Preparation of Nd_2O_3 from NdFeB Scraps AITranslate
Abstract AITranslate
Nd2O3 is obtained from NdFeB scraps by H2SO4-double salt process.Laborato ry-scale test shows the process is stable and practicable (purity of obtained Nd2O3>95%,re covery>85%,other techno-economic data are quite satisfactory), and worthy to be popular ized.
KeyWords AITranslate
1陈卫平,杨庆山,何碧宁,刘甲祥.NdFeB废料中钴的回收研究[J].稀有金属与硬质合金,2006,34(2):55-57. 被引量:1
2于利蒙,罗晋如,强文江,乔袆,孙光飞.烧结钕铁硼制备快淬带性能的研究[J].金属功能材料,2008,15(6):1-3.
3肖荣晖.钕铁硼生产中废料的回收及利用[J].有色冶炼,2001,30(1):23-25. 被引量:26
4江泽佐,钟春兰,卢阶主,张亮玖.钕铁硼回收料盐酸优溶液氯酸钠氧化法除铁[J].化工技术与开发,2018,47(8):55-57. 被引量:6
5卢阶主,羊多彦.钕铁硼回收料盐酸优溶液氧化法除铁[J].湖南有色金属,2019,35(2):27-29. 被引量:4
6汪金良,刘兴润.钕铁硼废料焙砂的碳热还原试验研究[J].中国稀土学报,2019,37(1):84-90. 被引量:3
1唐杰,杨梨容,赵导文,张林,刘畅.烧结Nd-Fe-B磁体废料回收Nd2O3的方法研究[J].稀有金属与硬质合金,2020(1):5-8.
2黄劲松,齐美富.钕铁硼废料资源化利用工艺综述[J].中国资源综合利用,2008,26(11):4-5. 被引量:12
3唐杰,魏成富,赵导文,林红,田桂华.烧结钕铁硼废料中Nd2O3的回收[J].稀有金属与硬质合金,2009,37(1):9-11. 被引量:14
4许涛,彭会清,林忠,吕保义.稀土固体废物的成因、成分分析及综合利用[J].稀土,2010,31(2):34-39. 被引量:25
5魏成富,代强,唐杰,杨梨容,李想,张林.硫酸复盐法回收NdFeB废料中含铁水的处理[J].绵阳师范学院学报,2010,29(5):38-40. 被引量:8
6张雪峰,王大鹏,张倩.钕铁硼废料回收利用[J].科技创新导报,2012,9(13):149-150. 被引量:10
7廖春生,吴声,王嵩龄,程福祥,张玻,严纯华.引入阻断剂的硫酸稀土皂化萃取工艺研究[J].中国稀土学报,2012,30(5):533-537. 被引量:1
8董传博,刘敏,赖伟鸿,尹小文,王雁,岳明,索红莉.硫化物除杂法回收钕铁硼废料中稀土元素的研究[J].硅酸盐通报,2013,32(10):2127-2132. 被引量:4
9尹小文,刘敏,赖伟鸿,董传博,岳明,索红莉.草酸盐沉淀法回收钕铁硼废料中稀土元素的研究[J].稀有金属,2014,38(6):1093-1098. 被引量:17
10刘开明.钕铁硼废料中钴的回收试验条件研究[J].中国建材科技,2015,24(4):45-46. 被引量:1
1陈大林,马玉天,张燕,杨万虎,陈治毓.从金还原后液中提取金、钯的工艺研究[J].贵金属,2013,34(S01):8-12.
2攀钢研究院成功攻克细粒级钛精矿高效成型难题[J].新材料产业,2017,0(3):94-94.
3杨丹,刘永平,曾青云.常压下微波辅助还原法制备纳米氧化亚铜[J].湿法冶金,2010,29(1):29-31. 被引量:4
4大吨位毒死蜱工艺开发获突破[J].山东农药信息,2008(4):16-16.
5大吨位毒死蜱工艺开发获突破[J].杭州化工,2008,38(1):46-46.
6姜书凯.大吨位毒死蜱工艺开发获突破[J].农药市场信息,2008(17):33-33.
7汤培平,徐敏,王宝璐,李竟菲,陈云霞,朱丽,刘宏宇.冶金法制备太阳能硅过程的湿法提纯研究[J].精细化工,2009,26(8):733-737. 被引量:9
8栾广英,杜德胜.简介影响三筒湿式振动球磨机磨矿效果的因素[J].中国钨业,1995,0(8):19-20.
9田君,赵庆芳,尹敬群,蔡恒亮,陈曙生,程荣辉.用环烷酸石油亚砜从混合氯化稀土溶液中萃取分离钇[J].湿法冶金,2001,20(1):37-40. 被引量:4
10汤培平,陈云霞,徐敏,朱丽,刘宏宇,王文宾.冶金法制备太阳能硅过程的湿法除硼研究[J].化学工程,2010,38(11):68-71. 被引量:10
Basic Information:
DOI:
Chinese Library Classification Number:TF845.032[冶金工程—有色金属冶金]
Citation Information:
Nd2O3 is obtained from NdFeB scraps by H2SO4-double salt process.Laborato ry-scale test shows the process is stable and practicable (purity of obtained Nd2O3>95%,re covery>85%,other techno-economic data are quite satisfactory), and worthy to be popular ized.
quote
| GB/T 7714-2015 | [1] LIN He-cheng. Preparation of Nd_2O_3 from NdFeB Scraps[J]. Rare Metals and Cemented Carbides, 1997(3): 4-7. |
| MLA | [1] LIN He-cheng. "Preparation of Nd_2O_3 from NdFeB Scraps." Rare Metals and Cemented Carbides, no. 3, 1997, pp. 4-7. |
| APA | [1] LIN He-cheng. (1997). Preparation of Nd_2O_3 from NdFeB Scraps. Rare Metals and Cemented Carbides(3), 4-7. |
| IEEE | [1] LIN He-cheng, "Preparation of Nd_2O_3 from NdFeB Scraps," Rare Metals and Cemented Carbides, no. 3, pp. 4-7, 1997. keywords: {NdFeB, Nd_2O_3, preparation} |