WC-gCo (containing 0.8 % Cr3 C2/VC) ultrafine cemented carbides were prepared at different sintering temperature by using mixture with different total carbon content of 5.66% and 5.70%. Change with ball milling time in the oxygen content of the mixture,size and internal strain of WC grains was measured, and the change of magnetic properties in the wc-gCo cemented carbides sintered at different temperatures with ball milling time was also investigated. The results show that the nano-size WC grains cannot be crushed by rolling ball milling. With the increase of ball milling time, the oxygen content of mixture with different carbon contents linearly increases,and the increase rate is slower with higher carbon content. Corn value of the ultrafine cemented carbides is a main factor affecting Hc value. Hc value increases at first and then decreases with the increase of Corn value showing a parabolic law, and the maximum Hc value is reached at a certain Corn value. It can be deduced that the carbon content affects the precipitation of V and Cr on the WC/Co interface and the formation of (W,Cr)Cx and (W,V)Cx interphases which can inhibit the growth of WC grains,and therefore affects the inhibition effect.
KeyWords AITranslate
1谢海根,易丹青,黄道远,李荐,刘刚,刘瑞.超细晶硬质合金的制备[J].稀有金属与硬质合金,2007,35(4):14-17. 被引量:15
2张立,吴冲浒,陈述,熊湘君,单成.晶粒生长抑制剂在硬质合金中的微观行为[J].粉末冶金材料科学与工程,2010,15(6):667-673. 被引量:22
3范景莲,李志希,缪群,黄伯云,吴恩熙.超细纳米硬质合金及晶粒长大抑制剂的研究[J].粉末冶金技术,2004,22(5):259-265. 被引量:35
4吴恩熙,雷贻文.超细硬质合金中晶粒生长抑制剂的作用[J].硬质合金,2002,19(3):136-139. 被引量:50
5王洪涛,王旭,余永宁.纳米WC/Co硬质合金粉末烧结早期的晶粒长大研究[J].稀有金属与硬质合金,2005,33(1):18-21. 被引量:17
6黄翔,易丹青,王斌,刘会群,陈丽勇,李会会,朱慧娟.V和Cr对超细WC-Co硬质合金Co粘结相成分与WC/Co界面组织结构的影响[J].粉末冶金材料科学与工程,2016,21(1):95-102. 被引量:8
1朱二涛,张久兴,羊建高.喷雾转化法制备WC-Co复合粉末制备硬质合金的研究进展[J].稀有金属与硬质合金,2019,47(3):70-78. 被引量:2
2郭圣达,余飞,易健宏,郭建锋,陈颢,王文静,羊建高.粉末原料对SPS法制备WC-6Co硬质合金组织性能的影响[J].稀有金属与硬质合金,2019,47(3):79-85. 被引量:4
3王娟梅,仝晓楠,高源.高性能煤化工浆料输出用硬质合金喷嘴的制备试验[J].机械研究与应用,2020,33(2):138-139.
4严维,王水龙,郭圣达,郭建锋,黄星,陈颢,李律达,曹赛鹏.Mo添加对WC-6Co硬质合金组织性能的影响[J].稀有金属与硬质合金,2020,48(4):73-78. 被引量:3
1胡杰,陈勇,刘丹华,徐平.无钯活化法制备WC-W2C复合粉末[J].广州化工,2019,47(24):66-69.
2张璐,李剑峰,尹运春,刘渊溢,陆必志.WC粉末特性对超细晶硬质合金烧结敏感性影响的研究[J].硬质合金,2020,37(1):51-59. 被引量:8
3严维,王水龙,郭圣达,郭建锋,黄星,陈颢,李律达,曹赛鹏.Mo添加对WC-6Co硬质合金组织性能的影响[J].稀有金属与硬质合金,2020,48(4):73-78. 被引量:3
4李律达,郭圣达,羊建高,王水龙,陈颢,曹赛鹏,黄星,张建波.添加剂对双晶结构硬质合金微观组织和性能的影响[J].稀有金属与硬质合金,2020,48(5):72-77.
5唐彦渊,钟志强,羊求民,王红云,徐国钻.碳含量对WC-10Co硬质合金微观组织及力学性能的影响[J].稀有金属与硬质合金,2021,49(6):73-78. 被引量:6
6张建,黄金,许家鹏,罗国强,沈强.金属Mo在500℃LiF-LiCl-LiBr-Li熔盐中的腐蚀行为研究[J].中国腐蚀与防护学报,2022,42(1):67-72.
7牛勇,陆柏贤,黄伟,张茂,唐学峰,马云飞,夏巨谌,胡国安,龚攀,王新云.塑性成形模具用硬质合金的研究进展[J].模具工业,2022,48(9):1-9.
8郭巨华,李彬,何人桂,汪建英,娄嘉,刘艳军,李詠侠,杨海林.Mo对WC-(8Co,2Ni)硬质合金组织与性能的影响[J].粉末冶金材料科学与工程,2022,27(5):488-497.
9曾瑞霖,李剑峰,马赛,龙宁华,张湘,吴育藩.WC粉末特性对PCB用超细晶硬质合金棒材微观组织结构和性能的影响[J].硬质合金,2022,39(6):454-460.
1陈鼎,姚亮,陈振华,王辉平,彭文.WC-Co类硬质合金的低周冲击疲劳性能研究[J].稀有金属与硬质合金,2017,45(3):71-75. 被引量:7
2曾申龙,敖进清,蒋睿,唐祁峰.Ni对Co基合金喷焊层组织与性能的影响[J].热加工工艺,2017,46(13):197-199.
3范昆.串级控温在硬质合金低压烧结炉中的应用[J].机械工程师,2017(9):147-149.
4温鑫,金国,庞学佳,蔡召兵,张子晗,崔秀芳,王海斗,徐滨士.热处理对真空热压烧结NiCrCoTiV高熵合金组织结构及耐腐蚀性能的影响[J].材料导报,2017,31(12):79-83. 被引量:16
5黄继华,陈浩,周国安,曹智威.钨合金力学行为的计算机数值模拟─—宏观力学性能[J].北京科技大学学报,1997,19(6):550-553. 被引量:1
6宁新龙,唐秀娟.9Cr18不锈钢化学成分与热处理工艺对淬火硬度的影响及工艺方法改进[J].航空维修与工程,2017,0(6):64-65. 被引量:1
7尹超,张卫兵,谢晨辉,陆必志.原始WC粉末粒度组成对超细硬质合金组织及性能的影响[J].硬质合金,2017,34(1):7-13. 被引量:5
8林松,张坤,王卫兵,栾国红.2060铝锂合金FSW接头微观组织和力学性能[J].焊接学报,2017,38(6):101-104. 被引量:7
9周红霞,王军伟.GH4033和GH4169合金在520℃熔融NaCl-52 mass% MgCl_2中的腐蚀机理[J].材料热处理学报,2017,38(6):164-169. 被引量:2
10贾晓亮,王晶,张亦良,赵石雷.复杂应力状态下典型材料全载荷过程中的力学行为[J].应用基础与工程科学学报,2017,25(2):407-418. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程]
Citation Information:
WC-gCo (containing 0.8 % Cr3 C2/VC) ultrafine cemented carbides were prepared at different sintering temperature by using mixture with different total carbon content of 5.66% and 5.70%. Change with ball milling time in the oxygen content of the mixture,size and internal strain of WC grains was measured, and the change of magnetic properties in the wc-gCo cemented carbides sintered at different temperatures with ball milling time was also investigated. The results show that the nano-size WC grains cannot be crushed by rolling ball milling. With the increase of ball milling time, the oxygen content of mixture with different carbon contents linearly increases,and the increase rate is slower with higher carbon content. Corn value of the ultrafine cemented carbides is a main factor affecting Hc value. Hc value increases at first and then decreases with the increase of Corn value showing a parabolic law, and the maximum Hc value is reached at a certain Corn value. It can be deduced that the carbon content affects the precipitation of V and Cr on the WC/Co interface and the formation of (W,Cr)Cx and (W,V)Cx interphases which can inhibit the growth of WC grains,and therefore affects the inhibition effect.
quote
| GB/T 7714-2015 | [1] LIU Yan-jun, CHEN Kang-hua, LI Yong-xia, et al. Effects of Carbon Content in Cemented Carbides on Inhibition Effect of Grain Growth Inhibitors[J]. Rare Metals and Cemented Carbides, 2017(3): 65-70. |
| MLA | [1] LIU Yan-jun, et al., "Effects of Carbon Content in Cemented Carbides on Inhibition Effect of Grain Growth Inhibitors." Rare Metals and Cemented Carbides, no. 3, 2017, pp. 65-70. |
| APA | [1] LIU Yan-jun, CHEN Kang-hua, LI Yong-xia, WU En-xi, ZOU Dan, & XIE Yuan-yan. (2017). Effects of Carbon Content in Cemented Carbides on Inhibition Effect of Grain Growth Inhibitors. Rare Metals and Cemented Carbides(3), 65-70. |
| IEEE | [1] LIU Yan-jun, CHEN Kang-hua, LI Yong-xia, WU En-xi, ZOU Dan, and XIE Yuan-yan, "Effects of Carbon Content in Cemented Carbides on Inhibition Effect of Grain Growth Inhibitors," Rare Metals and Cemented Carbides, no. 3, pp. 65-70, 2017. keywords: {grain growth inhibitor;carbon content;WC-Co;cemented carbide;cobalt magnetism;magnetic coercivity;precipitated phase} |