Study of Crystallization Process during La and La_2(CO_3)_3 Precipitation with Sodium Bicarbonate AITranslate
Abstract AITranslate
Based on pH situ determination data,together with the results of variation in precipitation volume and precipitation partical size,the properties of lanthanum carbonate precipitated with sodium bicarbonate were investigated.The results show that crystalliazation active zone of lanthanum carbonate is in low molar ratio zone,where the moalr ratio is between 0.541~2.828.However,the crystallization of lanthanum carbonate in high molar ratio zone is inactive.At the same tine,the influence of stirring on the crystallization of lanthanum carbonate was examined ,the crystallization mechanism was discussed and the corresponding reaction equations were proposed.
KeyWords AITranslate
1黎敏 等.碳酸氢铵沉淀稀土及其结晶过程的研究进展[J].中国稀土学报,1999,:112-112.
2NAGASHIMA K,et al.The Synthesis of Crystalline Rare Earth Carbonate[J].Bull Chem Soc Jpn,1973,46:152.
3李永绣 等.pH值原位测定法研究碳酸铈的沉淀与结晶过程[J].中国稀土学报(专刊),1999,17:75-75.
4李永绣,黎敏,何小彬,胡平贵,辜子英.碳酸稀土的沉淀与结晶过程[J].中国有色金属学报,1999,9(1):165-170. 被引量:55
5哈姆斯基E B.化学工业中的结晶[M].北京:化学工业出版社,1984.
1Zonghe Yu,Meng Wang,Liangshi Wang,Longsheng Zhao,Zongyu Feng,Xu Sun,Xiaowei Huang.Preparation of crystalline mixed rare earth carbonates by Mg(HCO3)2 precipitation method[J].稀土学报:英文版,2020,0(3):292-298. 被引量:6
2湛含辉,罗彦伟,龙小兵,张晶晶,彭春来.流体力化学概念的提出与定义[J].湖南工业大学学报,2007,21(3):30-34. 被引量:2
3胡艳宏,李梅,柳召刚,阮莹,王觅堂,王丽.碳酸氢铵沉淀法制备大颗粒CeO_2的研究[J].稀土,2008,29(4):12-17. 被引量:7
4柳凌云,牟保畏,姚龙君,彭婧,李赫,萨如拉.高总量碳酸铈的制备和表征[J].稀土,2013,34(4):95-98. 被引量:6
5李慧琴,李健,赵永志,张瑞祥,郝先库,马显东.碳酸氢铵沉淀法制备大颗粒球形氧化钇的研究[J].稀土,2014,35(3):77-81. 被引量:12
6王嵩龄,刘艳,程福祥,吴声,廖春生.碳酸钠作沉淀剂制备碳酸稀土的研究[J].矿冶,2015,24(2):44-46. 被引量:22
7姜晓丽,陈建博,国树山,桑晓云,邢全生,张升强.用碳酸钠作沉淀剂制备低钠碳酸镧[J].稀土,2015,36(6):118-122. 被引量:11
8刘瑞金,赵治华,桑晓云,张正中,魏迪,张国光,张文斌,高媛.采用碳酸氢铵-氨水混合沉淀剂制备碳酸镧的研究[J].稀有金属与硬质合金,2017,45(2):51-54. 被引量:5
9高习贵,孙明华,孙明霞,冯昌法,孙久洲.正交试验法优选碳酸氢钠制备碳酸镨钕的研究[J].中国资源综合利用,2019,37(5):17-19. 被引量:5
10张文娟,马莹,丁艳蓉,赵拓,候少春,赵永志.植物提取液沉淀CeCl3工艺试验[J].中国稀土学报,2019,37(6):704-712.
1Zonghe Yu,Meng Wang,Liangshi Wang,Longsheng Zhao,Zongyu Feng,Xu Sun,Xiaowei Huang.Preparation of crystalline mixed rare earth carbonates by Mg(HCO3)2 precipitation method[J].稀土学报:英文版,2020,0(3):292-298. 被引量:6
2李大鹏,吕灵灵,王沿森,叶阑珊,高玮.硫酸稀土复盐制备氯化稀土的技术研究[J].稀土,2022,43(1):113-118. 被引量:1
3李钿,张扬,王学重.碳酸铈反应结晶过程研究[J].稀土,2020,0(1):1-10. 被引量:1
4刘跃军,刘亦武,魏珊珊,阙永生.复合剪切力场下纳米SiO_2的制备及原位改性[J].硅酸盐学报,2010,38(6):1064-1069. 被引量:2
5阙永生,刘跃军,杨军.油酸包覆针状氢氧化镁纳米粉体的制备[J].中国粉体技术,2010,16(3):50-53. 被引量:2
6李志华,李梅,柳召刚,胡艳宏,吴锦秀.大颗粒稀土氧化物的制备[J].内蒙古科技大学学报,2010,29(2):116-119. 被引量:2
7岑治,夏长林,姬志强,许朝辉,杨海涛,郭英.高浓度溶液共沉技术制备晶型碳酸镨钕工业化生产试验研究[J].稀土,2010,31(4):92-95. 被引量:5
8王占龙,张泽凯,王稚真,陈银飞.钙铝石涂层对整体铜锰铈催化剂高温催化性能的影响[J].稀土,2011,32(4):40-45. 被引量:2
9丁龙,周新木,周雪珍,李静,刘艳珠,李东平,李永绣.镧石型碳酸镨钕向碱式碳酸镨钕的相转变反应特征及其应用[J].无机化学学报,2014,30(7):1518-1524. 被引量:5
10陆梅,邱光怀,马永,张香标,高为正.小粒度高总量碳酸铈的制备[J].稀有金属与硬质合金,2019,47(1):16-18.
1娄利平,古玉琛,张太红.采用化学法降低碳酸镧产品中的非稀土杂质[J].包钢科技,2010,36(6):33-36. 被引量:1
2贺来荣.硫化矿湿法浸出机理研究[J].金川科技,2017,0(1):50-52.
3陈喜平,李旺兴.废槽衬的性能研究[J].有色金属:冶炼部分,2003(6):35-37. 被引量:4
4王春花,黄桂文.串级萃取理论应用于一步萃取多出口生产线技术改造[J].江西冶金,1997,17(1):22-25.
5吴名胜,诸全头.碳酸氢钠与氯化钙溶液真的不反应吗[J].化学教育,2008,29(2):65-66. 被引量:14
6闫森,童雄.强化难处理硫化铜矿物微生物浸出过程的研究[J].国外金属矿选矿,2000,37(11):13-18. 被引量:16
7张娟,王志,郭占成.添加NaHCO_3强化铝酸钠溶液分解析出一水软铝石[J].中国有色金属学报,2010,20(12):2445-2452.
8碳酸法生产稀土氧化物新工艺[J].稀土信息,1994(11):15-15.
9林海玲,范必威.方山口石煤提钒焙烧相变机理的研究[J].稀有金属,2001,25(4):273-277. 被引量:26
10刘晓渝,张冬临.细说碳酸氢钠与碳酸钠的鉴别[J].教学仪器与实验,2008(6):34-35.
Basic Information:
DOI:
Chinese Library Classification Number:TF845[冶金工程—有色金属冶金]
Citation Information:
Based on pH situ determination data,together with the results of variation in precipitation volume and precipitation partical size,the properties of lanthanum carbonate precipitated with sodium bicarbonate were investigated.The results show that crystalliazation active zone of lanthanum carbonate is in low molar ratio zone,where the moalr ratio is between 0.541~2.828.However,the crystallization of lanthanum carbonate in high molar ratio zone is inactive.At the same tine,the influence of stirring on the crystallization of lanthanum carbonate was examined ,the crystallization mechanism was discussed and the corresponding reaction equations were proposed.
quote
| GB/T 7714-2015 | [1] JIAO Xiao-yan, LUO Xian-man, YANG Yu-jun, et al. Study of Crystallization Process during La and La_2(CO_3)_3 Precipitation with Sodium Bicarbonate[J]. Rare Metals and Cemented Carbides, 2001(2): 4-8. |
| MLA | [1] JIAO Xiao-yan, et al., "Study of Crystallization Process during La and La_2(CO_3)_3 Precipitation with Sodium Bicarbonate." Rare Metals and Cemented Carbides, no. 2, 2001, pp. 4-8. |
| APA | [1] JIAO Xiao-yan, LUO Xian-man, YANG Yu-jun, GU Zi-ying, & LI Yong-xiu. (2001). Study of Crystallization Process during La and La_2(CO_3)_3 Precipitation with Sodium Bicarbonate. Rare Metals and Cemented Carbides(2), 4-8. |
| IEEE | [1] JIAO Xiao-yan, LUO Xian-man, YANG Yu-jun, GU Zi-ying, and LI Yong-xiu, "Study of Crystallization Process during La and La_2(CO_3)_3 Precipitation with Sodium Bicarbonate," Rare Metals and Cemented Carbides, no. 2, pp. 4-8, 2001. keywords: {sodium bicarbonate;pH situ determination;crystallization process;lanthanum carbonate} |