A comparison between friction stir welding, linear friction welding and rotary friction welding AITranslate

Technological Education Institute of Crete; National Technical University of Athens; Kingston University
AITranslate
Publisher: Springer Nature
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Three friction welding processes are compared for temperature, stresses and strains, as well as strain rates developed in the early phases of the processes, which are essential in their successful development. These are friction stir welding (FSW), linear friction welding (LFW) and rotary friction welding (RFW). Their common characteristic is the use of friction to generate adequate energy and raise temperature locally in order to create favorable conditions for welding at the interface between two parts. Although the mode of movement is different for each one of them, welds are produced through plastic deformation. The Lagrangian and coupled Eulerian-Lagrangian numerical models developed have produced results which are in qualitative agreement with experiments and have shed a light on the commonalities of these friction welding processes.

KeyWords AITranslate

Friction welding (FW) Finite element analysis Thermomechanical process Ti6Al4V
No data

Basic Information:

DOI:https://doi.org/10.1007/s40436-016-0163-4

Chinese Library Classification Number:

Citation Information:

Three friction welding processes are compared for temperature, stresses and strains, as well as strain rates developed in the early phases of the processes, which are essential in their successful development. These are friction stir welding (FSW), linear friction welding (LFW) and rotary friction welding (RFW). Their common characteristic is the use of friction to generate adequate energy and raise temperature locally in order to create favorable conditions for welding at the interface between two parts. Although the mode of movement is different for each one of them, welds are produced through plastic deformation. The Lagrangian and coupled Eulerian-Lagrangian numerical models developed have produced results which are in qualitative agreement with experiments and have shed a light on the commonalities of these friction welding processes.

quote

GB/T 7714-2015 [1] Achilles Vairis, George Papazafeiropoulos, AndreasMarios Tsainis. Advances in Manufacturing, 2016(4). DOI:10.1007/s40436-016-0163-4.
MLA [1] Achilles Vairis, et al., Advances in Manufacturing, no. 4, 2016, https://doi.org/10.1007/s40436-016-0163-4.
APA [1] Achilles Vairis, George Papazafeiropoulos, & AndreasMarios Tsainis. (2016). Advances in Manufacturing(4). https://doi.org/10.1007/s40436-016-0163-4