Application of PLC in Charge Preparation & Weighing System of ISF AITranslate

Changsha Nonferrous Metallurgical Design Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The paper describes the application of PC984 PLC in the Charge preparation & weighing system of ISF, including the process, system configuration, software design and control function. The method for high reliability and precision of the weighing control system and the technical features are also described.

KeyWords AITranslate

ISF weighing system PLC control system

1奥斯特隆姆 K J(瑞典).自适应控制[M].北京:科学出版社,1992..

1周永华,刘荣.采用PLC消除“卡料”故障[J].电世界,1996,37(2):12-13.

2徐仕华,李熙.150T铁水包称量台车设计[J].科技信息,2013(6):392-393.

3田斌,贾斌,刘峰,牛燕光.自适应控制技术在散状料称量系统中的应用[J].莱钢科技,2011(3):39-40.

4吴忠业,张杏生.各种称量系统在现代大型烧结生产中的应用[J].衡器,2002,31(6):33-34.

5朱贤学.高炉喷煤称量系统称重补偿[J].酒钢科技,2003(B02):71-72.

6梁瑞秋,章正悌.用PLC弥补本钢5号高炉原料称量系统的欠缺[J].基础自动化,1998,5(2):32-33.

7陈铁军,王彩琴.核子秤称量系统在原料混匀配料中的应用与改进[J].山东冶金,2006,28(4):74-75. 被引量:1

8章正悌.工业控制机PC984—B在本钢5号高炉原料称量系统中的应用[J].本钢技术,1998(7):4-6.

9宋贵芳,黄家瑞.称量车结构优化分析[J].冶金设备,2007(S2):65-66.

10段方民,张强,李维富.基于现场总线的智能称量系统[J].可编程控制器与工厂自动化(PLC FA),2004(10):51-53.

Basic Information:

DOI:

Chinese Library Classification Number:TF355.2[冶金工程—冶金机械及自动化]

Citation Information:

The paper describes the application of PC984 PLC in the Charge preparation & weighing system of ISF, including the process, system configuration, software design and control function. The method for high reliability and precision of the weighing control system and the technical features are also described.

quote

GB/T 7714-2015 [1] HE Guang. Application of PLC in Charge Preparation & Weighing System of ISF[J]. Rare Metals and Cemented Carbides, 1999(4): 57-61.
MLA [1] HE Guang. "Application of PLC in Charge Preparation & Weighing System of ISF." Rare Metals and Cemented Carbides, no. 4, 1999, pp. 57-61.
APA [1] HE Guang. (1999). Application of PLC in Charge Preparation & Weighing System of ISF. Rare Metals and Cemented Carbides(4), 57-61.
IEEE [1] HE Guang, "Application of PLC in Charge Preparation & Weighing System of ISF," Rare Metals and Cemented Carbides, no. 4, pp. 57-61, 1999. keywords: {ISF;weighing system;PLC;control system}