Vanadium Recovery from Vanadium-containing Leaching Solution with High Iron Concentration by Reducing Precipitating-Redissolving AITranslate

China Aluminum Zhengzhou Research Institute;China Aluminum Zhengzhou Research Institute;China Aluminum Zhengzhou Research Institute;China Aluminum Zhengzhou Research Institute;China Aluminum Zhengzhou Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Vanadium was recovered from vanadium-containing ceaching solution with high iron concentra- tion by reducing precipitating-redissolving process. The process steps of pre-neutralizing of leaching solu- tion,preparation and redissolving of vanadium acid concentrate and the influence factors of each link were investigated. The results show that this process can recover vanadium and prepare qualified Vz 05 , but the overall recovery rate of vanadium is relatively low.

KeyWords AITranslate

vanadium-containing leaching solution with high iron concentration vanadium recovery reducing precipitating redissolving

1Zhou Xiangyang, Li Changlin, Li Jie, et al. Leaching of vanadium from carbonaceous shale[J]. Hydrometallur- gy,2009,99(1-2): 97-99.

2陈家铺,于淑秋,伍志春.湿法冶金中铁的分离与应用[M].北京:冶金工业出版社,1991.82-92.

3Claassen J O, Meyer E H O,Rennie J,et al. Iron precipi- tation from zinc- rich solutions: defining the Zincor Process[J]. Hydrometallurgy, 2002,67 (1-3) : 87-108.

4冯雅丽,李浩然,罗小兵,等.粘土矿湿法提钒工艺[P].中国专利:101215646A,2008-07-09.

5新开公社钒冶炼厂,湖南冶金研究所.新开公社钒冶炼厂水浸渣酸浸制取偏钒酸铵工艺试验[J].湖南冶金,1997,(3):33-47.

6YB/T53042006.五氧化二钒[s].

1董竑君,蒋训雄,范艳青,张登高,汪胜东,冯林永,刘巍.二氧化硫还原沉淀粗碲的研究[J].有色金属:冶炼部分,2014(9):55-58. 被引量:11

2张菊花,张力,张伟,杨丽梅,张武,顾松青.溶剂萃取法净化含钒溶液的研究现状[J].材料与冶金学报,2013,12(3):189-196. 被引量:3

3齐兆树,李青刚.从碱性含钒溶液中萃取钒的研究[J].有色金属:冶炼部分,2014(10):43-48. 被引量:3

4许万祥,张卜升,李波,王治钧,王靖坤.海绵铜浸出液还原沉淀氯化亚铜[J].湿法冶金,2015,34(4):301-304. 被引量:2

5蒋霖,伍珍秀.酸性含钒溶液除硅工艺研究[J].稀有金属,2017,41(2):221-224.

6刘秀庆,吴文花.提高铅阳极泥中Te回收率的实验研究[J].稀有金属与硬质合金,2016,44(6):22-25. 被引量:1

7张耀辉,饶磊,马孟臣,刘自民,桂满城.化学还原沉淀法处理含铬废酸的试验研究[J].安徽冶金,2016,0(4):25-27. 被引量:2

8杨洪飚,何蔼平,刘时杰.从失效载体催化剂回收铂的工艺研究[J].贵金属,2005,26(4):9-13. 被引量:7

9兰兴华.置换沉淀铜的现在和未来[J].资源再生,2009(6):41-43.

10张丽霞.通过臭氧氧化—氰化作用处理含黄铁矿的金-银难处理矿石[J].湿法冶金,2006,25(2):106-106.

Basic Information:

DOI:

Chinese Library Classification Number:TF841.3[冶金工程—有色金属冶金]

Citation Information:

Vanadium was recovered from vanadium-containing ceaching solution with high iron concentra- tion by reducing precipitating-redissolving process. The process steps of pre-neutralizing of leaching solu- tion,preparation and redissolving of vanadium acid concentrate and the influence factors of each link were investigated. The results show that this process can recover vanadium and prepare qualified Vz 05 , but the overall recovery rate of vanadium is relatively low.

quote

GB/T 7714-2015 [1] LI Chang-lin, ZHOU Yun-feng, FU Hai-xia, et al. Vanadium Recovery from Vanadium-containing Leaching Solution with High Iron Concentration by Reducing Precipitating-Redissolving[J]. Rare Metals and Cemented Carbides, 2012(5): 10-14.
MLA [1] LI Chang-lin, et al., "Vanadium Recovery from Vanadium-containing Leaching Solution with High Iron Concentration by Reducing Precipitating-Redissolving." Rare Metals and Cemented Carbides, no. 5, 2012, pp. 10-14.
APA [1] LI Chang-lin, ZHOU Yun-feng, FU Hai-xia, ZHOU Xiang-yang, & LI Jie. (2012). Vanadium Recovery from Vanadium-containing Leaching Solution with High Iron Concentration by Reducing Precipitating-Redissolving. Rare Metals and Cemented Carbides(5), 10-14.
IEEE [1] LI Chang-lin, ZHOU Yun-feng, FU Hai-xia, ZHOU Xiang-yang, and LI Jie, "Vanadium Recovery from Vanadium-containing Leaching Solution with High Iron Concentration by Reducing Precipitating-Redissolving," Rare Metals and Cemented Carbides, no. 5, pp. 10-14, 2012. keywords: {vanadium-containing leaching solution with high iron concentration;vanadium recovery;reducing precipitating;redissolving}