Study of structural, electrical and optical properties of vanadium oxide condensed films deposited by spray pyrolysis technique AITranslate

Ferdowsi University of Mashhad; Ferdowsi University of Mashhad; Ferdowsi University of Mashhad; Damghan University
AITranslate
Publisher: Springer Nature
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Vanadium oxides condensed films are prepared on glass substrates, using spray pyrolysis (SP) technique. The effects of substrate temperature, vanadium concentration in initial solution and the solution spray rate on the nano-structural, electrical, and optical properties of deposited films were investigated. Characterizations of the samples were performed using X-ray diffraction (XRD), scanning electron microscopy (SEM), and UV-Vis spectroscopy methods. The type and concentration of the charge carriers were determined and measured by Hall effect experiment. XRD patterns showed that the prepared films had polycrystalline structure, mostly tetragonal β-V2O5 and V4O9 phases with the preferred orientation along (200) direction. The Hall effect experiment revealed that all samples were n-type, except the ones deposited at substrate temperatures T sub = 300 °C and T sub = 450 °C, vanadium concentration 0.1 mol/L and solution spray rate 10 mL/min. The charge carrier concentrations obtained were in the range 1016–1018 cm−3. The lowest sheet resistance (R s) was obtained for the samples prepared at T sub = 450 °C, vanadium concentration 0.05 mol/L and solution spray rate 10 mL/min. It was also found that the optical transparency of the samples changed from 20% to 75% and the optical band gap of the samples was from 2.22 eV to 2.58 eV, depending on the deposition conditions.

KeyWords AITranslate

Vanadium oxide Thin films Optical properties Spray pyrolysis
No data

Basic Information:

DOI:https://doi.org/10.1007/s40436-013-0045-y

Chinese Library Classification Number:

Citation Information:

Vanadium oxides condensed films are prepared on glass substrates, using spray pyrolysis (SP) technique. The effects of substrate temperature, vanadium concentration in initial solution and the solution spray rate on the nano-structural, electrical, and optical properties of deposited films were investigated. Characterizations of the samples were performed using X-ray diffraction (XRD), scanning electron microscopy (SEM), and UV-Vis spectroscopy methods. The type and concentration of the charge carriers were determined and measured by Hall effect experiment. XRD patterns showed that the prepared films had polycrystalline structure, mostly tetragonal β-V2O5 and V4O9 phases with the preferred orientation along (200) direction. The Hall effect experiment revealed that all samples were n-type, except the ones deposited at substrate temperatures T sub = 300 °C and T sub = 450 °C, vanadium concentration 0.1 mol/L and solution spray rate 10 mL/min. The charge carrier concentrations obtained were in the range 1016–1018 cm−3. The lowest sheet resistance (R s) was obtained for the samples prepared at T sub = 450 °C, vanadium concentration 0.05 mol/L and solution spray rate 10 mL/min. It was also found that the optical transparency of the samples changed from 20% to 75% and the optical band gap of the samples was from 2.22 eV to 2.58 eV, depending on the deposition conditions.

quote

GB/T 7714-2015 [1] M. Mousavi, A. Kompany, N. Shahtahmasebi, et al. Advances in Manufacturing, 2013(1). DOI:10.1007/s40436-013-0045-y.
MLA [1] M. Mousavi, et al., Advances in Manufacturing, no. 1, 2013, https://doi.org/10.1007/s40436-013-0045-y.
APA [1] M. Mousavi, A. Kompany, N. Shahtahmasebi, & M. M. BagheriMohagheghi. (2013). Advances in Manufacturing(1). https://doi.org/10.1007/s40436-013-0045-y
IEEE [1] M. Mousavi, A. Kompany, N. Shahtahmasebi, and M. M. BagheriMohagheghi, Advances in Manufacturing, no. 1, 2013, doi: 10.1007/s40436-013-0045-y. keywords: {Vanadium oxide;Thin films;Optical properties;Spray pyrolysis}