Study on Denitration Activity of Transition Metals of Ag,Co,Ni and Cu on CeAlO Catalyst Carrier AITranslate
Abstract AITranslate
Transition metals of Ag,Co,Ni and Cu were doped on CeAlO catalyst carrier to investigate their denitration activity.The results from XRD,SEM and BET show that transition metals of Ag,Co,Ni and Cu can be well dispersed on CeAlO carrier to increase the number of catalyst active centers and then enhance water-gas shift reaction and improve NO conversion.The results from comparison study show that Ag can well interact with CeAlO carrier to form a reactive InAgO2 intermediate and accelerate Ag dispersion to ensure highest denitration activity and sulfur resistance in the Ag/CeAlO catalyst.
KeyWords AITranslate
1Boningari Thirupathi,Panagiotis G. Smirniotis.??Co-doping a metal (Cr, Fe, Co, Ni, Cu, Zn, Ce, and Zr) on Mn/TiO 2 catalyst and its effect on the selective reduction of NO with NH 3 at low-temperatures(J)Applied Catalysis B, Environmental . 2011
2Boxiong Shen,Xiaopeng Zhang,Hongqing Ma,Yan Yao,Ting Liu.A comparative study of Mn/CeO_2,Mn/ZrO_2 and Mn/Ce-ZrO_2 for low temperature selective catalytic reduction of NO with NH_3 in the presence of SO_2 and H_2O[J].环境科学学报:英文版,2013(4):791-800. 被引量:28
3Ari V?liheikki,Klito C. Petallidou,Christos M. Kalamaras,Tanja Kolli,Mika Huuhtanen,Teuvo Maunula,Riitta L. Keiski,Angelos M. Efstathiou.??Selective catalytic reduction of NO x by hydrogen (H 2 -SCR) on WO x -promoted Ce z Zr 1- z O 2 solids(J)Applied Catalysis B: Environmental . 2014
4Lilia Khalfallah Boudali,Abdelhamid Ghorbel,Paul Grange.??Characterization and reactivity of WO 3 –V 2 O 5 supported on sulfated titanium pillared clay catalysts for the SCR-NO reaction(J)Comptes rendus - Chimie . 2008 (6)
5Screening of doped MnO x –CeO 2 catalysts for low-temperature NO-SCR(J)Applied Catalysis B, Environmental . 2008 (3)
6J. Arfaoui,L. Khalfallah Boudali,A. Ghorbel,G. Delahay.??Effect of vanadium on the behaviour of unsulfated and sulfated Ti-pillared clay catalysts in the SCR of NO by NH 3(J)Catalysis Today . 2008 (3)
7Cristian Ciardelli,Isabella Nova,Enrico Tronconi,Daniel Chatterjee,Brigitte Bandl-Konrad,Michel Weibel,Bernd Krutzsch.Reactivity of NO/NO 2 –NH 3 SCR system for diesel exhaust aftertreatment: Identification of the reaction network as a function of temperature and NO 2 feed content[J]. Applied Catalysis B, Environmental . 2006 (1)
8Howard L. Fang,Herbert F.M. DaCosta.??Urea thermolysis and NO x reduction with and without SCR catalysts(J)Applied Catalysis B, Environmental . 2003 (1)
9Gongshin Qi,Ralph T. Yang.??Performance and kinetics study for low-temperature SCR of NO with NH 3 over MnO x –CeO 2 catalyst(J)Journal of Catalysis . 2003 (2)
10Huang, Helen Y.,Yang, Ralph T.Removal of NO by reversible adsorption on Fe-Mn based transition metal oxides. Langmuir . 2001
1杨洁,李侠,杜红伟,柳召刚.低温La/Ce掺杂锰基脱硝催化剂的制备及表征[J].稀有金属与硬质合金,2021,49(3):41-45. 被引量:2
1黄力,王虎,纵宇浩,常峥峰,高义博,李金珂,于洋.P对V-Mo/Ti脱硝催化剂的性能影响研究[J].钢铁钒钛,2022,43(1):67-73.
2王莹,赵然,张凯,武文斐.独居石负载钼氧化物催化材料制备及其NH3-SCR脱硝性能研究[J].稀有金属与硬质合金,2023,51(1):40-46.
1于强强,董园园,廖卫平,金明善,何涛,索掌怀.CeO_2-Al_2O_3负载金催化剂用于水煤气变换反应的催化活性[J].燃料化学学报,2010,38(2):223-229. 被引量:13
2范志强,封麟先,杨士林.用乙酰氯淬灭法测定Ziegler-Natta催化剂的活性中心数[J].高分子学报,1991,1(4):503-507. 被引量:5
3杨霞,秦绍东,龙俊英,孙守理.MoO_3对Ni/Al_2O_3催化剂CO甲烷化性能的影响[J].现代化工,2016,36(4):72-75.
4罗来涛,欧阳燕,刘文砥.铈对Ru/γ-Al_2O_3变换催化剂的改性研究[J].稀土,2005,26(4):25-29. 被引量:2
5闫少伟,梁川,范辉,李忠.Ni负载量对负载型Ni/SiO_2催化剂结构及性能的影响[J].太原理工大学学报,2012,43(5):544-548. 被引量:4
6罗来涛,刘文砥,王菊枝.过渡金属对Ru/Al_2O_3催化剂改性的影响[J].南昌大学学报:理科版,2004,28(3):246-249.
7缪应纯,王刚,刘树云,吴世鹏.Cu/TiO_2光催化还原硝酸根[J].曲靖师范学院学报,2013,32(6):31-35. 被引量:1
8张成喜,彭凯,李永祥.负载型Ni/Y催化剂性能与结构研究[J].石油炼制与化工,2016,47(2):38-41. 被引量:2
9王忠全.Cu掺杂ZnO光催化降解糖蜜酒精废水的研究[J].大众科技,2015,17(8):29-31.
10徐慧远,储伟,慈志敏.辉光放电等离子体对合成甲醇用铜基催化剂的改性作用[J].物理化学学报,2007,23(7):1042-1046. 被引量:10
Basic Information:
DOI:
Chinese Library Classification Number:O643.36[理学—物理化学];X734.2[环境科学与工程—环境工程]
Citation Information:
Transition metals of Ag,Co,Ni and Cu were doped on CeAlO catalyst carrier to investigate their denitration activity.The results from XRD,SEM and BET show that transition metals of Ag,Co,Ni and Cu can be well dispersed on CeAlO carrier to increase the number of catalyst active centers and then enhance water-gas shift reaction and improve NO conversion.The results from comparison study show that Ag can well interact with CeAlO carrier to form a reactive InAgO2 intermediate and accelerate Ag dispersion to ensure highest denitration activity and sulfur resistance in the Ag/CeAlO catalyst.
quote
| GB/T 7714-2015 | [1] XU Zhen-chong, WU Shuang, ZHOU Ming-dong, et al. Study on Denitration Activity of Transition Metals of Ag,Co,Ni and Cu on CeAlO Catalyst Carrier[J]. Rare Metals and Cemented Carbides, 2015(6): 46-51. |
| MLA | [1] XU Zhen-chong, et al., "Study on Denitration Activity of Transition Metals of Ag,Co,Ni and Cu on CeAlO Catalyst Carrier." Rare Metals and Cemented Carbides, no. 6, 2015, pp. 46-51. |
| APA | [1] XU Zhen-chong, WU Shuang, ZHOU Ming-dong, & LIU Jing-min. (2015). Study on Denitration Activity of Transition Metals of Ag,Co,Ni and Cu on CeAlO Catalyst Carrier. Rare Metals and Cemented Carbides(6), 46-51. |
| IEEE | [1] XU Zhen-chong, WU Shuang, ZHOU Ming-dong, and LIU Jing-min, "Study on Denitration Activity of Transition Metals of Ag,Co,Ni and Cu on CeAlO Catalyst Carrier," Rare Metals and Cemented Carbides, no. 6, pp. 46-51, 2015. keywords: {transition metal;CeAlO;catalyst carrier;denitration activity;sulfur resistance} |