Influence of Anion Existence on W Exchange Capacity in Na_2WO_4 Solution AITranslate
Abstract AITranslate
The effect of some anions,such as SO 2- 4,CI - and OH -,on the W exchange capacity is studied in this paper.The experiment results show that with the increasing of these anions,the W exchange capacity decreases.Meanwhile,with the existence of these three kinds of anions,the orthogonal experiment results show that the order of the degree effect on W exchange capacity is CI ->SO 2- 4>OH -,and that in the solution before exchange,[WO 3]=20g/l,[SO 2- 4]<0.03125mol/L,[CI -]<0.00846mol/L and [OH -]<0.4706 mol/L is feasible.With the existence of these anions,the W exchange capacity can be increased through series columns.
KeyWords AITranslate
1李洪桂等.稀有金属冶金学[M].北京:冶金工业出版社,1993,61.
2MONTGOMERY Douglas C.实验设计与分析[M].北京:中国统计出版社,1998.308
1王荣耕,赵建戌,李学平.利用离子交换树脂提取钨、钼的技术进展[J].河北化工,2005,28(2):16-18. 被引量:5
2肖学有,赵立夫,万林生,李飞,杨亮,陈玲.二次离子交换饱和吸附工艺制备超纯APT[J].中国钨业,2009,24(3):39-42. 被引量:3
3张理源,柴立元,王海鹰,刘晴,谭鑫波.高分子聚胺PED的合成及废水硫酸根的吸附性能[J].中南大学学报:自然科学版,2010,41(2):422-427. 被引量:3
4李洪桂,赵中伟.钨冶金强碱性阴离子交换过程的某些问题的理论分析[J].中国钨业,2010,25(5):35-39. 被引量:3
5万林生,孙丽,杨树生,陈玲,龚丹丹,李红超.钨冶炼溶液体系的非均匀化规律研究[J].稀有金属与硬质合金,2012,40(1):5-9.
6孙培梅,谢武明,李运姣,赵中伟,霍广生,孙召明.Na2WO4溶液离子交换中WO4^2—和SO4^2—分离系数的测定[J].中南工业大学学报,2002,33(1):25-27. 被引量:4
7孙培梅,谢武明,李洪桂,李运姣,赵中伟,霍广生,孙召明.Na_2WO_4溶液离子交换中WO_4^(2-)和SO_4^(2-)的吸附性能[J].中南工业大学学报,2002,33(3):238-241. 被引量:3
8曹才放,章行,李小文,邱晓辰,李昱芃,钟镇宇,王艺瞾,王建松.氯型季铵树脂对钨酸根吸附的热力学研究[J].有色金属科学与工程,2018,9(3):1-4. 被引量:2
1王荣耕,赵建戌,李学平.利用离子交换树脂提取钨、钼的技术进展[J].河北化工,2005,28(2):16-18. 被引量:5
2龚礼胜,王家恒,陈娟,白影超,帅琴.D301R树脂吸附-解吸钼的行为研究[J].分析试验室,2006,25(10):102-104. 被引量:6
3赵立夫,肖学有,万林生,李飞,杨亮,陈玲.二次离子交换饱和吸附法制取超高纯仲钨酸铵工艺优化[J].中国钨业,2009,24(4):32-35. 被引量:4
4李洪桂,赵中伟,霍广生,陈爱良.紧密结合生产实践为新技术研发奠定基础——中国钨湿法冶金理论研究取得重大成果[J].中国钨业,2009,24(5):45-48. 被引量:3
5赵中伟,方奇,李洪桂,霍广生,陈爱良.变参数离子交换的原理及其在钨冶金中的应用[J].稀有金属与硬质合金,2010,38(3):38-42. 被引量:2
6万林生,习雪康,严永海,章小兵.高纯钨酸铵溶液结晶制取超高纯APT的研究[J].稀有金属与硬质合金,2010,38(4):6-9.
7李洪桂,赵中伟.钨冶金强碱性阴离子交换过程的某些问题的理论分析[J].中国钨业,2010,25(5):35-39. 被引量:3
8郗大来,张雄康,蔡卫东.采用离子交换树脂回收钼酸铵生产过程中酸洗废液中钼的工艺[J].中国钼业,2011,35(6):38-40. 被引量:1
9专利技术[J].中国钼业,2011,35(6):40-40.
10孟凡忠,马红钦.SO_4^(2-)脱除现状及锆系复合材料的制备方法[J].化学工业与工程,2012,29(1):65-72. 被引量:1
1邓舜勤.离子交换法提取钨的新工艺[J].湿法冶金,1996,15(1):34-38. 被引量:7
2霍广生,孙培梅,贾根贵.关于钨钼分离的可能方法[J].稀有金属与硬质合金,1997,25(1):52-56. 被引量:12
3周春山,陈景文,熊兴安,刘丰良.Na_2WO_4溶液中砷的萃取色谱分离研究[J].稀有金属,1998,22(4):281-285. 被引量:3
4尹树普,赵静.离子交换工艺解吸钨过程中Cl、P、Sn等杂质行为的研究[J].中国钨业,2000,15(2):27-28. 被引量:1
5石明柱.仲钨酸铵的粒度与形貌对掺杂钨丝性能的影响[J].稀有金属材料与工程,1994,23(6):36-40. 被引量:3
6刘谟禧.黑钨矿压煮-萃取新工艺在我国的技术发展和工业实践[J].稀有金属与硬质合金,1996,24(2):48-50. 被引量:2
7曹淑红.粗Na_2 WO_4溶液的净化分离研究进展[J].稀有金属与硬质合金,1998,26(4):42-46. 被引量:1
8纳洪良,杨汝全.钨精矿中钨的氧化还原滴定法[J].冶金分析,1997,17(3):41-43. 被引量:2
9李汉广,彭志辉.氟化物CVD法直接制取特纯高致密异型钨制品[J].稀有金属材料与工程,1994,23(6):74-77. 被引量:13
10陈惠芳,张景怀.电渗析法从Na_2WO_4溶液中回收碱[J].稀有金属,1989,13(3):227-229.
Basic Information:
DOI:
Chinese Library Classification Number:TF841.1[冶金工程—有色金属冶金]
Citation Information:
The effect of some anions,such as SO 2- 4,CI - and OH -,on the W exchange capacity is studied in this paper.The experiment results show that with the increasing of these anions,the W exchange capacity decreases.Meanwhile,with the existence of these three kinds of anions,the orthogonal experiment results show that the order of the degree effect on W exchange capacity is CI ->SO 2- 4>OH -,and that in the solution before exchange,[WO 3]=20g/l,[SO 2- 4]<0.03125mol/L,[CI -]<0.00846mol/L and [OH -]<0.4706 mol/L is feasible.With the existence of these anions,the W exchange capacity can be increased through series columns.
quote
| GB/T 7714-2015 | [1] SUN Pei-mei, SUN Pei-mei, XIE Wu-ming, et al. Influence of Anion Existence on W Exchange Capacity in Na_2WO_4 Solution[J]. Rare Metals and Cemented Carbides, 2001(2): 1-3. |
| MLA | [1] SUN Pei-mei, et al., "Influence of Anion Existence on W Exchange Capacity in Na_2WO_4 Solution." Rare Metals and Cemented Carbides, no. 2, 2001, pp. 1-3. |
| APA | [1] SUN Pei-mei, SUN Pei-mei, XIE Wu-ming, & HUO Guang-sheng. (2001). Influence of Anion Existence on W Exchange Capacity in Na_2WO_4 Solution. Rare Metals and Cemented Carbides(2), 1-3. |
| IEEE | [1] SUN Pei-mei, SUN Pei-mei, XIE Wu-ming, and HUO Guang-sheng, "Influence of Anion Existence on W Exchange Capacity in Na_2WO_4 Solution," Rare Metals and Cemented Carbides, no. 2, pp. 1-3, 2001. keywords: {sodium tungstate solution;ion exchange;ammonium paratungstate(APT)} |