daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Silicone Elastomer with Surface-Enriched, Nonleaching Amphiphilic Side Chains for Inhibiting Marine Biofouling AITranslate

South China University of Technology; South China University of Technology; South China University of Technology; South China University of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Silicone elastomer is one of the ecofriendly fouling release materials. However, it suffers from poor fouling resistant performance during idle periods. We developed a silicone elastomer with self-stratifying, nonleaching amphiphilic side chains by grafting telomer of dodecafluoroheptyl methacrylate (DFMA), poly(ethylene glycol) methyl ether methacrylate (PEGMA), and 3-mercaptopropyl trimethoxysilane (KH590) to bis-silanol terminated silicone. The amphiphilic telomer can be self-enriched on the surface during coating formation because the fluorocarbon segment with low surface energy is incompatible with silicone. Meanwhile, the telomer with KH590 can cross-link to silicone so that it is nonleaching. Such modified silicone elastomer has a low surface energy and low elastic modulus close to the unmodified one because most of the amphiphilic telomers are on the surface, so the former as a coating still has excellent fouling release performance. Moreover, it has remarkable fouling resistance toward marine bacterial biofilm and diatoms under a suitable molar ratio of DFMA and PEGMA (GF1P2). Such a modified silicone elastomer is expected to find application to inhibit marine biofouling.

KeyWords AITranslate

silicone elastomer amphiphiles telomerization marine biofouling fouling release
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.9b00253

Chinese Library Classification Number:

Citation Information:

Silicone elastomer is one of the ecofriendly fouling release materials. However, it suffers from poor fouling resistant performance during idle periods. We developed a silicone elastomer with self-stratifying, nonleaching amphiphilic side chains by grafting telomer of dodecafluoroheptyl methacrylate (DFMA), poly(ethylene glycol) methyl ether methacrylate (PEGMA), and 3-mercaptopropyl trimethoxysilane (KH590) to bis-silanol terminated silicone. The amphiphilic telomer can be self-enriched on the surface during coating formation because the fluorocarbon segment with low surface energy is incompatible with silicone. Meanwhile, the telomer with KH590 can cross-link to silicone so that it is nonleaching. Such modified silicone elastomer has a low surface energy and low elastic modulus close to the unmodified one because most of the amphiphilic telomers are on the surface, so the former as a coating still has excellent fouling release performance. Moreover, it has remarkable fouling resistance toward marine bacterial biofilm and diatoms under a suitable molar ratio of DFMA and PEGMA (GF1P2). Such a modified silicone elastomer is expected to find application to inhibit marine biofouling.

quote

GB/T 7714-2015 [1] Haohang Zeng, Qingyi Xie, Chunfeng Ma, et al. ACS Applied Polymer Materials, 2019(1). DOI:10.1021/acsapm.9b00253.
MLA [1] Haohang Zeng, et al., ACS Applied Polymer Materials, no. 1, 2019, https://doi.org/10.1021/acsapm.9b00253.
APA [1] Haohang Zeng, Qingyi Xie, Chunfeng Ma, & Guangzhao Zhang. (2019). ACS Applied Polymer Materials(1). https://doi.org/10.1021/acsapm.9b00253
IEEE [1] Haohang Zeng, Qingyi Xie, Chunfeng Ma, and Guangzhao Zhang, ACS Applied Polymer Materials, no. 1, 2019, doi: 10.1021/acsapm.9b00253. keywords: {silicone elastomer;amphiphiles;telomerization;marine biofouling;fouling release}