Experimental Study on Recovery of Scandium and Vanadium from Red Mud by Leaching with Titanium Dioxide Wastewater AITranslate

School of Chemistry and Chemical Engineering,Henan Polytechnic University;School of Chemistry and Chemical Engineering,Henan Polytechnic University;School of Chemistry and Chemical Engineering,Henan Polytechnic University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The extraction of vanadium and scandium from red mud were carried out by leaching with tita-nium dioxide wastewater.The effects of liquid to solid ratio, leaching temperature, leaching time and stirring rate on the leaching rate of vanadium and scandium were investigated.The phase composition of lea-ching residue and the chemical composition of leaching solution were analyzed by XRD and ICP-AES.The results show that under the conditions of liquid to solid ratio of 6 mL/g, stirring rate of 400 r/min, leaching temperature of 75 ℃ and leaching time of 1 h, the leaching rates of V and Sc are 75% and 80%,respectively.Compared with the titanium dioxide wastewater, the leaching solution contains significantly decreased H+ concentration, vanadium and scandium are enriched and the concentration of iron and aluminum is also increased.Compared with the red mud, anhydrite minerals appears in the leaching residue, while calcite is completely dissolved, cancrinite, brookite and hematite are partially dissolved.

KeyWords AITranslate

scandium vanadium leaching red mud titanium dioxide wastewater

1柳晓,韩跃新,何发钰,李艳军,高鹏,李文博.赤泥的危害及其综合利用研究现状[J].金属矿山,2018,47(11):7-12. 被引量:32

2姜平国,廖春发.从赤泥盐酸浸出液中提取钪的工艺研究[J].中国有色冶金,2012,41(1):66-68. 被引量:13

3薛安,陈肖虎,唐晓宁.赤泥中浸出钪的工艺条件及动力学研究[J].有色金属:冶炼部分,2010(2):51-54. 被引量:15

4王克勤,李生虎.氧化铝赤泥盐酸浸出回收钒的试验研究[J].稀有金属与硬质合金,2012,40(6):5-8. 被引量:11

5崔佳娜,任慧莉.我国钛白粉生产工艺技术的发展及比较[J].稀有金属与硬质合金,2013,41(4):14-17. 被引量:13

6李具康,代佼.硫酸法钛白粉“三废”治理与利用的研究进展[J].环境科学导刊,2014,33(4):63-66. 被引量:8

7朱晓波,牛泽鹏,李望,白云涛,王涛,任博.溶剂萃取法回收钛白废液中钒的实验研究[J].稀有金属与硬质合金,2020(1):9-12. 被引量:4

1杨小慧,李望,朱晓波.D751螯合树脂吸附酸性溶液中钒(Ⅳ)离子的机制[J].中国有色金属学报,2022,32(12):3862-3870.

2郝立苗,黄妃慧,程国园,王勇伟,邢延岭,关洋,陈一韬.我国铝矾土尾矿资源化利用研究进展[J].现代矿业,2023,39(4):114-118.

3叶鑫,赵爱春,刘宸嘉,卓泽森,杨小容,秦妍梅,曾淼.赤泥中有价金属的回收工艺研究进展[J].湿法冶金,2023,42(3):229-235.

1黎娜,刘吉,邱峰.基于氧化铝赤泥的拜耳法回收再利用技术研究[J].世界有色金属,2020(19):1-2. 被引量:1

2张利祥,高一强,黄建洪,陈珊,张琴,陈允建,伏江丽.赤泥资源化综合利用研究进展[J].硅酸盐通报,2020,39(1):144-149. 被引量:30

3党海笑,张金喜,王建刚.水玻璃模数对碱激发赤泥胶凝材料性能影响研究[J].有色金属:冶炼部分,2020(9):115-119. 被引量:5

4张申.赤泥全链条综合利用探讨和应用[J].华东科技:综合,2020(5):0430-0430.

5高纯氧化钪及钪合金产业化基地项目[J].中国粉体工业,2021(3):66-66.

6田迎澳,郭玲珏,闫慧峰,曾煜辰,邹云玲.板钛矿/锐钛矿混晶TiO2的制备及光催化性能[J].纳米技术,2021,11(2):9-18.

7李诚,任利锋,张泽华.熔融法-X射线荧光光谱测定金红石矿石中18种主次量元素[J].环境化学,2021,40(5):1623-1627. 被引量:3

8梁晨,褚福浩,任强强,王小芳.煤气化飞灰流态化改性与再气化特性试验研究[J].洁净煤技术,2021,27(3):116-122. 被引量:4

Basic Information:

DOI:

Chinese Library Classification Number:TF09[冶金工程—冶金物理化学]

Citation Information:

The extraction of vanadium and scandium from red mud were carried out by leaching with tita-nium dioxide wastewater.The effects of liquid to solid ratio, leaching temperature, leaching time and stirring rate on the leaching rate of vanadium and scandium were investigated.The phase composition of lea-ching residue and the chemical composition of leaching solution were analyzed by XRD and ICP-AES.The results show that under the conditions of liquid to solid ratio of 6 mL/g, stirring rate of 400 r/min, leaching temperature of 75 ℃ and leaching time of 1 h, the leaching rates of V and Sc are 75% and 80%,respectively.Compared with the titanium dioxide wastewater, the leaching solution contains significantly decreased H+ concentration, vanadium and scandium are enriched and the concentration of iron and aluminum is also increased.Compared with the red mud, anhydrite minerals appears in the leaching residue, while calcite is completely dissolved, cancrinite, brookite and hematite are partially dissolved.

quote

GB/T 7714-2015 [1] LI Wang, YANG Xiao-hui, ZHU Xiao-bo. Experimental Study on Recovery of Scandium and Vanadium from Red Mud by Leaching with Titanium Dioxide Wastewater[J]. Rare Metals and Cemented Carbides, 2021(3): 1-4.
MLA [1] LI Wang, et al., "Experimental Study on Recovery of Scandium and Vanadium from Red Mud by Leaching with Titanium Dioxide Wastewater." Rare Metals and Cemented Carbides, no. 3, 2021, pp. 1-4.
APA [1] LI Wang, YANG Xiao-hui, & ZHU Xiao-bo. (2021). Experimental Study on Recovery of Scandium and Vanadium from Red Mud by Leaching with Titanium Dioxide Wastewater. Rare Metals and Cemented Carbides(3), 1-4.
IEEE [1] LI Wang, YANG Xiao-hui, and ZHU Xiao-bo, "Experimental Study on Recovery of Scandium and Vanadium from Red Mud by Leaching with Titanium Dioxide Wastewater," Rare Metals and Cemented Carbides, no. 3, pp. 1-4, 2021. keywords: {scandium;vanadium;leaching;red mud;titanium dioxide wastewater}