Research of Ag-based CeO_2 or γ-Al_2O_3Alloys AITranslate
Abstract AITranslate
Ag-based alloys containing 3% CeO2 or γ-Al2O3 were prepared by powder metallurgy. The microstructure of the Ag-based alloys is studied by X-ray diffraction and metallographic analysis,and the hardness,electrical conductivity, density and friction factor were also tested. The results show that both the two alloys have a relative density of more than 98%. Compared with pure silver metal, the electrical conductivity of the two alloys greatly decreases, the grains are obviously refined, the hardness is improved, but the friction factors of Ag and Cu are not obviously lowered.
KeyWords AITranslate
1周世平.高强度Pd-Ag-Cu合金电刷材料[J].贵金属,1999,20(4):23-26. 被引量:7
2冯本政,童泽新,杜军,谢昀.几种金基合金的耐磨特性[J].贵金属,1995,16(1):16-23. 被引量:9
3李健民.磨损金属学[M].北京:冶金工业出版社,1990.90-100.
4杨慧敏,李溪滨.粉末冶金铝基固体自润滑材料[J].润滑与密封,2001,26(4):55-56. 被引量:4
5陈亮维,黄富春,谢明,蔡云卓.银基氟化镁材料的研究[J].稀有金属材料与工程,2007,36(5):838-841. 被引量:2
6陈亮维,张晓梅,熊嘉骢,张婕.金诺芬的晶体结构研究[J].贵金属,2003,24(2):49-52. 被引量:3
7黄培云.粉末冶金原理[M].北京:冶金工业出版社,1988.341.
1吕琳,宁国松,陈明明.闭挤式精冲成形表面残余应力与耐腐蚀性实验分析[J].热加工工艺,2012,41(13):23-25. 被引量:2
2陈永泰,谢明,杨有才,张吉明,刘满门,王松,王塞北,胡洁琼,李爱坤.Ag-Cu-Zn合金凝固行为的研究[J].贵金属,2015,36(A01):50-53. 被引量:1
1韩济才,周杰,吕琳,邓亚军.精冲摩擦片齿部变形区的显微力学行为分析[J].塑性工程学报,2017,24(5):113-116. 被引量:5
2吕琳,周杰,邓明.闭挤式精冲直齿轮成形面的显微力学化学行为分析[J].塑性工程学报,2018,25(1):156-160. 被引量:1
3赵君,王剑平,魏明霞,张乃千,杨有才,赵通明,毕亚男,谢明.定向凝固Ag-28Cu-xNi系合金的组织和性能研究[J].贵金属,2022,43(S01):9-14.
1王梁,刘晓峰.白银在科技领域应用的新工艺研究[J].内蒙古科技与经济,2002(11):70-71. 被引量:2
2王继周,陈祖锦,马玉祥,周龙江.稀土银铜合金的高温氧化[J].贵金属,1989,10(4):11-17.
3熊易芬.银及银合金的内氧化[J].贵金属,1990,11(2):39-47. 被引量:6
4于炜.银及其合金中微量元素的分析[J].贵金属,1993,14(1):70-76. 被引量:3
5刘泽光.银复合钎料的结构特性和钎接头的应力消除[J].贵金属,1997,18(3):19-22. 被引量:1
6张力.原子吸收光谱法测定银基合金中铅镉镍锰[J].理化检验:化学分册,1989,25(6):333-334.
7虞澜,何纯孝,戴松林.微量Ti·Gd对银的组织和再结晶特性的影响[J].贵金属,1999,20(1):20-24. 被引量:2
8于炜.纯银及银基合金中微量元素的分析[J].有色金属与稀土应用,1992(4):42-49.
9专利信息[J].稀有金属快报,2006,25(5):37-37.
10高彩茹,李晋霞,邰振中,王佳夫.稀土银合金铸态及再结晶组织的观察与分析[J].铸造,2001,50(5):266-269. 被引量:9
Basic Information:
DOI:
Chinese Library Classification Number:TG146.32[金属学及工艺—金属材料]
Citation Information:
Ag-based alloys containing 3% CeO2 or γ-Al2O3 were prepared by powder metallurgy. The microstructure of the Ag-based alloys is studied by X-ray diffraction and metallographic analysis,and the hardness,electrical conductivity, density and friction factor were also tested. The results show that both the two alloys have a relative density of more than 98%. Compared with pure silver metal, the electrical conductivity of the two alloys greatly decreases, the grains are obviously refined, the hardness is improved, but the friction factors of Ag and Cu are not obviously lowered.
quote
| GB/T 7714-2015 | [1] CHEN Liang-wei, LUO Xi-ming, XIE Ming, et al. Research of Ag-based CeO_2 or γ-Al_2O_3Alloys[J]. Rare Metals and Cemented Carbides, 2009(1): 1-4. |
| MLA | [1] CHEN Liang-wei, et al., "Research of Ag-based CeO_2 or γ-Al_2O_3Alloys." Rare Metals and Cemented Carbides, no. 1, 2009, pp. 1-4. |
| APA | [1] CHEN Liang-wei, LUO Xi-ming, XIE Ming, & ZHOU Shi-ping. (2009). Research of Ag-based CeO_2 or γ-Al_2O_3Alloys. Rare Metals and Cemented Carbides(1), 1-4. |
| IEEE | [1] CHEN Liang-wei, LUO Xi-ming, XIE Ming, and ZHOU Shi-ping, "Research of Ag-based CeO_2 or γ-Al_2O_3Alloys," Rare Metals and Cemented Carbides, no. 1, pp. 1-4, 2009. keywords: {Ag-based alloy;CeO2;γ-Al2O3;powder metallurgy;self-lubricating material} |