Rotating field driven structure of particulate magnetic filler in a drying polymer layer AITranslate
Abstract AITranslate
This paper presents computational studies of the dissipative self-organization of a system of soft magnetic particles in a drying thin layer of polymer solution set under a rotating magnetic field. The structure transformations during the layer drying is modeled for different situations including constant/increasing viscosity, regard/disregard of the hydrodynamic interactions, slow or fast drying with respect to the structure formation. All these factors are found influential on the final pattern of the particles distribution in the settled polymer film.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1016/j.commatsci.2010.05.001
Chinese Library Classification Number:
Citation Information:
This paper presents computational studies of the dissipative self-organization of a system of soft magnetic particles in a drying thin layer of polymer solution set under a rotating magnetic field. The structure transformations during the layer drying is modeled for different situations including constant/increasing viscosity, regard/disregard of the hydrodynamic interactions, slow or fast drying with respect to the structure formation. All these factors are found influential on the final pattern of the particles distribution in the settled polymer film.
quote
| GB/T 7714-2015 | [1] S.B. Kashevsky. Computational Materials Science, 2010(49). DOI:10.1016/j.commatsci.2010.05.001. |
| MLA | [1] S.B. Kashevsky. Computational Materials Science, no. 49, 2010, https://doi.org/10.1016/j.commatsci.2010.05.001. |
| APA | [1] S.B. Kashevsky. (2010). Computational Materials Science(49). https://doi.org/10.1016/j.commatsci.2010.05.001 |
| IEEE | [1] S.B. Kashevsky, Computational Materials Science, no. 49, 2010, doi: 10.1016/j.commatsci.2010.05.001. |