daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Direct Writing of Aligned Conjugated Polymer Micro-Ribbons for High-Performance Organic Electronics AITranslate

National University of Singapore; Fudan University; Fudan University; National University of Singapore; Fudan University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Organic semiconductors (OSCs) and relevant devices have presented their great potential in flexible and wearable electronics. Controlled solution deposition of organic semiconductors at a limited local region is highly expected because it can realize feasible and low-cost fabrication of highly integrated devices with low current leakage and free crosstalk between adjacent devices. Here, we reported a feasible microscale meniscus-guided direct writing method to purposely deposit conjugated polymer poly[2,5-(2-octyldodecyl)-3,6-diketopyrrolopyrrole-alt-5,5-(2,5-di(thien-2-yl)thieno[3,2-b]thiophene)] micro-ribbons at preset local regions. The direct writing of OSCs was carried out on a microscale with the width of written micro-ribbons down to 5 μm, which was seldomly reported before. Direct writing operation induced anisotropic crystallization of organic semiconducting micro-ribbons, which further enhanced the electrical performance of organic transistors with a device on/off ratio of 5.1 × 104 and carrier mobility of 1.05 cm2 V–1 s–1. Small-angle X-ray diffraction analysis further proved the existence of anisotropic crystallization behavior. This technique shed light on the feasible and convenient fabrication of future high-performance organic electronics.

KeyWords AITranslate

direct writing conjugated polymer DPPDTT fieldeffect transistor anisotropic crystallization
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c01600

Chinese Library Classification Number:

Citation Information:

Organic semiconductors (OSCs) and relevant devices have presented their great potential in flexible and wearable electronics. Controlled solution deposition of organic semiconductors at a limited local region is highly expected because it can realize feasible and low-cost fabrication of highly integrated devices with low current leakage and free crosstalk between adjacent devices. Here, we reported a feasible microscale meniscus-guided direct writing method to purposely deposit conjugated polymer poly[2,5-(2-octyldodecyl)-3,6-diketopyrrolopyrrole-alt-5,5-(2,5-di(thien-2-yl)thieno[3,2-b]thiophene)] micro-ribbons at preset local regions. The direct writing of OSCs was carried out on a microscale with the width of written micro-ribbons down to 5 μm, which was seldomly reported before. Direct writing operation induced anisotropic crystallization of organic semiconducting micro-ribbons, which further enhanced the electrical performance of organic transistors with a device on/off ratio of 5.1 × 104 and carrier mobility of 1.05 cm2 V–1 s–1. Small-angle X-ray diffraction analysis further proved the existence of anisotropic crystallization behavior. This technique shed light on the feasible and convenient fabrication of future high-performance organic electronics.

quote

GB/T 7714-2015 [1] Weilin Liu, Conghuan Wang, Qiusong Chen, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.2c01600.
MLA [1] Weilin Liu, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.2c01600.
APA [1] Weilin Liu, Conghuan Wang, Qiusong Chen, Jun Ding, & Guodong Zhu. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.2c01600
IEEE [1] Weilin Liu, Conghuan Wang, Qiusong Chen, Jun Ding, and Guodong Zhu, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.2c01600. keywords: {direct writing conjugated polymer DPPDTT fieldeffect transistor anisotropic crystallization}