daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Polyimide Aerogels as Lightweight Dielectric Insulators for Carbon Nanotube Cables AITranslate

Ohio Aerospace Institute;Rice University;Ohio Aerospace Institute;NASA Glenn Research Center, 21000 Brookpark Road;Rice University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Replacing copper as the central conductor with carbon nanotube (CNT) yarn has potential for greatly reducing the weight of data and power cables for any number of aerospace and automotive applications. Polyimide aerogels, with lightweight and low dielectric constants approaching one, have promise to even further reduce the weight of the cable as the dielectric insulation layer. In this paper, polyimide aerogels containing 4,4′-bis(4-aminophenoxy)biphenyl (BAPB) in the backbone and two different cross-linkers (1,3,5-triaminophenoxybenzene, TAB, or poly(isobutylene-alt-maleic anhydride), PMA-D) were examined as potential coatings on CNT yarns. The effects of polyimide concentration and different solvent combinations on the quality of the coating were also examined. The best quality coatings were obtained with aerogels made by using PMA-D as the cross-linker, high polymer concentration, and a mixture of solvents. This work demonstrates the feasibility of using polyimide aerogels as the dielectric layer for lightweight CNT data and power cables. More improvements need to be made in the future, including scale up of the coating process, coating quality, and durability.

KeyWords AITranslate

lightweight dielectric insulator cables CNT yarns polyimide aerogel BAPB
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00241

Chinese Library Classification Number:

Citation Information:

Replacing copper as the central conductor with carbon nanotube (CNT) yarn has potential for greatly reducing the weight of data and power cables for any number of aerospace and automotive applications. Polyimide aerogels, with lightweight and low dielectric constants approaching one, have promise to even further reduce the weight of the cable as the dielectric insulation layer. In this paper, polyimide aerogels containing 4,4′-bis(4-aminophenoxy)biphenyl (BAPB) in the backbone and two different cross-linkers (1,3,5-triaminophenoxybenzene, TAB, or poly(isobutylene-alt-maleic anhydride), PMA-D) were examined as potential coatings on CNT yarns. The effects of polyimide concentration and different solvent combinations on the quality of the coating were also examined. The best quality coatings were obtained with aerogels made by using PMA-D as the cross-linker, high polymer concentration, and a mixture of solvents. This work demonstrates the feasibility of using polyimide aerogels as the dielectric layer for lightweight CNT data and power cables. More improvements need to be made in the future, including scale up of the coating process, coating quality, and durability.

quote

GB/T 7714-2015 [1] Haiquan Guo, Oliver S. Dewey, Linda S. McCorkle, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00241.
MLA [1] Haiquan Guo, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00241.
APA [1] Haiquan Guo, Oliver S. Dewey, Linda S. McCorkle, Mary Ann B. Meador, & Matteo Pasquali. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00241
IEEE [1] Haiquan Guo, Oliver S. Dewey, Linda S. McCorkle, Mary Ann B. Meador, and Matteo Pasquali, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00241. keywords: {lightweight;dielectric insulator;cables;CNT yarns;polyimide aerogel;BAPB}