daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

First principles calculations of elastic properties under pressure in SiC AITranslate

Suranaree University of Technology and Synchrotron Light Research Institute; Suranaree University of Technology and Synchrotron Light Research Institute; Case Western Reserve University
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

First principles density functional theory is employed to study the elastic constants and sound velocities in wurtzite-SiC under pressure. The focus is on the behavior of the elastic constants (Cij) and sound velocities ( C ij / ρ ) as a function of pressure. The pressure dependences of the transverse acoustic modes in sound velocities which correspond to the wurtzite to rocksalt phase transformation is analyzed. We found that the phase transformation from wurtzite to rocksalt structure relates to an orthorhombic strain with two components: (1) a traceless compression along the [0 0 0 1] axis which corresponds to the sound velocity C 44 / ρ and (2) a traceless compression along [ 0 1 1 ¯ 0 ] direction which corresponds to the sound velocity C 66 / ρ .

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.commatsci.2010.01.042

Chinese Library Classification Number:

Citation Information:

First principles density functional theory is employed to study the elastic constants and sound velocities in wurtzite-SiC under pressure. The focus is on the behavior of the elastic constants (Cij) and sound velocities ( C ij / ρ ) as a function of pressure. The pressure dependences of the transverse acoustic modes in sound velocities which correspond to the wurtzite to rocksalt phase transformation is analyzed. We found that the phase transformation from wurtzite to rocksalt structure relates to an orthorhombic strain with two components: (1) a traceless compression along the [0 0 0 1] axis which corresponds to the sound velocity C 44 / ρ and (2) a traceless compression along [ 0 1 1 ¯ 0 ] direction which corresponds to the sound velocity C 66 / ρ .

quote

GB/T 7714-2015 [1] Kanoknan Sarasamak, Sukit Limpijumnong, Walter R.L. Lambrecht. Computational Materials Science, 2010(49). DOI:10.1016/j.commatsci.2010.01.042.
MLA [1] Kanoknan Sarasamak, et al., Computational Materials Science, no. 49, 2010, https://doi.org/10.1016/j.commatsci.2010.01.042.
APA [1] Kanoknan Sarasamak, Sukit Limpijumnong, & Walter R.L. Lambrecht. (2010). Computational Materials Science(49). https://doi.org/10.1016/j.commatsci.2010.01.042
IEEE [1] Kanoknan Sarasamak, Sukit Limpijumnong, and Walter R.L. Lambrecht, Computational Materials Science, no. 49, 2010, doi: 10.1016/j.commatsci.2010.01.042.