Bottom-Up Strategy Toward 3D Porous MXene/MoS2 Nanosheets/Graphene Nanoarchitectures as Highly-Efficient Hydrogen Evolution Electrocatalysts AITranslate

AITranslate
Publisher: Youke Publish Co., Ltd.
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

As a core component in the electrochemical water splitting system, the cathode catalyst is capable of boosting the kinetics of the hydrogen evolution reaction (HER), while the scarcity and expenditure of current noble metal-based electrocatalysts seriously restrict the large-scale commercial development of hydrogen manufacturing devices. Here, we present a robust and controllable self-assembly method for the spatial construction of three-dimensional (3D) porous ternary nanoarchitectures comprising Ti3C2Tx MXene, MoS2 nanosheets, and graphene (MX/MoS2/G). This bottom-up strategy contributes to the intriguing structural features of the resulting nanoarchitectures, including 3D crosslinked porous networks, ultrathin walls, plentiful exposed reactive sites, and numerous efficient electron channels. As a consequence, the optimized MX/MoS2/G electrocatalyst depicts superior electrocatalytic HER performance in terms of a competitive onset potential, a small Tafel slope, a large electrochemically active surface area, and exceptional durability, which significantly outperforms the bare MXene, MoS2, graphene, as well as binary MXene/graphene and MoS2/graphene electrocatalysts.

KeyWords AITranslate

3D graphene electrocatalyst hydrogen evolution MoS2 nanosheets Ti3C2Tx MXene
No data

Basic Information:

DOI:

Chinese Library Classification Number:

Citation Information:

As a core component in the electrochemical water splitting system, the cathode catalyst is capable of boosting the kinetics of the hydrogen evolution reaction (HER), while the scarcity and expenditure of current noble metal-based electrocatalysts seriously restrict the large-scale commercial development of hydrogen manufacturing devices. Here, we present a robust and controllable self-assembly method for the spatial construction of three-dimensional (3D) porous ternary nanoarchitectures comprising Ti3C2Tx MXene, MoS2 nanosheets, and graphene (MX/MoS2/G). This bottom-up strategy contributes to the intriguing structural features of the resulting nanoarchitectures, including 3D crosslinked porous networks, ultrathin walls, plentiful exposed reactive sites, and numerous efficient electron channels. As a consequence, the optimized MX/MoS2/G electrocatalyst depicts superior electrocatalytic HER performance in terms of a competitive onset potential, a small Tafel slope, a large electrochemically active surface area, and exceptional durability, which significantly outperforms the bare MXene, MoS2, graphene, as well as binary MXene/graphene and MoS2/graphene electrocatalysts.

quote

GB/T 7714-2015 [1] Bottom-Up Strategy Toward 3D Porous MXene/MoS2 Nanosheets/Graphene Nanoarchitectures as Highly-Efficient Hydrogen Evolution Electrocatalysts[J]. Rare Metals, 2026(3).
MLA [1] "Bottom-Up Strategy Toward 3D Porous MXene/MoS2 Nanosheets/Graphene Nanoarchitectures as Highly-Efficient Hydrogen Evolution Electrocatalysts." Rare Metals, no. 3, 2026.
APA [1] (2026). Bottom-Up Strategy Toward 3D Porous MXene/MoS2 Nanosheets/Graphene Nanoarchitectures as Highly-Efficient Hydrogen Evolution Electrocatalysts. Rare Metals(3).
IEEE [1] "Bottom-Up Strategy Toward 3D Porous MXene/MoS2 Nanosheets/Graphene Nanoarchitectures as Highly-Efficient Hydrogen Evolution Electrocatalysts," Rare Metals, no. 3, 2026. keywords: {3D graphene;electrocatalyst;hydrogen evolution;MoS2 nanosheets;Ti3C2Tx MXene}