Upgrading of Co and Its Separation from Impurities in Weakly Co-containing Solution AITranslate

Zhongnan University of Technology;Zhongnan University of Technology;Zhongnan University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Study is made on the upgrading of Co from low-grade concentrate calcine leachateand its separation from impurities. The studied leachate is free of Fe and Cu, with Co contentonly about 1 g/L while the impurities such as Mg. an. Ni. Mn. St etc in it are about ten times asmuch as Cab. After absorption by absorbent and then processing by HCl at room temperature, thecontent of Co in Hcf solution is about 13 g/L, and Co in the effluent is less than 1 mg/L. Afterevaporating and concentration. Co could be upgraded to over 20 g/L in the enriched solution andseparated from Si. The total recovery of Co to rich Co solution could reach as much as 98. 7%.Then extracted by N235 to separate impuritys CoC12 could reach the technical-purity standard.

KeyWords AITranslate

linnaeite concentrate Co upgrading separation

1杨保祥,彭毅,周有全,朱军.硫钴精矿提钴工艺及技术经济分析[J].钢铁钒钛,1998,19(2):35-38. 被引量:1

2刘淑清.攀枝花硫钴精矿浸出液净化试验研究[J].四川有色金属,2007(1):9-13. 被引量:2

3彭毅,杨保祥,刘淑清.攀枝花硫钴精矿浸出净化液镍钴分离及钴产品制备的试验研究[J].四川有色金属,2006(3):26-30. 被引量:5

4陈立三.硫酸锌溶液深度净化旋流液固分离研究[J].株冶科技,1995,23(1):25-30.

5李亮,杨成.攀枝花某地钒钛磁铁矿选矿基础试验研究[J].钢铁钒钛,2011,32(1):29-33. 被引量:10

6李俊翰,孙宁,罗金华.攀西某钒钛磁铁矿的物质组成与结构特征研究[J].钢铁钒钛,2016,37(5):70-75. 被引量:9

7王放,赵洪兴,肖燕飞,徐志峰.CO_3^(2-)型TOMAC自碱性溶液中萃取硫代亚砷酸[J].有色金属科学与工程,2016,7(2):14-18. 被引量:5

8朱智超.稀土产品中钍的测定[J].中国测试,2013,39(5):53-55. 被引量:2

9邬汉骐.电渗技术用于微细粒物料脱水的新进展[J].湖南有色金属,1990,0(5):26-30.

10赵缨,阮鸿兴.还原焙烧产品中锡的物相分析方法研究[J].冶金分析,2000,20(3):29-32. 被引量:3

Basic Information:

DOI:

Chinese Library Classification Number:TF816.032[冶金工程—有色金属冶金]

Citation Information:

Study is made on the upgrading of Co from low-grade concentrate calcine leachateand its separation from impurities. The studied leachate is free of Fe and Cu, with Co contentonly about 1 g/L while the impurities such as Mg. an. Ni. Mn. St etc in it are about ten times asmuch as Cab. After absorption by absorbent and then processing by HCl at room temperature, thecontent of Co in Hcf solution is about 13 g/L, and Co in the effluent is less than 1 mg/L. Afterevaporating and concentration. Co could be upgraded to over 20 g/L in the enriched solution andseparated from Si. The total recovery of Co to rich Co solution could reach as much as 98. 7%.Then extracted by N235 to separate impuritys CoC12 could reach the technical-purity standard.

quote

GB/T 7714-2015 [1] CHENG Ben-cheng, ZHONG Shi-an, CHENG Dong-ming. Upgrading of Co and Its Separation from Impurities in Weakly Co-containing Solution[J]. Rare Metals and Cemented Carbides, 1998(2): 8-12.
MLA [1] CHENG Ben-cheng, et al., "Upgrading of Co and Its Separation from Impurities in Weakly Co-containing Solution." Rare Metals and Cemented Carbides, no. 2, 1998, pp. 8-12.
APA [1] CHENG Ben-cheng, ZHONG Shi-an, & CHENG Dong-ming. (1998). Upgrading of Co and Its Separation from Impurities in Weakly Co-containing Solution. Rare Metals and Cemented Carbides(2), 8-12.
IEEE [1] CHENG Ben-cheng, ZHONG Shi-an, and CHENG Dong-ming, "Upgrading of Co and Its Separation from Impurities in Weakly Co-containing Solution," Rare Metals and Cemented Carbides, no. 2, pp. 8-12, 1998. keywords: {linnaeite, concentrate, Co, upgrading, separation}