Band Alignment and Optical Properties of 1D/2D Sb2Se3/PtSe2 Heterojunctions AITranslate

Institute of Chemical Engineering Sciences (FORTH/ICE-HT); Institute of Chemical Engineering Sciences (FORTH/ICE-HT);Univ Rennes;Univ Rennes;Univ Rennes; Institute of Chemical Engineering Sciences (FORTH/ICE-HT)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The heterojunction between two materials brought into contact, for example, in the form of vertical van der Waals heterostructures, exhibits interesting features offering functionalities to devices stimulated by light. We report in this article an investigation of the optical and electronic properties of the heterojunction formed between Sb2Se3, a material with a promising role in photovoltaics characterized by one-dimensional (1D) topology (ribbons), and an emerging two-dimensional (2D) material, PtSe2, exhibiting unique optical properties for photoelectronics and photonics. The controlled growth of PtSe2 on Sb2Se3 underlayer takes place using a transfer-free process by low-temperature selenization of 1–2 nm Pt films thermally evaporated on Sb2Se3 ultrathin substrates. X-ray photoelectron spectroscopy (XPS) data analyzed in the context of the Kraut method provided an estimate for the band offsets at the interface. The valence band offset and the conduction band offset of the PtSe2/Sb2Se3 heterojunction were found to be −0.25 and 1.0 eV, respectively, indicating a type-II heterojunction. The ultrabroad optical absorption of the heterojunction and the protection offered by PtSe2 to Sb2Se3, against oxidation of the latter, render this particular heterojunction a robust candidate for applications in photovoltaics. Finally, the current study of a heterojunction between materials of different dimensionalities may pave the way for a rational design in the field of trans-dimensional heterostructures.

KeyWords AITranslate

PtSe2 Sb2Se3 typeII heterostructure band alignment selfpowered photodetector thermally assisted conversion (TAC)
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c00541

Chinese Library Classification Number:

Citation Information:

The heterojunction between two materials brought into contact, for example, in the form of vertical van der Waals heterostructures, exhibits interesting features offering functionalities to devices stimulated by light. We report in this article an investigation of the optical and electronic properties of the heterojunction formed between Sb2Se3, a material with a promising role in photovoltaics characterized by one-dimensional (1D) topology (ribbons), and an emerging two-dimensional (2D) material, PtSe2, exhibiting unique optical properties for photoelectronics and photonics. The controlled growth of PtSe2 on Sb2Se3 underlayer takes place using a transfer-free process by low-temperature selenization of 1–2 nm Pt films thermally evaporated on Sb2Se3 ultrathin substrates. X-ray photoelectron spectroscopy (XPS) data analyzed in the context of the Kraut method provided an estimate for the band offsets at the interface. The valence band offset and the conduction band offset of the PtSe2/Sb2Se3 heterojunction were found to be −0.25 and 1.0 eV, respectively, indicating a type-II heterojunction. The ultrabroad optical absorption of the heterojunction and the protection offered by PtSe2 to Sb2Se3, against oxidation of the latter, render this particular heterojunction a robust candidate for applications in photovoltaics. Finally, the current study of a heterojunction between materials of different dimensionalities may pave the way for a rational design in the field of trans-dimensional heterostructures.

quote

GB/T 7714-2015 [1] Kapil Bhorkar, Labrini Sygellou, Michel Cathelinaud, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00541.
MLA [1] Kapil Bhorkar, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00541.
APA [1] Kapil Bhorkar, Labrini Sygellou, Michel Cathelinaud, Donglou Ren, JeanLuc Adam, & Spyros N. Yannopoulos. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00541
IEEE [1] Kapil Bhorkar, Labrini Sygellou, Michel Cathelinaud, Donglou Ren, JeanLuc Adam, and Spyros N. Yannopoulos, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c00541. keywords: {PtSe2 Sb2Se3 typeII heterostructure band alignment selfpowered photodetector thermally assisted conversion (TAC)}