Superhydrophilic Sandwich Structure Aerogel Membrane for Emulsion Separation and Heavy Metal Ion Removal AITranslate

Ningbo University; China|University of Chinese Academy of Sciences; Ningbo Institute of Materials Technology & Engineering; China|University of Chinese Academy of Sciences; Ningbo University; China|University of Chinese Academy of Sciences; China|University of Chinese Academy of Sciences
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Water pollution has been increasingly becoming a serious environmental and health challenge in recent years. This is compounded by the often coexisting oil pollution and heavy metal pollution. It is of great practical significance to develop materials that can simultaneously deal with these two kinds of water pollution problems. In this study, a simple and green approach is proposed for preparing matrix-free citric acid modified alginate-based aerogel membrane by simple sol spraying, chemical cross-linking, and freeze-drying methods. The aerogel membrane with dense upper and lower surfaces and a loose interlayer possesses the properties of superhydrophilicity and underwater superoleophobic and strong antiadhesion performances, and it can realize the separation of highly viscous miscible oil–water emulsions with a separation efficiency of over 99.5%, even in corrosive and high-salt environments. The membrane has shown strong stability during 3000 min of uninterrupted cross-flow filtration of emulsion, which reflects the good long-term separation performance of the membrane. The prepared membrane can also be used for the removal of various heavy metal ions from water under gravity, with a removal efficiency >99% and an adsorption capacity of about 240 mg/g for Pb2+. The modified membrane which features low cost, a simple and green preparation process, excellent oil–water separation, and heavy metal removal capabilities possesses great application potential in the treatment of polluted water.

KeyWords AITranslate

alginate citric acid superhydrophilicity emulsion separation heavy metal ion adsorption
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c00802

Chinese Library Classification Number:

Citation Information:

Water pollution has been increasingly becoming a serious environmental and health challenge in recent years. This is compounded by the often coexisting oil pollution and heavy metal pollution. It is of great practical significance to develop materials that can simultaneously deal with these two kinds of water pollution problems. In this study, a simple and green approach is proposed for preparing matrix-free citric acid modified alginate-based aerogel membrane by simple sol spraying, chemical cross-linking, and freeze-drying methods. The aerogel membrane with dense upper and lower surfaces and a loose interlayer possesses the properties of superhydrophilicity and underwater superoleophobic and strong antiadhesion performances, and it can realize the separation of highly viscous miscible oil–water emulsions with a separation efficiency of over 99.5%, even in corrosive and high-salt environments. The membrane has shown strong stability during 3000 min of uninterrupted cross-flow filtration of emulsion, which reflects the good long-term separation performance of the membrane. The prepared membrane can also be used for the removal of various heavy metal ions from water under gravity, with a removal efficiency >99% and an adsorption capacity of about 240 mg/g for Pb2+. The modified membrane which features low cost, a simple and green preparation process, excellent oil–water separation, and heavy metal removal capabilities possesses great application potential in the treatment of polluted water.

quote

GB/T 7714-2015 [1] Hao Zhang, Yuenan Zhang, Ling Fu, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00802.
MLA [1] Hao Zhang, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00802.
APA [1] Hao Zhang, Yuenan Zhang, Ling Fu, Ozioma Udochukwu Akakuru, Zongbao Wang, Aiguo Wu, & Yujie Zhang. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00802
IEEE [1] Hao Zhang, Yuenan Zhang, Ling Fu, Ozioma Udochukwu Akakuru, Zongbao Wang, Aiguo Wu, and Yujie Zhang, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00802. keywords: {alginate;citric acid;superhydrophilicity;emulsion separation;heavy metal ion adsorption}