Preparation of Ag/BaSn1-xSb_xO_3CuO Electrical Contact Material by Solution Immersion AITranslate
Abstract AITranslate
BaSn1-xSbxO3 ceramic powder was synthesized by solid-state reaction and then immersed in cupric acetate and dried to prepare BaSn1-xSbxO3 CuO composite powder by solid-state reaction at first and then prepare Ag/BaSn1-xSbxO3 CuO composite powder by mechanical mixing with Ag powder.Meanwhile,Ag/BaSn1-xSbxO3 CuO composite powder was prepared by mechanical mixing of the powders.And then the composite powders from the above two processes were sintered by the same process to prepare Ag/BaSn1-xSbxO3 CuO electrical contact material.Density,bending strength and resistivity of the two electric contact materials were compared.The results show that CuO can be distributed more uniformly in BaSn1-xSbxO3 composite powder by solution immersion to greatly accelerate powder sintering and improve material microstructure and the comprehensive performance of Ag/BaSn1-xSbxO3 CuO electrical contact material.
KeyWords AITranslate
1姚超,汪信,吴凤芹,林西平.纳米二氧化锡导电粉体的制备[J].新技术新工艺,2004(6):52-54. 被引量:2
2Meng Fanbin,Lu Janguo,Lu Ningyi,et al.Mass material transfer of Ag/SnO2 contact material in DC level. Elctrical contacts——2006 proceedings of the 52nd IEEE Holm conference on electrical contacts . 2006
3Wingert, P.,Chi-Hung Leung.Comparison of the Inherent Arc Erosion Behaviors of Silver-Cadmium Oxide and Silver-Tin Oxide Contact Materials. Components, Hybrids, and Manufacturing Technology, IEEE Transactions on . 1987
4王宝珠,王胜恩,白惠珍,姚芳.新型银-金属氧化物触头材料成分设计与制粉[J].河北工业大学学报,2001,30(3):77-81. 被引量:20
5Jun Wanga,Dongmei Liu,Yaping Wang.Microstructure and properties of Ag-SnO2 materials with highSnO2 content. Journal of Alloys and Compounds . 2014
6李忠,文春梅,王瑞玉,郑华艳,谢克昌.醋酸铜热解制备无氯Cu2O/AC催化剂及其催化氧化羰基化[J].高等学校化学学报,2009(10):2024-2031. 被引量:29
1李海军,刘飞,丁宙,盛轲炎,董晓晗,王铮莹,陈太炎,袁鞠世港,周子健,庞仕强,左晨,张力,黄江.浸泡法在绝缘子伞裙硅橡胶辐照交联过程中的应用[J].电瓷避雷器,2020(6):211-214. 被引量:3
1胡娟,李文强,张晓莲,张爱霞,陈莉,曾向宏.2020年国内有机硅进展[J].有机硅材料,2021,35(3):63-86. 被引量:10
2庞仕强,袁鞠世港,张格非,黄江.电子束流测量装置设计与实验[J].电力电子技术,2021,55(10):5-7. 被引量:1
3赖永华.衰减全反射红外光谱在电力设备橡胶密封件鉴别中的应用[J].变压器,2022,59(4):20-23. 被引量:2
1单连文.浸泡法再生在水处理工艺中的应用[J].节能,1999,18(7):26-27. 被引量:1
2毛传斌,周廉.Bi系氧化物超导体粉末制备发展及现状[J].稀有金属材料与工程,1994,23(6):1-7. 被引量:2
3王岳化,腾志君,高玉保,顾章平.铜线表面氧化研究及处理方法[J].低压电器,2012(22):8-10. 被引量:1
4徐航,李艳,王洪涛,李明雪,韩奎.TiO_2基染料敏化太阳能电池的表面修饰及性能研究[J].光电子.激光,2017,28(3):243-249. 被引量:1
5杨静,何业东,杨宏.AlCl_3溶液浸泡对非铬酸系铝箔化成速度及比电容的影响[J].电子元件与材料,2010,29(1):42-44. 被引量:1
6郭宏,王巍,邢伟,李艳明.电气/机械混合四余度无刷直流力矩电动机绕组短路分析[J].航空学报,2010,31(5):975-982. 被引量:6
7马萍,张宝宏,巩桂英,徐宇虹.V_2O_5(TiO_2)/S复合材料作锂电池正极的性能研究[J].电子元件与材料,2007,26(8):42-45. 被引量:12
8由宏新,招聪,曲斌,刘润杰,官国清,徐立军,阿布里提.硬模板法制备固体氧化物燃料电池Ni0.5Cu0.5Ba0.05Ox包覆管状SDC立体阳极[J].燃料化学学报,2016,44(10):1272-1280.
9林克芝,王晓琳,徐艳辉.化学处理对多壁碳纳米管电化学储锂性能的影响[J].电源技术,2006,30(2):93-96. 被引量:4
10陈忠元,居亚兰,张文锋,朱云峰,李李泉.一种新型碱性多孔聚合物电解质的制备与性能研究[J].材料导报:纳米与新材料专辑,2009,23(2):316-318.
Basic Information:
DOI:
Chinese Library Classification Number:TM503.5[电气工程—电器]
Citation Information:
BaSn1-xSbxO3 ceramic powder was synthesized by solid-state reaction and then immersed in cupric acetate and dried to prepare BaSn1-xSbxO3 CuO composite powder by solid-state reaction at first and then prepare Ag/BaSn1-xSbxO3 CuO composite powder by mechanical mixing with Ag powder.Meanwhile,Ag/BaSn1-xSbxO3 CuO composite powder was prepared by mechanical mixing of the powders.And then the composite powders from the above two processes were sintered by the same process to prepare Ag/BaSn1-xSbxO3 CuO electrical contact material.Density,bending strength and resistivity of the two electric contact materials were compared.The results show that CuO can be distributed more uniformly in BaSn1-xSbxO3 composite powder by solution immersion to greatly accelerate powder sintering and improve material microstructure and the comprehensive performance of Ag/BaSn1-xSbxO3 CuO electrical contact material.
quote
| GB/T 7714-2015 | [1] CAI Ding-yun, LIU Xin-yu, YUAN Chang-lai, et al. Preparation of Ag/BaSn1-xSb_xO_3CuO Electrical Contact Material by Solution Immersion[J]. Rare Metals and Cemented Carbides, 2015(6): 52-55. |
| MLA | [1] CAI Ding-yun, et al., "Preparation of Ag/BaSn1-xSb_xO_3CuO Electrical Contact Material by Solution Immersion." Rare Metals and Cemented Carbides, no. 6, 2015, pp. 52-55. |
| APA | [1] CAI Ding-yun, LIU Xin-yu, YUAN Chang-lai, LI Bo, WANG Wei, & GAO Pan. (2015). Preparation of Ag/BaSn1-xSb_xO_3CuO Electrical Contact Material by Solution Immersion. Rare Metals and Cemented Carbides(6), 52-55. |
| IEEE | [1] CAI Ding-yun, LIU Xin-yu, YUAN Chang-lai, LI Bo, WANG Wei, and GAO Pan, "Preparation of Ag/BaSn1-xSb_xO_3CuO Electrical Contact Material by Solution Immersion," Rare Metals and Cemented Carbides, no. 6, pp. 52-55, 2015. keywords: {electrical contact material;Ag/BaSn1-xSbxO3CuO;solution immersion;cupric acetate;compre-hensive performance} |