Technological Study on Germanium Recovery from Germanium-containing Polymetallic Materials AITranslate

School of Materials Science and Engineering, Shanghai University;School of Materials Science and Engineering, Shanghai University;School of Materials Science and Engineering, Shanghai University;School of Materials Science and Engineering, Shanghai University;School of Materials Science and Engineering, Shanghai University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Germanium-containing polymetallic materials were pretreated progressively with hydrochloric acid-ammonium fluoride-potassium,and then separated by distillation using hydrochloric acid to extract germanium tetrachloride.The final recovery of germanium is about 95.20%.The dosages were systematically studied through experiments of pretreatment hydrochloric acid,ammonium fluoride,potassium permanganate and distillation hydrochloric acid,and then optimum process conditions were determined.Compared with the conventional hydrometallurgical process of sulfuric acid leaching-tannin precipitation-germanium concentrate-hydrochloric acid distillation for germanium extraction,the recovery of germanium in the above process is improved by about 21%.

KeyWords AITranslate

germanium-containing polymetallic material germanium recovery hydrochloric acid-ammonium fluoride-potassium permanganate pretreatment hydrochloric acid distillation technological study

1李苗苗,苏小平,冯德伸,王学武,左建龙.GaAs/Ge太阳能电池用锗单晶的研究新进展[J].金属功能材料,2010,17(6):78-82. 被引量:12

2刘福财,袁琴,王铁艳.煤烟尘制取四氯化锗的研究[J].稀有金属,2011,35(4):623-626. 被引量:11

3郑海鹏.有机锗的生理功能及在食品中的应用[J].微量元素与健康研究,2011,28(4):65-67. 被引量:23

4普世坤,严云南,陈代凤.硅-锗合金废料中锗的回收研究[J].中国有色冶金,2011,40(4):57-59. 被引量:9

5罗星,张泽彪,彭金辉,王万坤,姚现召.拌酸熟化法从含锗渣中浸出锗的试验研究[J].稀有金属,2012,36(2):311-315. 被引量:12

6普世坤,兰尧中,靳林,肖春宏.提高含锗煤烟尘氯化蒸馏回收率的工艺研究[J].稀有金属,2012,36(5):817-821. 被引量:12

7普世坤,兰尧中.从粉煤灰中回收锗的湿法工艺研究[J].稀有金属与硬质合金,2012,40(5):15-17. 被引量:10

8张家敏,雷霆,张玉林,冯林永.从含锗褐煤中干馏提锗和制取焦炭的试验研究[J].稀有金属,2007,31(3):371-376. 被引量:18

9赵立奎,黄和明.含锗烟尘中锗的提取工艺方法探讨[J].稀有金属,2006,30(z2):111-113. 被引量:13

10冯德伸,苏小平,闵振东,尹士平.Φ300 mm红外锗单晶生长及性能测试[J].稀有金属,2006,30(5):692-694. 被引量:12

1张苏江,季根源,王楠,姜爱玲,尚磊.中国锗矿资源现状及其可持续发展对策研究[J].矿产保护与利用,2017,37(2):6-12. 被引量:22

2杨再磊,李长林,谢高,薛丹,滕文,陈代凤,普世坤.乳化氧化预处理-氯化蒸馏法回收锗的工艺研究[J].中国有色冶金,2018,47(1):58-61. 被引量:1

1茹丘旭,马滋蔓.锗在红外光学行业的应用思考[J].中国科技纵横,2018,0(22):217-218.

2仝一喆.硫化锌精矿加压氧浸炼锌工艺过程锗的强化富集[J].稀有金属与硬质合金,2018,46(3):10-12. 被引量:4

3季根源,张洪平,李秋玲,夏浩东.中国稀土矿产资源现状及其可持续发展对策[J].中国矿业,2018,27(8):9-16. 被引量:57

4茹丘旭,马滋蔓.锗的应用趋向及预测分析[J].科技创新导报,2018,15(22):68-69. 被引量:2

5李明,张培新,蔡玉曼.碱熔-电感耦合等离子体质谱测定多金属矿中的锗[J].江苏科技信息,2019,36(4):31-35. 被引量:3

6花冬蕾.有色金属矿山资源勘查可持续发展对策研究[J].世界有色金属,2019,44(2):100-101. 被引量:1

7覃先欢.解析广西矿产资源的开发利用及可持续发展[J].中国金属通报,2018(11):272-272. 被引量:1

8赵汀,王登红,刘超,李德先,周凤英.中国锗矿成矿规律与开发利用现状[J].地质学报,2019,93(6):1245-1251. 被引量:16

9宋俊祎,谭银龙,蒋玉仁,胡碧茹,吴文健.能“锗”多劳[J].化学教育(中英文),2019,40(14):1-6. 被引量:2

10马奎,洛桑才仁,陈超,张万益,王丰翔.全球锗资源分布、供需及消费趋势研究[J].矿产保护与利用,2019,39(5):16-25. 被引量:12

1融入居室之美 SONY嵌入式播放机[J].数码,2005(4):156-156.

2蒋伟,蒋开喜,王海北,蒋训雄,张邦胜.一种从锗精矿制备高纯二氧化锗的新工艺[J].矿冶,2007,16(3):26-28. 被引量:3

3王向涛.有色金属在手机中的应用[J].中国金属通报,2005,0(15):19-19.

4黄和明.从含锗蒸馏渣中回收锗的工艺方法探讨[J].江苏冶金,1998,26(6):23-25.

5姚晓峰,徐慧朴.基于LABVIEW和OPC技术的蒸馏CAN总线控制系统[J].微计算机信息,2006(02Z):117-119. 被引量:2

6夏伟锋,冯飞,王权,熊斌,戈肖鸿.KOH各向异性腐蚀中预处理对硅表面粗糙度的影响[J].半导体光电,2010,31(4):579-582. 被引量:1

7王小珊,刘丽娟,夏明军,王晓洋,陈创天.Two Isostructural Multi-metal Borates: Syntheses, Crystal Structures and Characterizations of M_3LiNa_4Be_4B_(10)O_(24)F(M = Sr, Cd)[J].结构化学(英文),2015,34(10):1617-1625. 被引量:2

8李贺成,刘建平.光纤用四氯化锗含氢杂质的测定方法[J].分析试验室,1992,11(6):10-13. 被引量:2

9黄和明,赵立奎.高硅含锗物料中锗的提取工艺探讨[J].广东有色金属学报,2002,12(B09):33-35. 被引量:6

10黄显宾,林理彬,杨礼兵,邓建军,顾元朝,叶式灿,岳正谱,周少彤,李丰平,张思群.平行面多金属钨丝Z箍缩实验研究[J].强激光与粒子束,2005,17(5):793-796. 被引量:4

Basic Information:

DOI:

Chinese Library Classification Number:TN304.11[电子电信—物理电子学]

Citation Information:

Germanium-containing polymetallic materials were pretreated progressively with hydrochloric acid-ammonium fluoride-potassium,and then separated by distillation using hydrochloric acid to extract germanium tetrachloride.The final recovery of germanium is about 95.20%.The dosages were systematically studied through experiments of pretreatment hydrochloric acid,ammonium fluoride,potassium permanganate and distillation hydrochloric acid,and then optimum process conditions were determined.Compared with the conventional hydrometallurgical process of sulfuric acid leaching-tannin precipitation-germanium concentrate-hydrochloric acid distillation for germanium extraction,the recovery of germanium in the above process is improved by about 21%.

quote

GB/T 7714-2015 [1] PU Shi-kun, LAN Yao-zhong, ZHU Zhi-guo, et al. Technological Study on Germanium Recovery from Germanium-containing Polymetallic Materials[J]. Rare Metals and Cemented Carbides, 2015(6): 19-23.
MLA [1] PU Shi-kun, et al., "Technological Study on Germanium Recovery from Germanium-containing Polymetallic Materials." Rare Metals and Cemented Carbides, no. 6, 2015, pp. 19-23.
APA [1] PU Shi-kun, LAN Yao-zhong, ZHU Zhi-guo, XIE Tian-min, & YIN Guo-wen. (2015). Technological Study on Germanium Recovery from Germanium-containing Polymetallic Materials. Rare Metals and Cemented Carbides(6), 19-23.
IEEE [1] PU Shi-kun, LAN Yao-zhong, ZHU Zhi-guo, XIE Tian-min, and YIN Guo-wen, "Technological Study on Germanium Recovery from Germanium-containing Polymetallic Materials," Rare Metals and Cemented Carbides, no. 6, pp. 19-23, 2015. keywords: {germanium-containing polymetallic material;germanium recovery;hydrochloric acid-ammonium fluoride-potassium permanganate pretreatment;hydrochloric acid distillation;technological study}