Research Status of Tungsten Slag Recycling Technology AITranslate
Abstract AITranslate
China is a large country of tungsten industry, but there is a lack of effective industrialized treatment methods for tungsten slag.With the extensive exploitation of tungsten ore, the traditional landfill method is no longer suitable for the treatment of existing tungsten slag, resulting in the continuous accumulation of tungsten slag.At the same time, heavy metals in tungsten slag have caused serious environmental pollution.In view of these problems, many scholars are committed to solving the problem of tungsten slag accumulation and have carried out a lot of research to comprehensively recover and utilize the va-luable metals in tungsten slag.This paper summarizes the research progress on the recovery and utilization technology of tungsten slag at home and abroad in recent years, which is mainly divided into the recovery of valuable metals in tungsten slag and the use of tungsten slag to make special materials.Finally, the deve-lopment trend of tungsten slag recycling is prospected.
KeyWords AITranslate
1杨运光,万林生,龚丹丹.粗钨酸钠溶液深度脱磷工业试验研究[J].稀有金属与硬质合金,2019,47(4):1-6. 被引量:3
2袁博,李钟山,刘良先,柳群义,孙立楠,赵敏.我国钨资源储备规划形势分析[J].中国矿业,2016,25(1):15-18. 被引量:23
3李俊杰,何德文,周康根,龚丹丹.钨渣综合利用研究现状[J].矿产保护与利用,2019,39(3):125-132. 被引量:8
4陈林,杨延梅,杨玉飞,杨金忠,黄启飞.钨渣综合利用产生固体废物的污染特性[J].环境污染与防治,2015,37(12):66-70. 被引量:9
5杨金忠,高何凤,王宁,陈林,王健媛,杨玉飞.仲钨酸铵(APT)生产中钨渣的污染特性分析[J].环境工程技术学报,2015,5(6):525-530. 被引量:14
6戴艳阳,钟海云,李荐,钟晖.钨渣中有价金属综合回收工艺[J].中南工业大学学报,2003,34(1):36-39. 被引量:24
7戴艳阳,钟晖,钟海云.酸浸法从钨渣中回收铌、钽、钨[J].桂林工学院学报,2008,28(2):193-195. 被引量:9
8范泽坤,黄超,徐国钻,杨正锋,胡家园,唐孝江,梁勇.钨冶炼渣酸分解减量资源化实验研究[J].稀有金属与硬质合金,2020,48(2):1-4. 被引量:4
9杨利群.苏打烧结法处理低品位钨矿及废钨渣的研究[J].中国钼业,2008,32(4):25-27. 被引量:31
10杨少华,王君,谢宝如,赖晓晖,王浩然.低品位钨渣处理工艺[J].有色金属科学与工程,2015,6(6):29-32. 被引量:10
1彭伟,黄健,王振杰,刘安荣.钨冶炼渣中有价金属回收利用研究现状[J].化工进展,2022,41(12):6656-6663.
2李祖怡,张勇,郑彬涛,侯志明,龚丹丹.碱分解钨渣硫酸浸出的正交试验研究[J].稀有金属与硬质合金,2023,51(1):1-4.
1李立松.固态废物无害化处理技术研究[J].山西化工,2021,41(6):198-200.
2冯羽生,徐水太,许礼刚,闫光礼.产业集群视角下江西钨产业可持续发展的问题与对策研究[J].有色金属科学与工程,2021,12(5):103-109. 被引量:2
3张青鹏,李景杨.关于陈腐垃圾资源化利用的研究探讨[J].清洗世界,2021,37(12):140-142.
Basic Information:
DOI:
Chinese Library Classification Number:TF84.1[冶金工程—有色金属冶金]
Citation Information:
China is a large country of tungsten industry, but there is a lack of effective industrialized treatment methods for tungsten slag.With the extensive exploitation of tungsten ore, the traditional landfill method is no longer suitable for the treatment of existing tungsten slag, resulting in the continuous accumulation of tungsten slag.At the same time, heavy metals in tungsten slag have caused serious environmental pollution.In view of these problems, many scholars are committed to solving the problem of tungsten slag accumulation and have carried out a lot of research to comprehensively recover and utilize the va-luable metals in tungsten slag.This paper summarizes the research progress on the recovery and utilization technology of tungsten slag at home and abroad in recent years, which is mainly divided into the recovery of valuable metals in tungsten slag and the use of tungsten slag to make special materials.Finally, the deve-lopment trend of tungsten slag recycling is prospected.
quote
| GB/T 7714-2015 | [1] GONG Dan-dan, LI Zu-yi, ZHANG Yong, et al. Research Status of Tungsten Slag Recycling Technology[J]. Rare Metals and Cemented Carbides, 2021(6): 1-8. |
| MLA | [1] GONG Dan-dan, et al., "Research Status of Tungsten Slag Recycling Technology." Rare Metals and Cemented Carbides, no. 6, 2021, pp. 1-8. |
| APA | [1] GONG Dan-dan, LI Zu-yi, ZHANG Yong, WAN Lin-sheng, & REN Si-li. (2021). Research Status of Tungsten Slag Recycling Technology. Rare Metals and Cemented Carbides(6), 1-8. |
| IEEE | [1] GONG Dan-dan, LI Zu-yi, ZHANG Yong, WAN Lin-sheng, and REN Si-li, "Research Status of Tungsten Slag Recycling Technology," Rare Metals and Cemented Carbides, no. 6, pp. 1-8, 2021. keywords: {tungsten slag;tungsten smelting;alkali decomposition;valuable metal;recovery and utilization} |