All-In-One Energy Harvesting/Storage Integrated Systems Based on Eggshell Membranes All-In-One Energy Harvesting/Storage Integrated Systems Based on Eggshell Membranes AITranslate

Federal University of São Francisco Valley; Federal University of São Francisco Valley; Federal University of São Francisco Valley; Federal University of São Francisco Valley
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The development of implantable and wearable electronics and the concept of the internet of things proved a recent burgeoning growth with different applications. However, the integration of electrically driven devices depends on hard components that must be conveniently substituted by flexible and more efficient devices. Herein, the development of a simple and low-cost all-in-one flexible system based on triboelectric generators that harvest energy from the skin contact with the device is proposed and makes possible the storage of this energy in a supercapacitor prepared with the same support applied as collectors of triboelectric nanogenerators (eggshell membranes modified with graphene nanoplatelets and polypyrrole). This integrated prototype for the energy harvesting/storage device with the characteristic flexibility of natural eggshell membranes introduces promising properties of an autonomous device able to drive electronic devices integrated into flexible substrates.

KeyWords AITranslate

polypyrrole triboelectric graphene sustainability ecofriendly process eggshell membrane supercapacitors
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c00909

Chinese Library Classification Number:

Citation Information:

The development of implantable and wearable electronics and the concept of the internet of things proved a recent burgeoning growth with different applications. However, the integration of electrically driven devices depends on hard components that must be conveniently substituted by flexible and more efficient devices. Herein, the development of a simple and low-cost all-in-one flexible system based on triboelectric generators that harvest energy from the skin contact with the device is proposed and makes possible the storage of this energy in a supercapacitor prepared with the same support applied as collectors of triboelectric nanogenerators (eggshell membranes modified with graphene nanoplatelets and polypyrrole). This integrated prototype for the energy harvesting/storage device with the characteristic flexibility of natural eggshell membranes introduces promising properties of an autonomous device able to drive electronic devices integrated into flexible substrates.

quote

GB/T 7714-2015 [1] Giovanni da S. Oliveira, Iuri C. M. Candido, Ravi M. A. P. Lima, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00909.
MLA [1] Giovanni da S. Oliveira, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00909.
APA [1] Giovanni da S. Oliveira, Iuri C. M. Candido, Ravi M. A. P. Lima, & Helinando P. de Oliveira. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00909
IEEE [1] Giovanni da S. Oliveira, Iuri C. M. Candido, Ravi M. A. P. Lima, and Helinando P. de Oliveira, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c00909. keywords: {polypyrrole triboelectric graphene sustainability ecofriendly process eggshell membrane supercapacitors}