Study on Recovery of Molybdenum from High-sulphate Ammonium Molybdate Solution by Extraction AITranslate
Abstract AITranslate
Extraction method was employed to recover molybdenum from the high-sulphate ammonium molybdate solution obtained by the pressurized oxidized ammonia leaching-purification process of molybdenum concentrate.The effects of 2-octanol concentration, acid dosage, O/A phase ratio and oscillation time on Mo extraction were investigated.The results show that the optimal extraction conditions are 2-octanol volume fraction of 15%,1∶1 sulfuric acid dosage of 10% feed liquid volume, O/A phase ratio of 1.2/1 and oscillation time of 5 min.Through single-stage extraction, washing and single-stage stripping, the average Mo extraction rate reaches 99.61%,the Mo stripping rate is close to 100%,and the average Mo and SO42-contents are 161.99 g/L and 18 g/L,respectively, realizing the efficient recovery of molybdenum.
KeyWords AITranslate
1谢铿,王海北,张邦胜.辉钼精矿加压湿法冶金技术研究进展[J].金属矿山,2014,43(1):74-79. 被引量:13
2张亨.钼酸铵的生产研究进展[J].中国钼业,2013,37(2):49-54. 被引量:5
3何树荣.工业氧化钼实用生产技术及进展[J].材料开发与应用,2013,28(1):96-101. 被引量:5
4蒲敬文,鲁兴武,李冠军,张析.钼精矿制取四钼酸铵实验研究[J].甘肃冶金,2013,35(1):7-9. 被引量:7
5王晓亮,沈裕军,彭俊,刘强,周小舟.采用硫酸酸沉法从高硫钼酸铵溶液中回收钼的工艺研究[J].矿冶工程,2018,38(6):124-126. 被引量:3
6周新文,王磊,唐丽霞.离子交换法除杂制备钼酸铵[J].中国钼业,2011,35(3):33-35. 被引量:5
7曹耀华,刘红召,高照国,杨绍文.从彩钼铅粗精矿碱性浸出液中提取钼的新工艺[J].湿法冶金,2012,31(2):118-121. 被引量:6
8王海北,邹小平,蒋应平,张邦胜,张磊.溶剂萃取法从加压浸出液中提取钼[J].铜业工程,2011(5):21-26. 被引量:6
9徐徽,皮关华,陈白珍,石西昌,李俊丽.用溶剂萃取法从碱浸液中回收钼的研究[J].湖南师范大学自然科学学报,2007,30(1):43-46. 被引量:9
10钟宏,符剑刚,刘凌波.采用N235从含Mo,Mn酸浸液中萃取回收Mo[J].过程工程学报,2006,6(1):28-31. 被引量:10
1孙凯学.钼酸铵制备技术研究现状[J].云南化工,2021,48(10):32-34. 被引量:1
2马致远,刘勇,吕建芳,吕先谨,周吉奎.废石化催化剂萃钒余液中钼的回收[J].有色金属:冶炼部分,2022(9):112-116.
1马致远,刘勇,吕建芳,吕先谨,周吉奎.废石化催化剂萃钒余液中钼的回收[J].有色金属:冶炼部分,2022(9):112-116.
1伏彩萍.铋精矿加压氧化氨浸高效分离铜、硫和铋[J].矿冶工程,2020,40(2):111-113.
2孙颖,张廷安,吕国志,张伟光,麻海兰.含钒酸性溶液阴离子萃取分离钒铁的研究[J].有色金属:冶炼部分,2021(4):41-47. 被引量:2
3张娟,杜紫诚,骆如兵.正交试验法在高效液相色谱法测定水中甲醛含量的应用研究[J].广东化工,2021(7):170-171. 被引量:2
4王玉,程晓兵.盐酸多西环素结晶工艺的优化[J].国外医药:抗生素分册,2021,42(2):125-128.
5徐庆,王琳淞,武秀胜,张帆,李占勇.低温球形颗粒表面喷雾冷冻涂覆液膜的生长规律[J].天津科技大学学报,2021,36(1):42-47.
6马升峰,孟志军,李裕,许延辉,高天佐,关卫华,王荣,王永利.高浓度镨钕料液去除杂质铝的工艺研究(Ⅰ)[J].稀有金属与硬质合金,2021,49(2):9-14. 被引量:1
7支冬安,张志成,王辉,夏良树.Purex流程中铀、钚、锆、钌混合溶液界面污物的成因研究[J].核科学与工程,2021,41(2):427-432.
8丘丽莉,张魁芳,刘志强,王瑞祥,陈金清,钟晓聪,袁祥奕.硫酸体系中Cyanex272的萃镓性能研究[J].有色金属:冶炼部分,2021(5):86-91. 被引量:2
9李婷婷,刘瑞金,徐占宇,张文斌,张国光,高媛.高品质醋酸镧制备过程母液的资源化利用研究[J].稀有金属与硬质合金,2021,49(2):36-40.
10宫晓丹,张伟.从含铜锌粉置换渣中回收铜的工艺设计与应用研究[J].世界有色金属,2021(4):4-5. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TF841.2[冶金工程—有色金属冶金]
Citation Information:
Extraction method was employed to recover molybdenum from the high-sulphate ammonium molybdate solution obtained by the pressurized oxidized ammonia leaching-purification process of molybdenum concentrate.The effects of 2-octanol concentration, acid dosage, O/A phase ratio and oscillation time on Mo extraction were investigated.The results show that the optimal extraction conditions are 2-octanol volume fraction of 15%,1∶1 sulfuric acid dosage of 10% feed liquid volume, O/A phase ratio of 1.2/1 and oscillation time of 5 min.Through single-stage extraction, washing and single-stage stripping, the average Mo extraction rate reaches 99.61%,the Mo stripping rate is close to 100%,and the average Mo and SO42-contents are 161.99 g/L and 18 g/L,respectively, realizing the efficient recovery of molybdenum.
quote
| GB/T 7714-2015 | [1] ZHOU Xiao-zhou, SHEN Yu-jun, PENG Jun, et al. Study on Recovery of Molybdenum from High-sulphate Ammonium Molybdate Solution by Extraction[J]. Rare Metals and Cemented Carbides, 2021(2): 1-4. |
| MLA | [1] ZHOU Xiao-zhou, et al., "Study on Recovery of Molybdenum from High-sulphate Ammonium Molybdate Solution by Extraction." Rare Metals and Cemented Carbides, no. 2, 2021, pp. 1-4. |
| APA | [1] ZHOU Xiao-zhou, SHEN Yu-jun, PENG Jun, & LIU Qiang. (2021). Study on Recovery of Molybdenum from High-sulphate Ammonium Molybdate Solution by Extraction. Rare Metals and Cemented Carbides(2), 1-4. |
| IEEE | [1] ZHOU Xiao-zhou, SHEN Yu-jun, PENG Jun, and LIU Qiang, "Study on Recovery of Molybdenum from High-sulphate Ammonium Molybdate Solution by Extraction," Rare Metals and Cemented Carbides, no. 2, pp. 1-4, 2021. keywords: {high-sulfate ammonium molybdate solution;molybdenum;recovery;extraction;N235} |