeding method etc.) and treat ment methods of the precipitated products on Cl-content in Eu2O3. Optimum technological conditions for production of low-Cl-Eu2O3 have been found.
KeyWords AITranslate
1杨启山,曹艳秋,高丽娟,柳召刚,鲁毅强.高纯氧化铕清洁生产工艺的研究[J].稀土,2008,29(3):64-67. 被引量:7
2田皓,许延辉,张丞,马升峰,刘铃声.从盐酸体系中直接制备低氯根碳酸铈[J].稀土,2016,37(1):98-102. 被引量:7
3曾青云,郭守金,薛丽燕,曾繁钢,王莉.外场辅助制备低氯氧化镧前驱体[J].有色金属科学与工程,2018,9(5):7-13. 被引量:1
1刘夏璐,赵希锦.重金属防控行业开展清洁生产研究[J].科技创新与应用,2012,2(08Z):35-36.
2韩旗英,杨金华,李景芬.高纯氧化铕分离提纯工艺综述[J].湖南有色金属,2012,28(6):26-29. 被引量:2
3王军,李向阳,郝先库,张瑞祥,胡珊珊,马显东.锌与钐的萃取分离工艺研究[J].稀土,2015,36(5):102-106. 被引量:3
4杨德华,刘志强.荧光级氧化铕生产工艺评述[J].材料研究与应用,2016,10(2):75-80. 被引量:1
5王军,郝先库,李向阳,赵永志,马显东,张瑞祥.添加NH_4Cl的洗液对负载有机相中Zn^(2+)洗涤率的影响[J].稀土,2016,37(4):74-80. 被引量:2
6王军,郝先库,李向阳,张瑞祥,赵永志,刘海旺.料液中添加NH_4Cl对Sm^(3+)和Zn^(2+)萃取性能的影响[J].稀土,2017,38(1):13-19. 被引量:3
7张永华,吴锦绣,郭晓晖.降低氧化镨钕中氯根的工艺研究[J].有色金属:冶炼部分,2017(6):58-61. 被引量:3
8曾青云,郭守金,薛丽燕,曾繁钢,王莉.外场辅助制备低氯氧化镧前驱体[J].有色金属科学与工程,2018,9(5):7-13. 被引量:1
9李慧琴,魏迪,刘全,郝先库,张瑞祥,郭瑞华.NH_4HCO_3沉淀分离还原反萃余液中的稀土与锌工艺研究[J].中国稀土学报,2018,36(5):602-607. 被引量:4
10韩旗英,周勇,张魁芳,刘志强,凌诚,韩新福,钟德强.全萃取分离方法生产激光级氧化铕[J].有色金属:冶炼部分,2018(11):56-60.
1毛晓明,朱彤,李加福.使用低氯添加剂改善烧结矿RDI[J].炼铁技术通讯,2004,0(10):2-5.
2冷忠义,许延辉.直接从盐酸介质中制得低氯根碳酸钕[J].稀土信息,1997,3(12):5-5.
3王贵萍,王鸿瑛.荧光级氧化铕除钙工艺试验[J].江西冶金,1996,16(2):35-35. 被引量:1
4杨德华,刘志强.荧光级氧化铕生产工艺评述[J].材料研究与应用,2016,10(2):75-80. 被引量:1
5赵奇金,李日辉,赵德厚,董俊卿.低氯硫酸镍电解液生产镍粉[J].粉末冶金技术,1997,15(3):186-189. 被引量:3
6金世贵.对锅水氯根偏高的几个不能忽视的因素探讨[J].科技创新导报,2010,7(31):67-67.
7代云,徐远志,刁微之,左以专.氧化钴生产过程的非草酸盐沉钴工艺研究之一碳铵(反加)法自氯化钴溶液中沉钴[J].云南冶金,2007,36(3):32-36. 被引量:2
8王瑞哲,孙艳芹,吕庆,吴玮楠,冯帅,本刊编辑部.钒钛矿还原粉化低氯抑制剂的研究[J].河北联合大学学报:自然科学版,2013,35(2):4-6. 被引量:3
9何良东,廖善荣,周秋生,余旭,李栋.低钾低钠低氯高纯仲钨酸铵制备工艺研究[J].中国钨业,2016,31(2):63-67. 被引量:5
10王树忠.高炉煤气中含氯对煤气系统运行的影响[J].冶金动力,2006(5):22-22. 被引量:24
Basic Information:
DOI:
Chinese Library Classification Number:TF845.032[冶金工程—有色金属冶金]
Citation Information:
For producing fluorescent-grade low-Cl-Eu2O3, research was made on the ef fects of oxalic acid precipitation conditions (temperature, feeding method etc.) and treat ment methods of the precipitated products on Cl-content in Eu2O3. Optimum technological conditions for production of low-Cl-Eu2O3 have been found.
quote
| GB/T 7714-2015 | [1] HUANG Shi-yan, ZHOU Shao-hui, ZOU Dong. Research on Preparation of Fluorescent grade Low Cl- Eu_2O_3[J]. Rare Metals and Cemented Carbides, 1997(3): 1-3. |
| MLA | [1] HUANG Shi-yan, et al., "Research on Preparation of Fluorescent grade Low Cl- Eu_2O_3." Rare Metals and Cemented Carbides, no. 3, 1997, pp. 1-3. |
| APA | [1] HUANG Shi-yan, ZHOU Shao-hui, & ZOU Dong. (1997). Research on Preparation of Fluorescent grade Low Cl- Eu_2O_3. Rare Metals and Cemented Carbides(3), 1-3. |
| IEEE | [1] HUANG Shi-yan, ZHOU Shao-hui, and ZOU Dong, "Research on Preparation of Fluorescent grade Low Cl- Eu_2O_3," Rare Metals and Cemented Carbides, no. 3, pp. 1-3, 1997. keywords: {low-Cl^-,fluorescent-grade Eu_2O_3. preparation} |