Experimental Study on Flotation of Refractory Tellurium-containing Tailings AITranslate

Beijing Nonferrous Metal Research Institute;Beijing Nonferrous Metal Research Institute;Beijing Nonferrous Metal Research Institute;Beijing Nonferrous Metal Research Institute;Beijing Nonferrous Metal Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A tellurium recovery process from refractory tellurium-containing tailings was studied. The feasi-bility was discussed of tellurium recovery by the integrated process flowsheet of flotation, gravity separa- tion and magnetic separation. The results show that two types of concentrate from flotation and gravityseparation are obtained by one-stage grinding and flotation of raw tailings, gravity separation of flotation tailings, and magnetic separation of gravity-separation concentrate. The average tellurium grade of themixed concentrate is 1.65% ,and its total recovery is up to 45.97%. And the concentrate product can be used as metallurgical raw materials for further tellurium extraction.

KeyWords AITranslate

tellurium tetradymite tellurium-containing tailing flotation regrinding

1周令冶,陈少纯.稀散金属提取冶金【M].北京:冶金工业出版社.2008.

2胡赓熙,黄和慰,毛钜凡,等.浮选理论与工艺[M].长沙:中南工业大学出版社,1991.

3胡岳华,冯其名.矿物加工技术与设备[M].北京:科学出版社,2008.

1沈志刚,巩波.如何提高铜熔铸渣的回收率[J].科技创新与应用,2014,4(24):104-104.

2苏鸿英.镁废料的回收技术[J].资源再生,2010(5):32-33.

3李广志,王秋俐,孙月霞.6206内圈开裂原因分析[J].轴承,2004(3):25-26.

4于洪爱,李惠琪,孙玉宗,王大陆.等离子束表面冶金铜铝金属间化合物涂层的研究[J].山东科技大学学报:自然科学版,2006,25(2):43-46.

5以转型谋发展 以转型促跨越[J].太钢科技,2010(4):44-44.

6康人木,刘国权,吴文东,帅兴国,谢建国,黄斌,浦年文.钒渣生产V_2O_5尾渣全钒含量与相关工艺指标的函数关系[J].北京科技大学学报,2010,32(8):981-986.

7刘均波,王立梅,李惠琪,于洪爱.等离子束表面冶金Al_2Cu和-αAl复合涂层研究[J].材料热处理学报,2007,28(5):134-137.

8王艳华,樊娴.用内圆磨床的磨头磨精密轴套外圆[J].金属加工:冷加工,2013(6):35-35.

9戴伟,刘佳,程呈.基于齿形溢流槽的铝合金压铸件成形试验分析[J].特种铸造及有色合金,2015,35(7):730-733. 被引量:3

10何秀梅,纪宝忠.齿条磨削工装的改造[J].金属加工:冷加工,2010(24):41-42.

Basic Information:

DOI:

Chinese Library Classification Number:TG955[金属学及工艺—钳工工艺]

Citation Information:

A tellurium recovery process from refractory tellurium-containing tailings was studied. The feasi-bility was discussed of tellurium recovery by the integrated process flowsheet of flotation, gravity separa- tion and magnetic separation. The results show that two types of concentrate from flotation and gravityseparation are obtained by one-stage grinding and flotation of raw tailings, gravity separation of flotation tailings, and magnetic separation of gravity-separation concentrate. The average tellurium grade of themixed concentrate is 1.65% ,and its total recovery is up to 45.97%. And the concentrate product can be used as metallurgical raw materials for further tellurium extraction.

quote

GB/T 7714-2015 [1] ZHANG Lei, CHE Xiao-kui, ZHENG Qi, et al. Experimental Study on Flotation of Refractory Tellurium-containing Tailings[J]. Rare Metals and Cemented Carbides, 2013(1): 1-4.
MLA [1] ZHANG Lei, et al., "Experimental Study on Flotation of Refractory Tellurium-containing Tailings." Rare Metals and Cemented Carbides, no. 1, 2013, pp. 1-4.
APA [1] ZHANG Lei, CHE Xiao-kui, ZHENG Qi, YU Bao-qiang, & YAN Bo. (2013). Experimental Study on Flotation of Refractory Tellurium-containing Tailings. Rare Metals and Cemented Carbides(1), 1-4.
IEEE [1] ZHANG Lei, CHE Xiao-kui, ZHENG Qi, YU Bao-qiang, and YAN Bo, "Experimental Study on Flotation of Refractory Tellurium-containing Tailings," Rare Metals and Cemented Carbides, no. 1, pp. 1-4, 2013. keywords: {tellurium;tetradymite;tellurium-containing tailing;flotation;regrinding}