Study on Preparation of Rare Earth Metals with Low Oxygen and Titanium Content by Molten Salt Electrolysis AITranslate
Abstract AITranslate
Taking 6 kA rare earth electrolyzer as the research object, rare earth metals were prepared by electrolysis using fluorine salt system, and the effects of electrolysis temperature, oxide addition rate and metal extraction mode on the content of oxygen and titanium in rare earth metals were studied in combination with field production conditions and GDMS detection results.The results show that the oxygen and titanium content in rare earth metals can be stably controlled when rare earth metals are siphoned out of the oven, electrolytic temperature is controlled at 1 040~1 060 ℃,and oxide addition rate is 7~8 kg/h.The oxygen content in rare earth metals is less than 0.010% and the titanium content is less than 0.012%.
KeyWords AITranslate
1张德平,唐定骧,陈云贵,薛江,张洪杰,赵海东,孟健.滞销镧铈/镧镨铈混合稀土金属在金属材料中的应用[J].稀土,2009,30(5):70-77. 被引量:11
2杨超云,栾义坤,李殿中,李依依.稀土元素对高洁净度轴承钢中夹杂物的影响研究[J].炼钢,2016,32(4):54-59. 被引量:26
3杨光维,郝鑫,杨叠,王新华,黄福祥,王万军.GCr15轴承钢冶炼过程钢液洁净度变化[J].钢铁,2014,49(11):31-35. 被引量:14
4Heng Cui Yan-ping Bao Min Wang Wei-shuang Wu.Clogging behavior of submerged entry nozzles for Ti-bearing IF steel[J].矿物冶金与材料学报:英文版,2010,17(2):154-158. 被引量:13
5龚姚腾,李玉泽,逄启寿,王海辉,冯羽生.多因素对稀土电解槽电解效率的影响[J].有色金属工程,2019,9(8):53-58. 被引量:6
6王权,王玉峰,赵岳林,赵良忠,赵海营,夏云.稀土电解炉钨阴极失效原因分析[J].稀土,2019,40(5):106-114. 被引量:3
7刘木根,王亮亮.电解温度对稀土电解槽技术指标的影响研究[J].稀有金属与硬质合金,2014,42(6):16-19. 被引量:4
8王亮,逄启寿.稀土电解槽三维电场和温度场的分析研究[J].中国有色冶金,2017,46(6):44-47. 被引量:7
9张志宏,焦士琢,吴迪武,刘文淮.氧化物电解法制备钕铁合金的研究[J].稀土,1993,14(1):29-33. 被引量:4
10赵桂芳.熔盐电解制取稀土金属过程界面现象[J].江西有色金属,1989,3(1):10-11. 被引量:1
1熊志伟,刘爱民,刘玉宝,王旭,石忠宁.La_(2)O_(3)在LiF⁃NaF熔盐体系中的溶解行为[J].材料与冶金学报,2022,21(3):167-171.
2逄启寿,忻治霖,林小程,龚姚腾,王郅阳.稀土电解槽电化学三维时变流场数值模拟[J].有色金属科学与工程,2022,13(3):152-158. 被引量:1
1李科臻,王新春.稀土电解槽槽电阻数据的降噪与分析[J].新型工业化,2022,12(8):153-158. 被引量:1
1李擎煜,曾鲜,程旭东.低红外发射率陶瓷层/金属层/陶瓷层复合薄膜高温性能研究[J].表面技术,2020,49(5):299-307. 被引量:2
2谭秀珍,李瑶,陈晶晶,朱刘,邓育宁.辉光放电质谱(GDMS)法校正高纯氧化铋中19种元素的相对灵敏度因子[J].中国无机分析化学,2019,9(6):63-68. 被引量:8
3田懿,巨亚锋,蒲晓莉,吕红刚,赵钰,冯定.油管悬挂器K形金属环密封特性模拟分析[J].石油机械,2021,49(5):81-88. 被引量:3
4廖春发,郭超,林觉远,蔡伯清,王旭.电流密度对稀土熔盐电解影响的研究进展[J].稀土,2021(1):122-128. 被引量:4
5刘杰,范晓勇,闫龙,高勇,李冬,周秋成.SJ型低温干馏炉燃烧影响因素研究[J].能源化工,2021,42(2):1-6.
Basic Information:
DOI:
Chinese Library Classification Number:TF845.6[冶金工程—有色金属冶金]
Citation Information:
Taking 6 kA rare earth electrolyzer as the research object, rare earth metals were prepared by electrolysis using fluorine salt system, and the effects of electrolysis temperature, oxide addition rate and metal extraction mode on the content of oxygen and titanium in rare earth metals were studied in combination with field production conditions and GDMS detection results.The results show that the oxygen and titanium content in rare earth metals can be stably controlled when rare earth metals are siphoned out of the oven, electrolytic temperature is controlled at 1 040~1 060 ℃,and oxide addition rate is 7~8 kg/h.The oxygen content in rare earth metals is less than 0.010% and the titanium content is less than 0.012%.
quote
| GB/T 7714-2015 | [1] LIU Hang, ZHANG Yao, QIAO Xiao-hui, et al. Study on Preparation of Rare Earth Metals with Low Oxygen and Titanium Content by Molten Salt Electrolysis[J]. Rare Metals and Cemented Carbides, 2021(2): 5-8. |
| MLA | [1] LIU Hang, et al., "Study on Preparation of Rare Earth Metals with Low Oxygen and Titanium Content by Molten Salt Electrolysis." Rare Metals and Cemented Carbides, no. 2, 2021, pp. 5-8. |
| APA | [1] LIU Hang, ZHANG Yao, QIAO Xiao-hui, & LUAN Yi-kun. (2021). Study on Preparation of Rare Earth Metals with Low Oxygen and Titanium Content by Molten Salt Electrolysis. Rare Metals and Cemented Carbides(2), 5-8. |
| IEEE | [1] LIU Hang, ZHANG Yao, QIAO Xiao-hui, and LUAN Yi-kun, "Study on Preparation of Rare Earth Metals with Low Oxygen and Titanium Content by Molten Salt Electrolysis," Rare Metals and Cemented Carbides, no. 2, pp. 5-8, 2021. keywords: {rare earth metal;oxygen content;titanium content;molten salt electrolysis;siphoning out} |