A Good-prospect Hydrometallurgical Process for Molybdenite AITranslate

School of Chemistry, Central South University;School of Chemistry, Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The methods of molybdenum extraction from molybdenite were introduced.Comparison is focusing on the advantages and disadvantages of various hydrometallurgical processes.The results showed that electro-oxidation process was the most promising for molybdenite.Some suggestions on intensifying leach are put forward.

KeyWords AITranslate

molybdenite rhenium hydrometallurgical process electro-oxidation outfield intensifying

1赵中伟.辉钼矿湿法浸出过程某些理论问题之浅见[J].稀有金属与硬质合金,1995,23(2):1-3. 被引量:10

2С.И.索包里,杨雨浓.很有希望的钼精矿综合处理工艺[J].稀有金属与硬质合金,1991(3):24-27. 被引量:1

1于常武,许士国,陈国伟,周立岱.矽卡岩型钼矿尾砂中重金属Mo的淋滤实验研究[J].生态环境,2008,17(2):636-640. 被引量:7

2于常武,许士国,陈国伟,周立岱.酸碱度温度对钼尾矿中Mo静态浸出的影响[J].环境科学与技术,2008,31(7):1-3. 被引量:2

3曹占芳,钟宏,闻振乾,符剑刚,陈娜.Ultrasonic Electro-oxidation Process of Molybdenite Concentrate[J].过程工程学报,2008,8(5):926-931. 被引量:1

4于常武,周立岱,陈国伟.钼污染物的产生及在环境中的迁移[J].化工环保,2008,28(5):413-417. 被引量:10

5陈洁,李典军,刘大春,杨斌.辉钼矿冶炼技术研究进展[J].甘肃冶金,2009,31(1):25-28. 被引量:10

6康绍辉,孟晋,王洪明,王平,杨剑飞.钼矿物湿法处理技术研究进展[J].湿法冶金,2012,31(6):333-337. 被引量:2

7闻振乾,钟宏,曹占芳,符剑刚,肖燕飞,张文轩.电氧化法湿法分解辉钼矿工艺条件的研究[J].稀有金属,2009,33(2):267-271. 被引量:3

8吴贤,李来平,张新,张文钲.用矿浆电解法分解辉钼矿试验研究[J].现代矿业,2009(10):61-64. 被引量:1

9曹占芳,钟宏,刘广义,符剑刚,闻振乾,王帅.Electric-oxidation extraction of molybdenite concentrate in alkaline NaCl electrolyte[J].中南大学学报:英文版,2010,17(3):480-484. 被引量:2

10徐海清,刘代云,刘慧勇.电氧化湿法分解钼中矿工艺[J].过程工程学报,2010,10(3):554-558. 被引量:3

1都基峻,田刚,张凡.钼冶炼工艺的循环经济探讨[J].环境工程,2011,29(S1):381-384. 被引量:3

2于常武,周立岱,陈国伟.钼污染物的产生及在环境中的迁移[J].化工环保,2008,28(5):413-417. 被引量:10

3陈春强,李明顺,赖燕平.火焰原子吸收光谱法测定锰矿恢复区植物中重金属[J].环境监测管理与技术,2009,21(3):48-49. 被引量:10

4杨大锦.2009年云南冶金年评[J].云南冶金,2010,39(2):37-55. 被引量:2

5徐海清,刘代云,刘慧勇.电氧化湿法分解钼中矿工艺[J].过程工程学报,2010,10(3):554-558. 被引量:3

6雷良奇,宋慈安,谢襄漓,李艳红,王飞.Acid mine drainage and heavy metal contamination in groundwater of metal sulfide mine at arid territory (BS mine,Western Australia)[J].中国有色金属学报:英文版,2010,20(8):1488-1493. 被引量:12

7练建军,许士国,于常武,韩成伟.重金属钼的迁移特性及人工湿地处理研究[J].环境保护科学,2010,36(6):7-10. 被引量:8

8蒋丽娟,奚正平,李来平,张新,梁静,张文钲.由等外品钼精矿制备氧化钼实验研究[J].稀有金属,2011,35(1):106-112. 被引量:6

9吴贤,曹亮,张文钲.2010年钼业年评[J].中国钼业,2010,34(6):1-8. 被引量:10

10田刚,都基峻,张凡,刘宇,石应杰.纯氧密闭干法焙烧硫化钼生产氧化钼工艺研究[J].环境工程技术学报,2011,1(2):157-161. 被引量:3

1邱定蕃.黄铜矿矿浆电解化学过程[J].有色金属:冶炼部分,1996(5):1-3. 被引量:7

2易军,曹才放.湿法分解钨酸钴的热力学分析[J].有色金属科学与工程,2013,4(5):44-47.

3符剑刚,钟宏,黄永平,卜向明.Mn^(3+)/Mn^(2+)间接电氧化法分解辉钼矿[J].中南大学学报:自然科学版,2004,35(5):797-801. 被引量:5

4曹占芳,钟宏,邱朝辉,符剑刚,刘广义,王帅.缓冲体系中辉钼矿电氧化浸出研究[J].现代化工,2009,29(S1):16-18. 被引量:3

5孙国学.金矿样品的分解[J].云南冶金:科学技术版,1989,18(5):45-49. 被引量:4

6赵中伟,赵天从,李洪桂,孙培梅,李运姣,刘茂盛.机械活化对硫化锌精矿浸出动力学的影响[J].有色金属,1995,47(2):81-83. 被引量:16

7曹占芳,钟宏,姜涛,刘广义,王帅.德兴铜矿辉钼矿精矿的选择性电氧化浸出与分离过程[J].中国有色金属学报,2013,23(8):2290-2295. 被引量:14

8张亚莉,于先进,张邦胜,张丽鹏,李德刚,李小斌.钙硅渣湿法处理工艺[J].有色金属:冶炼部分,2011(6):6-9.

9詹惠芳.电解氧化法制备黑镍的研究与应用[J].有色金属:冶炼部分,1995(3):14-16. 被引量:3

10崔晓莉,沃松涛,贾晓婷,任达森,沈杰,杨锡良,章壮健.通电加热氧化金属钛制备TiO_2薄膜及其光催化活性[J].钛工业进展,2005,22(1):24-26. 被引量:3

Basic Information:

DOI:

Chinese Library Classification Number:TF841[冶金工程—有色金属冶金]

Citation Information:

The methods of molybdenum extraction from molybdenite were introduced.Comparison is focusing on the advantages and disadvantages of various hydrometallurgical processes.The results showed that electro-oxidation process was the most promising for molybdenite.Some suggestions on intensifying leach are put forward.

quote

GB/T 7714-2015 [1] FU Jian-gang, ZHONG Hong. A Good-prospect Hydrometallurgical Process for Molybdenite[J]. Rare Metals and Cemented Carbides, 2003(4): 22-26.
MLA [1] FU Jian-gang, and ZHONG Hong. "A Good-prospect Hydrometallurgical Process for Molybdenite." Rare Metals and Cemented Carbides, no. 4, 2003, pp. 22-26.
APA [1] FU Jian-gang, & ZHONG Hong. (2003). A Good-prospect Hydrometallurgical Process for Molybdenite. Rare Metals and Cemented Carbides(4), 22-26.
IEEE [1] FU Jian-gang and ZHONG Hong, "A Good-prospect Hydrometallurgical Process for Molybdenite," Rare Metals and Cemented Carbides, no. 4, pp. 22-26, 2003. keywords: {molybdenite;rhenium;hydrometallurgical process;electro-oxidation;outfield intensifying}