In this work, we have synthesized a covalent organic polymer CPEP that exhibits high thermal and chemical stability, N-rich backbone, and spherical morphology that provide high surface-to-volume ratios for uniform confinement of Ni nanoparticles. Subsequently, the synthesis of the hybrid material Ni@CPEP was validated with various physicochemical characterizations and utilized as a potential catalyst for the degradation of vile organic dyes named Congo red, methylene blue, and methyl orange. The kinetic parameters affirmed its good catalytic response against all the dyes; in addition, thermodynamic parameters revealed the nonspontaneous and endothermic nature of degradation. As far as reusability is concerned, Ni@CPEP was reported as highly reusable with consistent performance in terms of reaction rate and stability, which is attributed to spherical morphology and uniform confinement of NPs.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c00793
Chinese Library Classification Number:
Citation Information:
In this work, we have synthesized a covalent organic polymer CPEP that exhibits high thermal and chemical stability, N-rich backbone, and spherical morphology that provide high surface-to-volume ratios for uniform confinement of Ni nanoparticles. Subsequently, the synthesis of the hybrid material Ni@CPEP was validated with various physicochemical characterizations and utilized as a potential catalyst for the degradation of vile organic dyes named Congo red, methylene blue, and methyl orange. The kinetic parameters affirmed its good catalytic response against all the dyes; in addition, thermodynamic parameters revealed the nonspontaneous and endothermic nature of degradation. As far as reusability is concerned, Ni@CPEP was reported as highly reusable with consistent performance in terms of reaction rate and stability, which is attributed to spherical morphology and uniform confinement of NPs.
quote
| GB/T 7714-2015 | [1] Deepika Yadav, Satish K. Awasthi. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c00793. |
| MLA | [1] Deepika Yadav, and Satish K. Awasthi. ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c00793. |
| APA | [1] Deepika Yadav, & Satish K. Awasthi. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c00793 |
| IEEE | [1] Deepika Yadav and Satish K. Awasthi, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c00793. keywords: {heterogeneous catalysis;covalent organic polymer;dye degradation;Ni nanoparticles;triazine} |