Nucleation Mechanism of HAP by Cathode Electrodeposition AITranslate
Abstract AITranslate
The nucleation mechanism and kinetics of HAP by electrodeposition was studied through constant -potential experiments. The results showed that there were differenti-t transient curves at different potential. However,it was found that linear relationship existed between i-t^1/2 at different potential with three-dimensional instantaneous nucleation. Crystal is grown faster with the negative shift of the additional potential,indicating that additional potential plays a remarkable role in the crystal growth.
KeyWords AITranslate
1俞耀庭.生物医学材料[M].天津:天津大学出版社,2000..
2赵中伟,李洪桂,孙培梅,李运姣,霍广生,兴户正纯,市野良一.电化学沉积生物陶瓷新方法[J].稀有金属与硬质合金,2002,30(1):6-8. 被引量:18
3刘芳,李志友,周科朝,黄伯云,刘咏,韩金鸽.低Ca/P比溶液电沉积羟基磷灰石涂层[J].中南工业大学学报,2002,33(1):63-66. 被引量:13
4刘榕芳,肖秀峰,陈古镛.钛/羟基磷灰石涂层的电沉积过程及其结构特征[J].福建师范大学学报:自然科学版,2001,17(1):45-49. 被引量:22
5柳厚田 (译).电化学方法中的仪器方法[M].上海:复旦大学出版社,1992.320.
6Greef R,et al.Instrumental methods in electrochemistry[J].Ellis Horwood Chich-ester,1985,15:304.
7Scharifker B,et al.Theroretical and experimental studies of multiple nucleation[J].Electrochemic Acta,1983,28(7):879.
1李运刚,蔡宗英,翟玉春,唐国章.FLINAK-Na_2SiF_6熔盐体系中Si的电结晶机理[J].有色金属,2005,57(2):66-68. 被引量:1
2Choi.,K,唐丹.添加VC对WC—Co合金显微结构形成的影响:抑制晶粒长大的机理[J].国外难熔金属与硬质材料,2001,17(1):21-25. 被引量:1
3梁行方,马宏军,段淑贞,石青荣,王新东.在氟盐体系中钕离子阴极过程的研究[J].稀土,1999,20(4):21-23. 被引量:5
4G.P.Demopoulos,李瑞兴.化学法制备细粒贵金属粉末[J].中国有色冶金,1989(4):49-54. 被引量:1
5Dobre.,T,魏文武.铅的电解精炼[J].株冶科技,1998,26(2):8-12.
6万林生.仲钨酸铵结晶成核速率的研究[J].化工冶金,1994,15(4):322-329. 被引量:13
7张保国,李继东,赫婷婷,王一雍.以Li_2CO_3为原料制备金属锂过程的电化学还原机制[J].稀有金属,2016,40(5):473-477. 被引量:2
8张英杰,杨显万,李敦钫,邓纶浩,邱定蕃.矿浆电解时金属的行为规律[J].有色金属,2000,52(2):41-43. 被引量:5
9宋玉强,石志强,李世春.铜粉和镍粉的烧结特性[J].机械工程材料,2003,27(2):40-42. 被引量:6
10侯宝.选矿-拜耳法一段法生产砂状氧化铝的技术研究[J].轻金属,2013(5):9-13. 被引量:3
Basic Information:
DOI:
Chinese Library Classification Number:TF111.5[冶金工程—冶金物理化学]
Citation Information:
The nucleation mechanism and kinetics of HAP by electrodeposition was studied through constant -potential experiments. The results showed that there were differenti-t transient curves at different potential. However,it was found that linear relationship existed between i-t^1/2 at different potential with three-dimensional instantaneous nucleation. Crystal is grown faster with the negative shift of the additional potential,indicating that additional potential plays a remarkable role in the crystal growth.
quote
| GB/T 7714-2015 | [1] CHEN Ai-liang, ZHAO Zhong-wei, CHEN Xing-yu, et al. Nucleation Mechanism of HAP by Cathode Electrodeposition[J]. Rare Metals and Cemented Carbides, 2005(4): 1-3. |
| MLA | [1] CHEN Ai-liang, et al., "Nucleation Mechanism of HAP by Cathode Electrodeposition." Rare Metals and Cemented Carbides, no. 4, 2005, pp. 1-3. |
| APA | [1] CHEN Ai-liang, ZHAO Zhong-wei, CHEN Xing-yu, JIA Xi-jun, & CHEN Jin. (2005). Nucleation Mechanism of HAP by Cathode Electrodeposition. Rare Metals and Cemented Carbides(4), 1-3. |
| IEEE | [1] CHEN Ai-liang, ZHAO Zhong-wei, CHEN Xing-yu, JIA Xi-jun, and CHEN Jin, "Nucleation Mechanism of HAP by Cathode Electrodeposition," Rare Metals and Cemented Carbides, no. 4, pp. 1-3, 2005. keywords: {hydroxyapatite;electrodeposition;instantaneous nucleation;continuous nucleation} |