Emission Spectrometry of Trace Antimony in Tungsten Concentrate AITranslate

Jiangxi Chongyi Zhangyuan Tungsten Industry Co., Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The emission spectrometry of trace antimony in tungsten concentrate was studied. The graphite powders was employed as the buffering agent containing the mixture carrier of sodium fluoride, sodium car- bonate and gallium oxide. The standard working curve of antimony is drawn based on three-standard-sam- ple method. The Sb detection limit of this spectrometry is 0. 003 % and its determination results are very close to those obtained by chemical method.

KeyWords AITranslate

tungsten concentrates trace antimony emission spectrometry graphite powder three- standard- sample method

1YS/T559-2006,钨发射光谱分析方法[S].

1张智怡,贾相如,刘永林,陈桂琴,徐芝亮.电感耦合等离子体发射光谱法测定白钨精矿中的钡和锑[J].中国检验检测,2020,28(3):21-22.

1曲哲,谢天生.俄歇定量分析中标准试样的制备[J].分析化学,1991,19(7):737-741.

2黄典文,梁志启.分光光度间接法测定微量锑的研究[J].广东工业大学学报,1997,0(2):53-55. 被引量:1

3顾永祚,高杰,潘杨.甲基绿-萃取光度法测定锑[J].分析试验室,1994,13(6):36-38. 被引量:5

4张荣,梁玉珍,高立娣.锑(Ⅲ)-苯基荧光酮-混合表面活性剂光度法测定微量锑[J].化学分析计量,2004,13(1):44-45. 被引量:4

5侯明,陈华芳.Sb(Ⅲ)-甲基橙-溴化十六烷基三甲铵的高灵敏显色反应研究及应用[J].分析试验室,1999,18(1):5-8. 被引量:6

6白延涛,高楼军,柴红梅,范樱樱.桑色素荧光猝灭法测定水中微量锑[J].分析试验室,2014,33(4):452-454. 被引量:2

7方迪.电感耦合等离子体原子发射光谱(ICP-AES)法测定铅精矿中的锑[J].中国无机分析化学,2016,6(3):50-52. 被引量:4

8曹文魁.分析实验中减小误差的措施[J].仪器仪表与分析监测,2002(3):40-41.

9赵胜民,杨悦莉.光谱定量分析准理想工作曲线的建立[J].地质实验室,1992,8(6):350-354.

10江子伟,倪自利,王志群.锑-槲皮素络合物极谱吸附波的研究[J].北京大学学报:自然科学版,1994,30(4):434-437. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:O657.31[理学—分析化学]

Citation Information:

The emission spectrometry of trace antimony in tungsten concentrate was studied. The graphite powders was employed as the buffering agent containing the mixture carrier of sodium fluoride, sodium car- bonate and gallium oxide. The standard working curve of antimony is drawn based on three-standard-sam- ple method. The Sb detection limit of this spectrometry is 0. 003 % and its determination results are very close to those obtained by chemical method.

quote

GB/T 7714-2015 [1] CHEN Hai-yan. Emission Spectrometry of Trace Antimony in Tungsten Concentrate[J]. Rare Metals and Cemented Carbides, 2010(1): 42-43.
MLA [1] CHEN Hai-yan. "Emission Spectrometry of Trace Antimony in Tungsten Concentrate." Rare Metals and Cemented Carbides, no. 1, 2010, pp. 42-43.
APA [1] CHEN Hai-yan. (2010). Emission Spectrometry of Trace Antimony in Tungsten Concentrate. Rare Metals and Cemented Carbides(1), 42-43.
IEEE [1] CHEN Hai-yan, "Emission Spectrometry of Trace Antimony in Tungsten Concentrate," Rare Metals and Cemented Carbides, no. 1, pp. 42-43, 2010. keywords: {tungsten concentrates;trace antimony;emission spectrometry;graphite powder;three- standard- sample method}