Extending the p-Doping of Polymers to an Air Stable Lewis Acid–Base Adduct by Increasing the Acidity of the Dopant AITranslate

Tianjin University; Tianjin University; Tianjin University; Tianjin University; Tianjin University; Tianjin University; Tianjin University; Tianjin University; Tianjin University; Tianjin University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Among various molecular p-dopants, some Lewis acids have shown recognizable doping effect by the formation of Lewis acid–base adduct for increased hole concentration in organic semiconductors. However, the doping product is often unstable in air by the interference of water. Here near amorphous conjugated polymer poly(indacenodithiophene-co-benzothiadiazole) (IDT-BT) was doped with four Lewis acid dopants of varying acidities, zinc-, borane-, carbonium- and oxonium-based molecules, respectively. Bearing stronger acidity, the oxonium dopant (C6H15O)+BF4– yielded the most air-stable Lewis acid–base adduct, which was confirmed by direct comparison of electron paramagnetic resonance and UV–vis absorption spectra of the four doping systems measured in air. A single polaron species of radical cation was produced between the IDT-BT host and the oxonium dopant, with a binding stoichiometry of 1:1 according to the model study using a benzothiadiazole-derivatized molecule. Via modulating the dopant quantity, the performance of thin-film transistors based on (C6H15O)+BF4–-doped IDT-BT was optimized with enhanced mobility, significantly reduced threshold voltage, higher on/off ratio, and excellent air-stability due to the additional carriers produced by the stable Lewis acid–base adduct. Notably, while the semiconductor layer was processed in air, the (C6H15O)+BF4–-doped device exhibited almost no loss of performance as compared with that under inert atmosphere. We demonstrate that the performance and air stability of Lewis acid-doped polymer and transistor devices thereby can be improved by increasing the acidity of the dopant.

KeyWords AITranslate

molecular doping Lewis acids air stability charge transport organic thin film transistors
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c00342

Chinese Library Classification Number:

Citation Information:

Among various molecular p-dopants, some Lewis acids have shown recognizable doping effect by the formation of Lewis acid–base adduct for increased hole concentration in organic semiconductors. However, the doping product is often unstable in air by the interference of water. Here near amorphous conjugated polymer poly(indacenodithiophene-co-benzothiadiazole) (IDT-BT) was doped with four Lewis acid dopants of varying acidities, zinc-, borane-, carbonium- and oxonium-based molecules, respectively. Bearing stronger acidity, the oxonium dopant (C6H15O)+BF4– yielded the most air-stable Lewis acid–base adduct, which was confirmed by direct comparison of electron paramagnetic resonance and UV–vis absorption spectra of the four doping systems measured in air. A single polaron species of radical cation was produced between the IDT-BT host and the oxonium dopant, with a binding stoichiometry of 1:1 according to the model study using a benzothiadiazole-derivatized molecule. Via modulating the dopant quantity, the performance of thin-film transistors based on (C6H15O)+BF4–-doped IDT-BT was optimized with enhanced mobility, significantly reduced threshold voltage, higher on/off ratio, and excellent air-stability due to the additional carriers produced by the stable Lewis acid–base adduct. Notably, while the semiconductor layer was processed in air, the (C6H15O)+BF4–-doped device exhibited almost no loss of performance as compared with that under inert atmosphere. We demonstrate that the performance and air stability of Lewis acid-doped polymer and transistor devices thereby can be improved by increasing the acidity of the dopant.

quote

GB/T 7714-2015 [1] Yang Liu, Bin Zhao, Jingyu Liu, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c00342.
MLA [1] Yang Liu, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c00342.
APA [1] Yang Liu, Bin Zhao, Jingyu Liu, Zhongli Wang, Ziqi Liang, Weijia Dong, Chenhui Xu, Bin Wang, Zhuping Fei, & Yang Han. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c00342
IEEE [1] Yang Liu, Bin Zhao, Jingyu Liu, Zhongli Wang, Ziqi Liang, Weijia Dong, Chenhui Xu, Bin Wang, Zhuping Fei, and Yang Han, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c00342. keywords: {molecular doping;Lewis acids;air stability;charge transport;organic thin film transistors}