Abstract AITranslate
year operation with vacuum dryer instead of the resistance furnace to dry APT has showed a distinct improvement of product quality, and much faster evaporation, with remarkable economic benefits. The popularization of the said equipment is suggested.
KeyWords AITranslate
1刘士军.几种钨同多酸盐及钨的同多酸离子的热力学性质研究.中南工业大学(博士论文)[M].长沙,1999..
2李洪桂.稀有金属冶金原理及工艺[M].北京:冶金工业出版社,1987.196.
3莫以浩.钨冶炼的原理与工艺[M].北京:轻工业出版社,1984..
1许杰,姜厚春.用于市政污泥干化的干燥机选型及设计计算[J].化工机械,2022,49(2):309-312. 被引量:1
1王依琳,尹鹏宇,王孚懋.太阳能-热泵复合污泥干燥系统设计[J].现代制造技术与装备,2022,58(7):98-100.
1韩德奇.有机合成的“新基石”——DMC[J].中外医疗,2000,0(3):11-11. 被引量:1
2刘尚宜,黎莹莹,汤易慧,张秋萍,靳菲.超声波对蒸馏水蒸发过程的影响[J].山东化工,2016,45(21):19-20.
3于士君.外热式自然循环蒸发器的计算[J].石油化工高等学校学报,1995,8(1):22-28.
4DW系列带式干燥机[J].沿海企业与科技,2004(8):18-18.
5吴松海,孙永利,贾绍义.磁场对蒸馏水蒸发过程的影响[J].石油化工高等学校学报,2006,19(1):10-12. 被引量:10
6吴金星,董其伍,魏新利,王定标,刘敏珊.椭圆腔板束强化降膜蒸发研究[J].化工设计,2001,11(1):30-33. 被引量:3
7宋长运,黄德东,薛祥军,石永华.水基涂料及其湿法喷涂[J].铸造技术,2006,27(8):889-890. 被引量:1
8孙剑锋,李里特,李法德,王颉.多针电极高压静电场下蒸馏水蒸发的研究[J].安徽农业科学,2009,37(22):10363-10364. 被引量:2
9吴金星,董其伍,刘敏珊,魏新利,王学生.板壳式降膜蒸发器结构及性能研究[J].郑州工业大学学报,1997,18(4):7-12. 被引量:5
10王信之.真空炼钢理论(一)[J].大型铸锻件,1987(4):36-48. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TQ136.13[化学工程—无机化工]
Citation Information:
year operation with vacuum dryer instead of the resistance furnace to dry APT has showed a distinct improvement of product quality, and much faster evaporation, with remarkable economic benefits. The popularization of the said equipment is suggested.
quote
| GB/T 7714-2015 | [1] CHEN Tian-ling. Application of Drum Vacuum Dryer in Our Plant[J]. Rare Metals and Cemented Carbides, 1999(4): 54-56. |
| MLA | [1] CHEN Tian-ling. "Application of Drum Vacuum Dryer in Our Plant." Rare Metals and Cemented Carbides, no. 4, 1999, pp. 54-56. |
| APA | [1] CHEN Tian-ling. (1999). Application of Drum Vacuum Dryer in Our Plant. Rare Metals and Cemented Carbides(4), 54-56. |
| IEEE | [1] CHEN Tian-ling, "Application of Drum Vacuum Dryer in Our Plant," Rare Metals and Cemented Carbides, no. 4, pp. 54-56, 1999. keywords: {drum vacuum dryer;APT drying;application} |