Solvent Extraction of Sc from HCl Leachate of Chloride Dust AITranslate
Abstract AITranslate
Solvent extraction of Sc was investigated experimentally The extraction systemconsisted of P2O4, twroving agent, and kerosene. The results show that the extraction rates ofSc can reach up to 99. 7 %, the removing rates of Fe and Mn are 98. 1 % and 99. 3 % respectively,the stripping rates from organic phase with NaOH reach up to 99.6% with effective separationfrom Fe and Mn.
KeyWords AITranslate
1孙本良,肖飞,翟玉春,田彦文.含钪氯化烟尘的盐酸浸出液中钪与铁、锰的分离[J].稀土,1997,18(4):12-15. 被引量:7
2何锦林,谭红,蔡汝义,程翔.用P204从钛氯化烟尘酸浸液中萃取钪[J].稀有金属,1990,14(4):256-259. 被引量:9
3杨智发,孙世清,李道纯.溶剂萃取法从氯化烟尘中提取钪[J].稀有金属,1989,13(3):217-222. 被引量:8
4柯家骏.湿法冶金提钪的进展[J]稀有金属,1987(05).
5程瑞学,孙隆熙,宋素华,杨慧振.用腐植酸从钨渣的盐酸浸出液中分离和富集钪[J]稀有金属,1981(06).
1马荣锴,罗星,冯吉福,李勇.赤泥提铁尾矿酸浸液中钪的萃取[J].轻金属,2020(5):11-15. 被引量:5
1邱叶红,董惠,朱刘.钪回收提取技术发展现状[J].中国资源综合利用,2021,39(10):145-147. 被引量:1
2李望,刘月,朱晓波.D2EHPA/氯化钠强化萃取赤泥酸浸液中钪及抑制铁的实验研究[J].中南大学学报:英文版,2021,28(10):3029-3039. 被引量:2
3田野,康泽双,刘中凯,闫琨,张腾飞,张延利,曹瑞雪.低温等离子体耦合生物滴滤处理拜耳法生产氧化铝溶出过程中VOCs的研究[J].轻金属,2022(9):59-62.
4朱光祥,宋静,陶东平,曲景奎,孟龙,齐涛.锆冶炼废酸中钪的萃取分离[J].中国有色金属学报,2023,33(2):577-589.
5李博文,姚雨琦,高少轩,阮耀阳,罗惠华,邓博纳.赤泥磷酸浸出液中稀土的萃取行为研究[J].化工矿物与加工,2023,52(8):1-5.
1孙本良,肖飞,翟玉春,田彦文.含钪氯化烟尘的盐酸浸出液中钪与铁、锰的分离[J].稀土,1997,18(4):12-15. 被引量:7
2孙本良,田彦文,翟玉春,肖飞.氯化烟尘中钪浸出条件的实验研究[J].东北大学学报:自然科学版,1997,18(6):606-609. 被引量:3
3何锦林,谭红,蔡汝义,程翔.冶炼钛氯化烟尘提取钪的工艺研究[J].稀土,1989(6):59-61. 被引量:8
4何锦林,谭红,蔡汝义,程翔.用P204从钛氯化烟尘酸浸液中萃取钪[J].稀有金属,1990,14(4):256-259. 被引量:9
5孙本良,肖飞,田彦文,翟玉春.从含钪氯化烟尘中提取钪[J].化工冶金,1998,19(1):11-18. 被引量:2
6颜世宏,李作顺,李宗安,刘期虎,杨广禄.真空蒸馏法净化高纯金属钪中的杂质铁[J].稀土,1995,16(4):64-66. 被引量:4
7林河成.钪的工业及其市场[J].世界有色金属,1994,19(3):8-12. 被引量:9
8陆庆桃,倪福生,陈寅初.钪的应用及其提取冶金的进展[J].上海有色金属,1995,16(3):160-166. 被引量:9
9李国栋,刘永林.高纯金属钪的制备工艺及提纯机理研究[J].内蒙古大学学报:自然科学版,1997,28(5):614-618. 被引量:6
10许孙曲,许菱.从镁、铝和铁废料中回收钪[J].中国物资再生,1998(2):5-6.
Basic Information:
DOI:
Chinese Library Classification Number:TF845.103[冶金工程—有色金属冶金];TF823.052[冶金工程—有色金属冶金]
Citation Information:
Solvent extraction of Sc was investigated experimentally The extraction systemconsisted of P2O4, twroving agent, and kerosene. The results show that the extraction rates ofSc can reach up to 99. 7 %, the removing rates of Fe and Mn are 98. 1 % and 99. 3 % respectively,the stripping rates from organic phase with NaOH reach up to 99.6% with effective separationfrom Fe and Mn.
quote
| GB/T 7714-2015 | [1] SUN Ben-liang, XIAO Fei, DI Yu-chun, et al. Solvent Extraction of Sc from HCl Leachate of Chloride Dust[J]. Rare Metals and Cemented Carbides, 1998(2): 5-8. |
| MLA | [1] SUN Ben-liang, et al., "Solvent Extraction of Sc from HCl Leachate of Chloride Dust." Rare Metals and Cemented Carbides, no. 2, 1998, pp. 5-8. |
| APA | [1] SUN Ben-liang, XIAO Fei, DI Yu-chun, & TIAN Yan-wen. (1998). Solvent Extraction of Sc from HCl Leachate of Chloride Dust. Rare Metals and Cemented Carbides(2), 5-8. |
| IEEE | [1] SUN Ben-liang, XIAO Fei, DI Yu-chun, and TIAN Yan-wen, "Solvent Extraction of Sc from HCl Leachate of Chloride Dust," Rare Metals and Cemented Carbides, no. 2, pp. 5-8, 1998. keywords: {scanium, solvent extraction, separation} |