Effect of Heat Treatment on Microstructure and Hardness of AlCrFeNiTi High Entropy Alloy AITranslate
Abstract AITranslate
AlCrFeNiTi high entropy alloy was prepared by vacuum arc melting in argon atmosphere.The influences were investigated of heating temperature,holding time and cooling methods on microstructure and hardness of AlCrFeNiTi high entropy alloy with methods of X-ray diffraction,metalloscope and Vickers hardness tester.The results show that the as-cast AlCrFeNiTi high entropy alloy is composed of two kinds of solid solutions with different body centered cubic structure,forming typical high entropy alloy microstructure of dendrite,interdendrite,andα+βeutectic.With the increase of heating temperature,the dendrite phase experiences a process of first coarsening and subsequent refinement at 900℃.As the holding time increases and cooling rate decreases,the microstructures of dendrite and interdendrite coarsen,but the hardness of alloy shows tendency to ascend.The hardness of alloy after heat treatment depends on the content and morphology of dendrite phase,and meanwhile the residual internal stress also play an important role in the hardness of the alloy cooled at high speed.
KeyWords AITranslate
1刘源,李言祥,陈祥,陈敏.多主元高熵合金研究进展[J].材料导报,2006,20(4):4-6. 被引量:80
2洪丽华,张华,唐群华,温建程,戴品强.Al_(0.5)CrCoFeNi高熵合金高温氧化的研究[J].稀有金属材料与工程,2015,44(2):424-428. 被引量:14
3赵春凤,吴波,杨上金,周泽友,熊远鹏,陈祖华.热处理工艺对AlCoCrFeNiTi_(0.5)高熵合金的显微组织和硬度的影响[J].广西大学学报:自然科学版,2014,39(2):407-416. 被引量:7
4谢红波,刘贵仲,郭景杰,毛炜乾,郝聪敏.回火工艺对AlFeCrCoCu高熵合金组织及耐蚀性能的影响研究[J].稀有金属与硬质合金,2015,43(4):51-56. 被引量:6
1张微,刘亮,商剑,赵作福,张越,齐锦刚,王冰.磁控溅射AlCrFeNiTi高熵合金薄膜的组织和表面形貌[J].电镀与涂饰,2021,40(19):1489-1493. 被引量:3
2张晓蓉,尚华龙.退火对AlCuFeNiTiCr_(x)高熵合金硬度的影响[J].金属热处理,2023,48(2):170-173.
3王子玥,郭敏,于雪,姜小丹,农智升,朱景川.退火对Al_(1.5)CrCuFeMnTi高熵合金组织和硬度的影响[J].稀有金属与硬质合金,2019,47(2):15-21. 被引量:2
1章奇,李忠文,于治水.光纤激光器制备FeNiMoCoCrTi高熵合金过程与研究综述[J].电子科技,2021,34(7):67-72.
2秦海宁,张伟强,柳泉,周新雨,杨尔其.磁控溅射制备高熵氧化物薄膜的阻挡扩散性能[J].电镀与涂饰,2022,41(9):641-646.
3雷声,胡正强,申家升,刘亚峰,薛正伟,张翔.退火温度对FeCoCrNiTi高熵合金组织及性能的影响[J].材料热处理学报,2022,43(12):83-90.
4程驰,郭朝乾,李海庆,李剑微,曲帅杰,张程,林松盛.物理气相沉积制备高熵氮化物涂层的进展[J].电镀与涂饰,2023,42(3):40-49. 被引量:1
5王彦龙,张旭东,党步裕,高淼,徐洁.不同溅射功率下CoCrFeNiCu高熵合金涂层的耐腐蚀及其抗氧化性能[J].西安工程大学学报,2023,37(4):48-55.
1陈婵娟.马氏体不锈钢的CO_2气体保护焊[J].热加工工艺,2012,41(21):231-232. 被引量:2
2任英磊,金涛,管恒荣,胡壮麒.固溶处理对1种镍基单晶高温合金组织的影响[J].稀有金属材料与工程,2003,32(4):287-290. 被引量:6
3胡海明,吕乐扬,刘勇.Al-Ti-B变质剂对ZA27合金组织及性能的影响[J].机械工程材料,1997,21(6):23-25. 被引量:3
4古东懂,韩宝军,何琼.Mg-Gd-Y-Nd-Zr合金的时效热处理工艺优化[J].特种铸造及有色合金,2015,35(6):659-662. 被引量:3
5张观杰,刘海林,曾茵,朱绍严.固溶时间及后处理工艺对镁合金组织和耐腐蚀性能的影响[J].热加工工艺,2015,44(20):162-164. 被引量:3
6冯剑,黄金亮,贾玉鑫.轧制变形对Mg-12Li-3Gd-3Y-0.6Zr合金组织与性能的影响[J].热加工工艺,2014,43(4):74-76. 被引量:4
7陆世英.不锈钢概论(11)[J].不锈:市场与信息,2010(18):18-19.
8顾建,符寒光,雷永平.回火工艺对含硼中碳高铬铸铁组织与性能的影响[J].材料热处理学报,2013,34(9):107-111. 被引量:2
9张洪.30CrMnSiA钢制组件真空热处理工艺研究[J].机械工人:热加工,2006,30(9):40-40.
10薛小怀,钱百年,国旭明,楼松年.氩气保护对埋弧焊焊缝氧氮含量和冲击韧性的影响[J].机械工程材料,2003,27(3):27-29. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TG113[金属学及工艺—物理冶金]
Citation Information:
AlCrFeNiTi high entropy alloy was prepared by vacuum arc melting in argon atmosphere.The influences were investigated of heating temperature,holding time and cooling methods on microstructure and hardness of AlCrFeNiTi high entropy alloy with methods of X-ray diffraction,metalloscope and Vickers hardness tester.The results show that the as-cast AlCrFeNiTi high entropy alloy is composed of two kinds of solid solutions with different body centered cubic structure,forming typical high entropy alloy microstructure of dendrite,interdendrite,andα+βeutectic.With the increase of heating temperature,the dendrite phase experiences a process of first coarsening and subsequent refinement at 900℃.As the holding time increases and cooling rate decreases,the microstructures of dendrite and interdendrite coarsen,but the hardness of alloy shows tendency to ascend.The hardness of alloy after heat treatment depends on the content and morphology of dendrite phase,and meanwhile the residual internal stress also play an important role in the hardness of the alloy cooled at high speed.
quote
| GB/T 7714-2015 | [1] CUI Pu-chang, ZHANG Yi-ming, FU Sheng, et al. Effect of Heat Treatment on Microstructure and Hardness of AlCrFeNiTi High Entropy Alloy[J]. Rare Metals and Cemented Carbides, 2017(1): 52-57. |
| MLA | [1] CUI Pu-chang, et al., "Effect of Heat Treatment on Microstructure and Hardness of AlCrFeNiTi High Entropy Alloy." Rare Metals and Cemented Carbides, no. 1, 2017, pp. 52-57. |
| APA | [1] CUI Pu-chang, ZHANG Yi-ming, FU Sheng, LUAN Tian, & NONG Zhi-sheng. (2017). Effect of Heat Treatment on Microstructure and Hardness of AlCrFeNiTi High Entropy Alloy. Rare Metals and Cemented Carbides(1), 52-57. |
| IEEE | [1] CUI Pu-chang, ZHANG Yi-ming, FU Sheng, LUAN Tian, and NONG Zhi-sheng, "Effect of Heat Treatment on Microstructure and Hardness of AlCrFeNiTi High Entropy Alloy," Rare Metals and Cemented Carbides, no. 1, pp. 52-57, 2017. keywords: {AlCrFeNiTi high entropy alloy;heat treatment;microstructure;hardness;dendrite;interdendrite;α+βeutectic microstructure} |