Abstract AITranslate

In this study, a coupled discrete element-finite element approach was developed to predict the effective thermal properties of model pigmented coating layers. Using this approach the influence of coating structure and pigment and binder characteristics was investigated. It was found that pigments with a broader particle size distribution (PSD) resulted in a higher effective thermal conductivity of the coating layer due to the denser coating structure formed by the pigments. Furthermore, the predicted effective thermal conductivities of the coating layers were found to increase with pigment morphology changing from spherical, to needle-like, and to platy. The effective thermal conductivity of the coating layer increased with the increase in the binder content up to the critical pigment volume concentration (CPVC), but declined when the binder content was higher than CPVC. Lastly, it was found that an empirical equation; k eff = A ( 1 - φ v ) 3 k p φ p k l φ l , where kp and kl are the thermal conductivities of pigment and latex, and φp, φl, and φv are the volume fractions of pigment, latex, and voids respectively, can be used to estimate the effective thermal conductivity of the coating layer in good agreement with the FEM–DEM simulation results.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.commatsci.2010.05.027

Chinese Library Classification Number:

Citation Information:

In this study, a coupled discrete element-finite element approach was developed to predict the effective thermal properties of model pigmented coating layers. Using this approach the influence of coating structure and pigment and binder characteristics was investigated. It was found that pigments with a broader particle size distribution (PSD) resulted in a higher effective thermal conductivity of the coating layer due to the denser coating structure formed by the pigments. Furthermore, the predicted effective thermal conductivities of the coating layers were found to increase with pigment morphology changing from spherical, to needle-like, and to platy. The effective thermal conductivity of the coating layer increased with the increase in the binder content up to the critical pigment volume concentration (CPVC), but declined when the binder content was higher than CPVC. Lastly, it was found that an empirical equation; k eff = A ( 1 - φ v ) 3 k p φ p k l φ l , where kp and kl are the thermal conductivities of pigment and latex, and φp, φl, and φv are the volume fractions of pigment, latex, and voids respectively, can be used to estimate the effective thermal conductivity of the coating layer in good agreement with the FEM–DEM simulation results.

quote

GB/T 7714-2015 [1] Pooya Azadi, Ramin Farnood, Ning Yan. Computational Materials Science, 2010(49). DOI:10.1016/j.commatsci.2010.05.027.
MLA [1] Pooya Azadi, et al., Computational Materials Science, no. 49, 2010, https://doi.org/10.1016/j.commatsci.2010.05.027.
APA [1] Pooya Azadi, Ramin Farnood, & Ning Yan. (2010). Computational Materials Science(49). https://doi.org/10.1016/j.commatsci.2010.05.027
IEEE [1] Pooya Azadi, Ramin Farnood, and Ning Yan, Computational Materials Science, no. 49, 2010, doi: 10.1016/j.commatsci.2010.05.027.