Research on Hot Filament Arrangement in Diamond Film Deposition on Cemented Carbide Tools with Complicated Shape AITranslate

School of Mechanical and Power Engineering, Henan University of Technology;School of Mechanical and Power Engineering, Henan University of Technology;School of Mechanical and Power Engineering, Henan University of Technology;School of Mechanical and Power Engineering, Henan University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Characteristics were comparatively analyzed of common hot-filament arrangement in hot-filament chemical vapor deposition of diamond films on cemented carbide tools with complicated shape.Then diamond films were deposited on YG6 cemented carbide drill surface by ultrasound-assisted acid-alkali pretreatment and parallel arrangement of single-row two filaments with the optimized deposition process.Surface quality of diamond films was tested by microscopic examination and drilling experiments were performed on carbon fiber reinforced epoxy resin matrix composites to analyze wear morphology of the coated tools and access quality of the drilled holes.The results show that diamond films can be deposited uniformly on cutting edge with improved filament arrangement method.Diamond films exhibit good adhesion during drilling,and reduce tool wear and burr and edge failure in the access of the drilled holes to a certain extent.

KeyWords AITranslate

diamond film coating cemented carbide tool with complicated shape hot-filament chemical vapor deposition hot-filament arrangement drilling

1薛宏国,孙方宏,马玉平,陈明.高性能超细晶粒金刚石涂层刀具制备及试验研究[J].人工晶体学报,2006,35(6):1251-1256. 被引量:7

2沈彬,孙方宏,张志明,沈荷生,郭松寿.CVD金刚石薄膜涂层整体式刀具的制备与应用[J].金刚石与磨料磨具工程,2011,31(1):1-5. 被引量:16

3唐璧玉,靳九成.灯丝形变对金刚石薄膜沉积的影响[J].人工晶体学报,1996,25(4):339-342. 被引量:2

4孙心瑗,周灵平,李宇农,余晓光.热丝CVD法沉积金刚石薄膜用灯丝研究现状及改进[J].粉末冶金工业,2005,15(6):26-32. 被引量:4

5刘海涛,向道辉,杨广斌,梁松,马德印.热丝CVD金刚石涂层硬质合金衬底两步法预处理的研究[J].金刚石与磨料磨具工程,2012,32(6):25-28. 被引量:9

6张骋,徐锋,赵云,左敦稳.硬质合金刀具金刚石涂层的热应力仿真[J].机械制造与自动化,2011,40(6):100-104. 被引量:2

7孙方宏,陈明,张志明,沈荷生.高性能CVD金刚石薄膜涂层刀具的制备和试验研究[J].机械工程学报,2003,39(7):101-106. 被引量:25

1万松峰,陈永刚,丁佳伟.(AlCrNbSiTiV)N高熵合金氮化薄膜溅镀参数的灰关联分析优化[J].电镀与涂饰,2020,39(1):20-25.

2李晓刚,黎子辉,叶俊文.基于文献数据可视化的真空镀膜技术研究与应用分析[J].真空科学与技术学报,2022,42(11):863-875.

1许幸新,张晓辉,张春林,郑友益.复杂形状硬质合金刀具金刚石涂层的制备及铣削特性研究[J].稀有金属与硬质合金,2014,42(3):63-68. 被引量:1

2唐华生.金刚石薄膜涂层技术的发展[J].润滑与密封,1990(5):58-61.

3宋亚林,程敏.热丝化学气相沉积(HFCVD)制备金刚石薄膜涂层刀具[J].鄂州大学学报,2013,20(3):78-80. 被引量:5

4赵齐,代明江,韦春贝,邱万奇,侯惠君.钨丝到基体表面距离对HFCVD金刚石薄膜质量的影响[J].材料导报,2013,27(22):22-25. 被引量:2

5黄世平.磷化工艺对钢铁件磷化膜的影响[J].变压器,1989,26(10):38-39.

6李建国,刘实,李依依,胡东平,李军,周德惠.热丝法气相沉积金刚石薄膜的影响因素[J].金刚石与磨料磨具工程,2004,24(1):41-44. 被引量:5

7杨海东,孔晓玲,韦山.金刚石涂层刀具干切削硅铝合金性能研究[J].合肥工业大学学报:自然科学版,2003,26(6):1276-1278. 被引量:11

8赵齐,代明江,韦春贝,邱万奇,侯惠君,谭笛.厚钛过渡层缓解铜基上热丝CVD金刚石薄膜内应力[J].表面技术,2013,42(5):19-23. 被引量:4

9简小刚,朱正宇,雷强.热丝CVD金刚石涂层膜基界面结合强度研究新进展[J].金刚石与磨料磨具工程,2016,36(3):11-16. 被引量:2

10宋波,沈彬,雷学林,程雷,孙方宏.大批量微细刀具HFCVD涂层制备的温度场仿真与试验分析[J].真空科学与技术学报,2015,35(2):166-173.

Basic Information:

DOI:

Chinese Library Classification Number:TG174.444[金属学及工艺—金属表面处理]

Citation Information:

Characteristics were comparatively analyzed of common hot-filament arrangement in hot-filament chemical vapor deposition of diamond films on cemented carbide tools with complicated shape.Then diamond films were deposited on YG6 cemented carbide drill surface by ultrasound-assisted acid-alkali pretreatment and parallel arrangement of single-row two filaments with the optimized deposition process.Surface quality of diamond films was tested by microscopic examination and drilling experiments were performed on carbon fiber reinforced epoxy resin matrix composites to analyze wear morphology of the coated tools and access quality of the drilled holes.The results show that diamond films can be deposited uniformly on cutting edge with improved filament arrangement method.Diamond films exhibit good adhesion during drilling,and reduce tool wear and burr and edge failure in the access of the drilled holes to a certain extent.

quote

GB/T 7714-2015 [1] XU Xing-xin, ZHANG Xiao-hui, XIANG Dao-hui, et al. Research on Hot Filament Arrangement in Diamond Film Deposition on Cemented Carbide Tools with Complicated Shape[J]. Rare Metals and Cemented Carbides, 2016(6): 68-72.
MLA [1] XU Xing-xin, et al., "Research on Hot Filament Arrangement in Diamond Film Deposition on Cemented Carbide Tools with Complicated Shape." Rare Metals and Cemented Carbides, no. 6, 2016, pp. 68-72.
APA [1] XU Xing-xin, ZHANG Xiao-hui, XIANG Dao-hui, & ZHAO Bo. (2016). Research on Hot Filament Arrangement in Diamond Film Deposition on Cemented Carbide Tools with Complicated Shape. Rare Metals and Cemented Carbides(6), 68-72.
IEEE [1] XU Xing-xin, ZHANG Xiao-hui, XIANG Dao-hui, and ZHAO Bo, "Research on Hot Filament Arrangement in Diamond Film Deposition on Cemented Carbide Tools with Complicated Shape," Rare Metals and Cemented Carbides, no. 6, pp. 68-72, 2016. keywords: {diamond film;coating;cemented carbide tool with complicated shape;hot-filament chemical vapor deposition;hot-filament arrangement;drilling}