Calculation of the field emission current from carbon nanotubes using the Bardeen transfer Hamiltonian method AITranslate
Abstract AITranslate
We have theoretically calculated the field emission current from carbon nanotubes using the Bardeen transfer Hamiltonian method. The tunneling matrix element in proposed modeling of the electron field emission from armchair carbon nanotubes is built and considered based on the tunneling approach of Bardeen. The electron field emission currents are calculated at small voltage and temperature.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1016/j.commatsci.2010.04.027
Chinese Library Classification Number:
Citation Information:
We have theoretically calculated the field emission current from carbon nanotubes using the Bardeen transfer Hamiltonian method. The tunneling matrix element in proposed modeling of the electron field emission from armchair carbon nanotubes is built and considered based on the tunneling approach of Bardeen. The electron field emission currents are calculated at small voltage and temperature.
quote
| GB/T 7714-2015 | [1] Nguyen Ngoc Hieu, Nguyen Van Hanh, Tran Cong Phong. Computational Materials Science, 2010(49). DOI:10.1016/j.commatsci.2010.04.027. |
| MLA | [1] Nguyen Ngoc Hieu, et al., Computational Materials Science, no. 49, 2010, https://doi.org/10.1016/j.commatsci.2010.04.027. |
| APA | [1] Nguyen Ngoc Hieu, Nguyen Van Hanh, & Tran Cong Phong. (2010). Computational Materials Science(49). https://doi.org/10.1016/j.commatsci.2010.04.027 |
| IEEE | [1] Nguyen Ngoc Hieu, Nguyen Van Hanh, and Tran Cong Phong, Computational Materials Science, no. 49, 2010, doi: 10.1016/j.commatsci.2010.04.027. |