A Composite Gas-Phase Explosives Sensor with Frequency-Resistance Dual-Signal Display Based on Surface Acoustic Wave A Composite Gas-Phase Explosives Sensor with Frequency-Resistance Dual-Signal Display Based on Surface Acoustic Wave AITranslate
Abstract AITranslate
The surface acoustic wave (SAW) technology has been widely used for hazardous gas detection, but the low sensitivity, poor selectivity, long response/recovery time, and signal “false positives” of the sensors have limited its application for gas-phase explosives detection. In this paper, a composite gas-phase explosives sensor with frequency-resistance dual-signal display was designed by transferring 25 layers of graphene (rGO) in the sensing area of the SAW device and coupling p-aminothiophenol (PATP)-modified gold nanoparticles (AuNPs). The rGO:AuNP/PATP-SAW sensor shows signal response from two signal dimensions, frequency and resistance, to 0.1–80 ppm TNT gas with a low detection limit (DL) of 41.2 ppb. The composite sensor has a short response/recovery time (9.8 s/27.1 s) with good selectivity, repeatability, and stability. The excellent gas-sensitive performance of the rGO:AuNP/PATP-SAW sensor was attributed to the fact that PATP provides a large number of selective capture groups, which are enriched in the sensing area by the presence of multiple strong interactions with 2,4,6-trinitrotoluene (TNT) molecules. This work will provide scientific guidance for the engineering promotion of surface acoustic wave gas-phase explosives sensors.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.2c01554
Chinese Library Classification Number:
Citation Information:
The surface acoustic wave (SAW) technology has been widely used for hazardous gas detection, but the low sensitivity, poor selectivity, long response/recovery time, and signal “false positives” of the sensors have limited its application for gas-phase explosives detection. In this paper, a composite gas-phase explosives sensor with frequency-resistance dual-signal display was designed by transferring 25 layers of graphene (rGO) in the sensing area of the SAW device and coupling p-aminothiophenol (PATP)-modified gold nanoparticles (AuNPs). The rGO:AuNP/PATP-SAW sensor shows signal response from two signal dimensions, frequency and resistance, to 0.1–80 ppm TNT gas with a low detection limit (DL) of 41.2 ppb. The composite sensor has a short response/recovery time (9.8 s/27.1 s) with good selectivity, repeatability, and stability. The excellent gas-sensitive performance of the rGO:AuNP/PATP-SAW sensor was attributed to the fact that PATP provides a large number of selective capture groups, which are enriched in the sensing area by the presence of multiple strong interactions with 2,4,6-trinitrotoluene (TNT) molecules. This work will provide scientific guidance for the engineering promotion of surface acoustic wave gas-phase explosives sensors.
quote
| GB/T 7714-2015 | [1] Jie Yang, Tianran Wang, Chushu Zhu, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.2c01554. |
| MLA | [1] Jie Yang, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.2c01554. |
| APA | [1] Jie Yang, Tianran Wang, Chushu Zhu, Xuyuan Yin, Peitao Dong, & Xuezhong Wu. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.2c01554 |
| IEEE | [1] Jie Yang, Tianran Wang, Chushu Zhu, Xuyuan Yin, Peitao Dong, and Xuezhong Wu, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.2c01554. keywords: {rGO SAW device TNT sensing frequencyresistance PATP} |