Barium Determination of Si-Ca-Ba Alloy by Spectrophotometry with Tribromoarsenazo AITranslate

Hubei Provincial Mechanical and Electrical Research Institute;Hubei Provincial Mechanical and Electrical Research Institute;Hubei Provincial Mechanical and Electrical Research Institute;Hubei Provincial Mechanical and Electrical Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The chromogenic reaction between tribromoarsenazo and barium was studied as well as the influ- ences of coexistent ions on the reaction. The results show that barium reacts with the chromogenic reagent in 0.3 mol/L H3PO4 solution to form a stable purple complex,which exhibits an absorption maximum at 618 nm with an apparent molar absorptivity of 3.90 × 104 L/(mol cm). Beer's law is obeyed with the barium content of 0-40 μg/25 mL. The chromogenic reaction is of high sensitivity and the speetrophotometry can be used to determine the barium content of Si-Ca-Ba alloy. The determined results are in agreement with the certified values, and the relative standard deviation (RSD) is less than 2%.

KeyWords AITranslate

tribromoarsenazo spectrophotometry Si-Ca-Ba alloy barium content

1沙艳梅,赵学沛,王明军,何雪梅.硅钙钡镁合金中钡钙镁的测定[J].岩矿测试,2004,23(4):308-310. 被引量:10

2罗道成,易平贵,陈安国,李佳秋.EDTA络合滴定法测定硅钙钡合金中钙和钡[J].冶金分析,2002,22(2):47-48. 被引量:11

3刘道平,陈先聪,周斌,汪绍红.硅钙钡及硅钡铁合金中钙、钡的测定[J].冶金分析,1996,16(1):54-55. 被引量:13

4孟平,陆军,龙如成.ICP-AES内标法测定硅钙钡合金中的元素[J].金属制品,2005,31(1):45-46. 被引量:9

5陈玉珍,刘迎新.β-环糊精─偶氮氯膦Ⅲ分光光度法测定微量钡[J].湘潭大学自然科学学报,1994,16(1):73-76. 被引量:3

6刘道平.钡-偶氮氯膦Ⅲ-铜(Ⅱ)-邻菲啰啉多元体系的显色反应及其应用[J].化学试剂,1992,14(1):13-14. 被引量:8

7沈令熙,凌蓉.钡—偶氮氯膦Ⅲ—锌—邻啡罗啉混合多核配合物显色反应的研究[J].痕量分析,1989,5(3):16-21. 被引量:5

8董丙成.均三溴偶氮胂光度法测定硅铝钡铁合金中的钡[J].山东冶金,1996,18(4):44-46. 被引量:3

9陈明岩.三溴偶氮胂光电比色法测定硫酸镍电解液中的钡[J].吉林冶金,1992(4):39-41. 被引量:1

1於利慧.两步法熔融制样-X射线荧光光谱法测定硅钙钡合金中9种主次量元素[J].理化检验:化学分册,2021,57(9):840-844. 被引量:2

2宁骏斌,赵书运,郭海珍.重量法测定铜阳极泥中硫酸钡[J].中国有色冶金,2022,51(2):89-92. 被引量:1

1张秀艳,刘丹娜,张红,包香春.电感耦合等离子体质谱法测定稀土熔盐电解回收料中铝铬镍锌[J].冶金分析,2022,42(9):68-74.

2万芒,刘伟,曾小平.熔融制样-X射线荧光光谱法测定稀土硅铁中11种主次元素[J].冶金分析,2023,43(1):54-61.

3王怀宇,王立华,蒋维,魏启珂,张浩.烟叶复烤回潮有限元分析及工艺参数优化[J].科学技术与工程,2023,23(16):6993-7001.

1吴丽娟.丁二酮肟分光光度法测定硅钙钡合金中的镍含量[J].冶金标准化与质量,2012(1):33-34.

2罗来辉,张莉.对硅钙钡合金中Ca、Ba的连续测定方法的探讨[J].黄山学院学报,2004,6(3):53-53. 被引量:1

3钟国秀,杨浩义,黄清华.偶氮氯膦Ⅲ分光光度法测定硅钙钡合金中钡含量[J].稀有金属与硬质合金,2009,37(2):34-36. 被引量:3

4郑会清,王翠翠,张有毅.ICP-OES法测定硅钙钡合金中主量和微量元素[J].广州化工,2013,41(21):98-99. 被引量:3

Basic Information:

DOI:

Chinese Library Classification Number:O657.32[理学—分析化学]

Citation Information:

The chromogenic reaction between tribromoarsenazo and barium was studied as well as the influ- ences of coexistent ions on the reaction. The results show that barium reacts with the chromogenic reagent in 0.3 mol/L H3PO4 solution to form a stable purple complex,which exhibits an absorption maximum at 618 nm with an apparent molar absorptivity of 3.90 × 104 L/(mol cm). Beer's law is obeyed with the barium content of 0-40 μg/25 mL. The chromogenic reaction is of high sensitivity and the speetrophotometry can be used to determine the barium content of Si-Ca-Ba alloy. The determined results are in agreement with the certified values, and the relative standard deviation (RSD) is less than 2%.

quote

GB/T 7714-2015 [1] ZHONG Guo-xiu, YANG Hao-yi, HUANG Qing-hua, et al. Barium Determination of Si-Ca-Ba Alloy by Spectrophotometry with Tribromoarsenazo[J]. Rare Metals and Cemented Carbides, 2010(1): 44-46.
MLA [1] ZHONG Guo-xiu, et al., "Barium Determination of Si-Ca-Ba Alloy by Spectrophotometry with Tribromoarsenazo." Rare Metals and Cemented Carbides, no. 1, 2010, pp. 44-46.
APA [1] ZHONG Guo-xiu, YANG Hao-yi, HUANG Qing-hua, & LU Fan. (2010). Barium Determination of Si-Ca-Ba Alloy by Spectrophotometry with Tribromoarsenazo. Rare Metals and Cemented Carbides(1), 44-46.
IEEE [1] ZHONG Guo-xiu, YANG Hao-yi, HUANG Qing-hua, and LU Fan, "Barium Determination of Si-Ca-Ba Alloy by Spectrophotometry with Tribromoarsenazo," Rare Metals and Cemented Carbides, no. 1, pp. 44-46, 2010. keywords: {tribromoarsenazo;spectrophotometry;Si-Ca-Ba alloy;barium content}