Study on Tungsten and Molybdenum Separation in the Ammonium Molybdate Crystallization Process AITranslate
Abstract AITranslate
Based on the difference in property of isopolyacid or heteropolyacid between tungsten and molybdenum,the crystallization process of ammonium molybdate feed solution was operated by acid precipitation or evaporation under various experimental conditions.And the separation effect between tungsten and molybdenum in that process was investigated.The results show that the separation degree of tungsten from molybdenum is low in the acid-precipitation process,but obviously improved in the case of ammonium phosphate addition.The evaporation process is influenced by final pH value and ratio of tungsten to molybdenum in feed solution.Especially when the ratio is large,the difference in crystallization rate between tungsten and molybdenum is obvious,resulting in good separation effect.
KeyWords AITranslate
1黄蔚庄,龚柏凡.柱式吸附法从钨酸钠溶液中分离钼的研究[J].稀有金属与硬质合金,1994,22(1):1-4. 被引量:7
2刘建,王秀山,杨子超,阎居梅.萃淋树脂CL-P507吸附分离钨、钼的研究——Ⅰ.树脂的吸附及分离性能[J].应用化学,1990,7(4):37-41. 被引量:11
3李绍秀,张秀娟.三烷基氧化膦萃取钨、钼的机理研究[J].化学世界,1998,39(5):257-260. 被引量:5
4黄蔚庄 张启修 龚柏凡等.一步离子交换法分离磷、砷、硅、钼制取纯钨酸铵[JJ[J].中南矿冶学院学报,1994,24:121-125.
5肖连生,张启修,龚柏藩,黄芍英.密实移动床-流化床离子交换技术从钨酸盐溶液中除钼试验研究[J].矿冶工程,2001,21(3):66-68. 被引量:13
6刘旭恒,孙放,赵中伟.钨钼分离的研究进展[J].稀有金属与硬质合金,2007,35(4):42-45. 被引量:17
7李洪桂.稀有金属冶金学[M].北京:冶金工业出版社,2006.6-11.
1李金辉,谢芳浩,乔珊,杨幼明.酸性溶液中钨钼离子的电化学行为[J].过程工程学报,2013,13(1):73-77. 被引量:2
2张家靓,赵中伟,陈星宇,刘旭恒.W-Mo-H_2O体系钨钼分离的热力学分析[J].中国有色金属学报,2013,23(5):1463-1470. 被引量:16
3赵文迪,章晓林,王其宏,景满,申培伦.钨钼分离工艺及机理研究进展[J].有色金属工程,2019,9(4):41-48. 被引量:5
1霍广生,彭超,陈星宇,廖春华,陈静.利用弱碱性阴离子交换树脂从硫化后的钨酸钠溶液中吸附除钼[J].中国有色金属学报,2014,24(6):1623-1628. 被引量:7
2刘旭恒,胡芳,赵中伟.大孔型树脂处理高浓度钨酸钠溶液[J].中国有色金属学报,2014,24(7):1895-1900. 被引量:4
3卢晓颖,霍广生,廖春华.利用D309树脂离子交换分离宏量钨和钼(英文)[J].中国有色金属学报:英文版,2014,24(9):3008-3013. 被引量:11
4杨幼明,张剑,张小林,刘小平,郭名亮.Cu还原MoO_4^(2-)产物特性研究[J].中国钨业,2014,29(6):30-34.
5朱先正,霍广生,倪捷,宋琼.Tungsten removal from molybdate solutions using chelating ion-exchange resin:Equilibrium adsorption isotherm and kinetics[J].中南大学学报:英文版,2016,23(5):1052-1057. 被引量:2
6张家靓,张立峰.Mo(VI)-V(V)-H_2O系的热力学平衡与钼酸盐深度除钒工艺的理论分析[J].稀有金属,2016,40(7):701-707. 被引量:7
7张勇.钨钼分离技术的最新研究进展[J].湖南有色金属,2016,32(6):21-25. 被引量:3
8邵康,李青刚,周钦,张贵清,曹佐英,曾理,关文娟.镍钼矿酸浸液中磷钼存在形态的热力学计算[J].中国有色金属学报,2017,27(7):1513-1519. 被引量:2
9郭福亮,陈星宇,赵中伟,何利华,杨凯华,杨珍.硫磷混酸分解白钨矿过程中伴生稀土的行为[J].中国有色金属学报,2018,28(2):387-396. 被引量:5
10李永立,赵中伟.作为可生物降解植入体替代材料的热轧AZ31B镁合金的磨损行为[J].中国有色金属学报,2017,27(12):2598-2604. 被引量:2
1薛生晖.钨湿法冶金过程中的杂多酸及其萃取[J].稀有金属与硬质合金,1989(1):5-8. 被引量:2
2杜建民,万冬林,胡述戈.石灰石、白灰中磷的分析方法研究[J].河南冶金,2000(1):21-21.
3魏改莉.钼酸铵生产中钙含量的控制研究[J].中国钼业,2016,40(4):46-48. 被引量:1
4万林生,周红张,杨亮,王忠兵,梁勇,杨运光.磷酸铵在(NH_4)_3PO_4-(NH_4)_2WO_4-NH_4OH-H_2O系中溶解度研究[J].中国钨业,2016,31(2):49-52.
5杨亮,万林生,舒柳飞.(NH_4)_3PO_4-NH_3·H_2O-H_2O体系中磷酸铵溶解度[J].有色金属科学与工程,2016,7(2):39-42. 被引量:1
6陈洲溪,薛生晖.溶剂萃取法分离工业钨酸钠溶液中的磷、砷、硅[J].有色金属,1991(1):69-73. 被引量:1
7张东风,尹兴仁.氧化钴中硅的测定[J].湖南有色金属,1993,0(4):249-252.
8贺晓唯,毕诗文.硅钼黄光度法快速测定赤泥中硅[J].冶金分析,2006,26(1):92-92. 被引量:4
9乔珊,卢博,杨幼明.铜还原钼磷杂多酸实验研究[J].上海有色金属,2012,33(1):12-15.
10游玉萍,石磊,王淑华,李瑾,任凤莲.微波消解—钼蓝光度法测定高纯氧化铝中二氧化硅的含量[J].铝镁通讯,2004(4):34-35.
Basic Information:
DOI:
Chinese Library Classification Number:TF841.2[冶金工程—有色金属冶金]
Citation Information:
Based on the difference in property of isopolyacid or heteropolyacid between tungsten and molybdenum,the crystallization process of ammonium molybdate feed solution was operated by acid precipitation or evaporation under various experimental conditions.And the separation effect between tungsten and molybdenum in that process was investigated.The results show that the separation degree of tungsten from molybdenum is low in the acid-precipitation process,but obviously improved in the case of ammonium phosphate addition.The evaporation process is influenced by final pH value and ratio of tungsten to molybdenum in feed solution.Especially when the ratio is large,the difference in crystallization rate between tungsten and molybdenum is obvious,resulting in good separation effect.
quote
| GB/T 7714-2015 | [1] GUO Chao, XIAO Lian-sheng. Study on Tungsten and Molybdenum Separation in the Ammonium Molybdate Crystallization Process[J]. Rare Metals and Cemented Carbides, 2010(3): 1-4. |
| MLA | [1] GUO Chao, and XIAO Lian-sheng. "Study on Tungsten and Molybdenum Separation in the Ammonium Molybdate Crystallization Process." Rare Metals and Cemented Carbides, no. 3, 2010, pp. 1-4. |
| APA | [1] GUO Chao, & XIAO Lian-sheng. (2010). Study on Tungsten and Molybdenum Separation in the Ammonium Molybdate Crystallization Process. Rare Metals and Cemented Carbides(3), 1-4. |
| IEEE | [1] GUO Chao and XIAO Lian-sheng, "Study on Tungsten and Molybdenum Separation in the Ammonium Molybdate Crystallization Process," Rare Metals and Cemented Carbides, no. 3, pp. 1-4, 2010. keywords: {ammonium molybdate feed solution;tungsten and molybdenum separation;acid-precipitation crystallization;evaporation crystallization} |